ASTM A497/A497M, "Standard Specification for Steel Welded Wire Reinforcement, Deformed, for Concrete," (withdrawn 2013).

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ASTM A497/A497M, "Standard Specification for Steel Welded Wire Reinforcement, Deformed, for Concrete," (withdrawn 2013).

Author(s):

Publication: Commentary Reference

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 1/1/2007

Abstract:
This specification covers steel-welded wire reinforcements, deformed for concrete reinforcement. The welded wire reinforcement shall be furnished either in flat sheets, or in rolls as specified by the purchaser. The wires shall be assembled, connected to every intersections, and shall be fabricated and finished wherein the wires shall conform to the required specifications. Tensile, bend and weld shear strength tests shall be performed to assure the specimens meet the mechanical property requirements.