Utilization of Waste CO<sub>2</sub> Generated Vaterite in Blended Cements

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Utilization of Waste CO2 Generated Vaterite in Blended Cements

Author(s): Ying Wang, Jesus Gonzalez, Craig W. Hargis

Publication: Symposium Paper

Volume: 362

Issue:

Appears on pages(s): 854-870

Keywords: cement, early age strength, setting time, sustainability, vaterite

DOI: 10.14359/51742014

Date: 6/17/2024

Abstract:
This paper discusses the results of a 5-10% vaterite replacement of SCMs in certain blended cements. In cement-fly ash blended cement, a 10% vaterite replacement of fly ash achieved a 40% higher strength at 1 day and maintained a consistently higher strength than the cement-fly ash blended cement control through 56 days. A 10% vaterite replacement of slag in a cement-slag blended cement achieved approximately 20% higher strength at 3 days. For a cement-slag-fly ash blended cement, a 10% replacement of fly ash with vaterite achieved a 30% to 50% strength increase through 7 days, and a 50 to 110-minute reduction in the initial setting. The bulk resistivity of all the blended cement was increased after including vaterite, indicating the potential for better durability. The alkali-silica reaction test resulted in low amounts of expansion confirming the vaterite-blended cements’ durability. Hydration analysis using isothermal calorimetry and thermogravimetry also showed extra early-age hydration reactions due to vaterite inclusion. Using vaterite in blended cement can help reduce the embodied carbon and enhance many of the engineering properties, such as setting time, early-age strength, and durability.