Leaching of Magnesium Phosphate Cement Pastes: Influence of the Mg/P Molar Ratio

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Leaching of Magnesium Phosphate Cement Pastes: Influence of the Mg/P Molar Ratio

Author(s): Laura Diaz Caselles, Ganaël Bon, Céline Cau Dit Coumes, Pascal Antonucci, Angélique Rousselet, Adel Mesbah, Valérie Montouillout

Publication: Symposium Paper

Volume: 362

Issue:

Appears on pages(s): 594-609

Keywords: cattiite, compressive strength, durability, K-struvite, leaching, magnesium phosphate cement, mineralogy

DOI: 10.14359/51741014

Date: 6/14/2024

Abstract:
This paper investigates the leaching behavior of magnesium phosphate cement-based materials (MPC) prepared using hard-burnt magnesia (MgO) and monopotassium phosphate (KH2PO4). Three different formulations of variable Mg/P molar ratios (1, 2, and 3) were tested. Upon hydration, K-struvite was the main hydrate formed in all cases. After 28 days of curing, mechanical properties were assessed on MPC mortars. Semi-dynamic leaching tests were performed on MPC paste monoliths for 28 days under well-controlled conditions and using demineralized water with a pH maintained at 7. Leaching solutions were frequently renewed. Solids were characterized before and after leaching using XRD and SEM/EDS. The cumulative element release, plotted against the square root of time, indicated that leaching was mainly controlled by diffusion in all samples. Examination of the solids revealed a zonation process involving K-struvite dissolution and cattiite precipitation. Analyses of leachates showed that fluxes of leached species increased with decreasing Mg/P molar ratios. This parameter was thus a key factor, influencing the pore network and the resistance of MPC-based materials to leaching.