Title:
Upcycling Basic Oxygen Furnace (BOF) Slag into a Carbon Negative Supplementary Cementitious Material (SCM) through Mineral Carbonation
Author(s):
Hadi Kazemi Kamy, Peter Nielsen, Bert Riems, and Liesbeth Horckmans
Publication:
Symposium Paper
Volume:
362
Issue:
Appears on pages(s):
558-569
Keywords:
BOF slag, Concurrent grinding/milling and carbonation, dynamic carbonation, mineral carbonation, reactive silica, SCM
DOI:
10.14359/51741011
Date:
6/14/2024
Abstract:
Lowering the direct CO2 emissions of cement production is a prime objective of the cement industry. Substitution of clinker, for instance with by-products from other industries, is a widely adopted means to reduce direct emissions. A bottleneck in lowering clinker content is the availability of known clinker-replacement materials, as beneficiation processes are often required to condition the materials for such use. This may range from grinding and purification operations to calcination treatments. A novel approach is to use mineral carbonation as a beneficiation step for the conversion of by-products, such as steel slag, into SCMs. The reaction with CO2 activates Ca-silicates by the formation of calcium carbonates and reactive silica, and more importantly, it enables sequestering of CO2 in stable mineral products. It also provides a recycling strategy for steel producers. The ERA-MIN3 project CO2 TREAT aims at transforming BOF slag into valuable SCMs for cement production. In this paper, the results of an experimental campaign to better understand the effect of process conditions for carbonating BOF slag, to obtain the highest degree of carbonation and reactivity, are presented.
Related References:
1. CEMBUREAU, The role of cement in the 2050 low carbon economy. 2016, The European Cement Association: Brussels.
2. Global Cement and Concrete Association, Getting the Numbers Right. 2018.
3. Bolte, G., et al., Development of composite cements characterized by low environmental footprint. Journal of Cleaner Production, 2019. 226: p. 503-514.
4. Matschei, T., B. Lothenbach, and F.P. Glasser, The role of calcium carbonate in cement hydration. Cement and Concrete Research, 2007. 37: p. 551-558.
5. Favier, A., et al., A sustainable future for the European Cement and Concrete Industry: Technology assessment for full decarbonisation of the industry by 2050. 2018, ETH Zurich.
6. EUROFER, European Steel in Figures. 2020.
7. Juenger, M.C., R. Snellings, and S.A. Bernal, Supplementary cementitious materials: New sources, characterization, and performance insights. Cement and Concrete Research, 2019. 122: p. 257-273.
8. Han, F., et al., Hydration heat evolution and kinetics of blended cement containing steel slag at different temperatures. Thermochimica Acta, 2015. 605: p. 43-51.
9. Huijgen, W.J., and R.N. Comans, Carbonation of Steel Slag for CO2 Sequestration: Leaching of Products and Reaction Mechanisms. Environmental Science and Technology, 2006. 40: p. 2790-2796.
10.Woodall, C.M., et al., Utilization of mineral carbonation products: current state and potential. Greenhouse Gases: Science and Technology, 2019. 9: p. 1096-1113.
11. Zajac, M., et al., Effect of carbonated cement paste on composite cement hydration and performance. Cement and Concrete Research, 2020. 134: p. 106090.
12.Hou, J., et al., Material properties of steel slag-cement binding materials prepared by precarbonated steel slag. Journal of Materials in Civil Engineering, 2018. 30: p. 04018208.
13. Snellings, R., K. Scrivener, B. Lothenbach (Eds.) A Practical Guide to microstructural Analysis of Cementitious Materials, Crc Press, 2016.
14. Steinour, H. H. (1959). “Some effects of carbon dioxide on mortars and concrete-discussion.” Journal of American Concrete Institute, 50(2), 905–907.
15. Schnabel, K., F. Brück, S. Poh, T. Mansfeldt, H. Weigand (2021) Technically exploitable mineral carbonation potential of four alkaline waste materials and effects on contaminant mobility. Greenhouse Gas Sci Technol. 0:1–14 (2021); doi: 10.1002/ghg.206
16.Nielsen, P., Quaghebeur, M., 2023 Determination of the CO2 Uptake of Construction Products Manufactured by Mineral Carbonation. Minerals 2023, 13, 1079. doi: 10.3390/min13081079
17. Zago, S.C.; Vernilli, F.; Cascudo, O. The Reuse of Basic Oxygen Furnace Slag as Concrete Aggregate to Achieve Sustainable Development: Characteristics and Limitations. Buildings 2023, 13, 1193. doi: 10.3390/buildings13051193
18.Huijgen, W. J., Witkamp, G. J., and Comans, R. N. (2005). Mineral CO2 sequestration by steel slag carbonation. Environ. Sci. Technol. 39, 9676–9682. doi: 10.1021/es050795f
19.Daval, D., Martinez, I., Corvisier, J., Findling, N., Goffé, B., Guyot, F., et al. (2009). Carbonation of Ca-bearing silicates, the case of wollastonite: experimental investigations and kinetic modeling. Chem. Geol. 265, 63–78. doi: 10.1016/j.chemgeo.2009.01.022.
20. Librandi, P., P. Nielsen, G. Costa, R. Snellings, M. Quaghebeur, R. Baciocchi (2019) Mechanical and environmental properties of carbonated steel slag compacts as a function of mineralogy and CO2 uptake. Journal of CO2 Utilization, 33, 201-214. doi: 10.1016/j.jcou.2019.05.028
21. Béarat H, M.J. McKelvy , A.V. Chizmeshya, D. Gormley, R. Nunez, R.W. Carpenter, K. Squires, G.H. Wolf, 2006, Carbon sequestration via aqueous olivine mineral carbonation: role of passivating layer formation. Environ Sci Technol. 2006, 40 (15),4802-8. doi: 10.1021/es0523340
22.Chakrabarty, D., and S. Mahapatra, 1999, Aragonite crystals with unconventional morphologies. J. Mater. Chem., 9, 2953-2957.S
23. Santos, V.H.J.M.D., D. Pontin, G.G.D. Ponzi, A.S.G. Stepanha, R.B. Martel, M..K. Schütz, S.M.O. Einloft, F.D. Vecchia, 2021 Application of Fourier Transform infrared spectroscopy (FTIR) coupled with multivariate regression for calcium carbonate (CaCO3) quantification in cement, Construction and Building Materials, 313, 125413, doi: 10.1016/j.conbuildmat.2021.125413