Rebalancing the Risk Equation for the Ready-Mix Producer Through In-Transit Management Systems

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Rebalancing the Risk Equation for the Ready-Mix Producer Through In-Transit Management Systems

Author(s): Nathan Tregger

Publication: Web Session

Volume: ws_S24_NathanTregger.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 3/24/2024

Abstract:
Water has an obvious effect on both placability and strength of ready-mix concrete. The ability to track and modify the water content during delivery through in-transit management (ITM) systems has a profound effect on the risk to both the producer and contractor. This presentation will explore how ITM systems combined with machine learning can help identify ways to improve consistency and provide confidence such that overdesign can be reduced while decreasing overall risk. Case studies will be presented to demonstrate how this has been accomplished in a real-world setting.