São Vicente Suspension Bridge Rehabilitation and Cable Substitution

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: São Vicente Suspension Bridge Rehabilitation and Cable Substitution

Author(s): Rafael Timerman,

Publication: Web Session

Volume: ws_S24_RafaelTimerman.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 3/24/2024

Abstract:
The São Vicente Suspension Bridge was built in 1914 as part of the plan for the sanitation of the São Vicente city. The bridge is listed by Brazilian historical heritage since 1982. In 2012, the conditions of the main structural elements were critical and needed recovery or substitution. The structural design considered the complete recovery of the steel main deck connected by rivets, the calculation of the new suspension system that would replace the existing one using temporary cables, towers and anchorage blocks. The bridge was reopened to the public in October of 2015.