Performance Review of High Performance Fiber Reinforced Concrete (HPFRC)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Performance Review of High Performance Fiber Reinforced Concrete (HPFRC)

Author(s): Nicolas Ginouse

Publication: Web Session

Volume: ws_S24_NicolasGinouse.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 3/24/2024

Abstract:
The demand for sustainable, durable and resilient infrastructures has never been as important as of today to ensure progress and growth of our modern society as well meeting our long term sustainability goals. The presentation will focus on actual durability and mechanical performances obtained during the production of high performance fiber reinforced concrete for heavy infrastructure projects. Some mix design aspects as well as critical production and quality control protocols to achieve consistent high performance results will be discussed.