Title: Preliminary Investigation of Textile Reinforced Concrete Exposed to an Aggregate Environment

Author(s): Paul Borg

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 3/24/2024

Abstract:
This session is one of 14 sessions that form the 16th Fiber Reinforced Polymer Reinforced Concrete Structures (FRPRCS-16) Symposium. It is co-sponsored by ACI Committee 440 and the International Institute for FRP in Construction (IIFC) for the purpose of advancing the understanding and application of FRP composites in civil infrastructure to serve the engineering profession and society. FRPRCS was first held in conjunction with the ACI 1993 Spring convention in Vancouver, British Columbia, Canada. Since 1993, FRPRCS has evolved into a prestigious and reputable international conference that has been held 15 times including 5 times in conjunction with ACI: British Columbia, Canada (1993); Baltimore (1999); Kansas City (2005); Tampa (2011); and Anaheim (2017).