Quantitative Analysis of Fly Ash Hydration Products Formed in Sulfate Environment

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Quantitative Analysis of Fly Ash Hydration Products Formed in Sulfate Environment

Author(s): Rajaram Dhole, Michael D.A. Thomas, Kevin J. Folliard, Thano Drimalas

Publication: Symposium Paper

Volume: 362

Issue:

Appears on pages(s): 412-431

Keywords: ettringite, fly ash, hydration products, monosulfate, scanning electron microscopy, X-ray diffraction

DOI: 10.14359/51740900

Date: 6/11/2024

Abstract:
Investigations were made into the hydration products formed by the fly ashes before and after exposure to sulfate solutions, and the impact of hydration products on the sulfate resistance of concrete. Pastes of selected Class C and Class F fly ashes were prepared by blending each fly ash with calcium hydroxide and a solution of sodium and potassium hydroxide. The quantities of ettringite, monosulfate, and portlandite formed in the paste samples at 28 days were determined by semi-quantitative X-ray diffraction analysis (XRD) using rutile as an internal standard. Subsequently, pastes were exposed to sulfate solutions of sodium and calcium in different concentrations for 90 days. At the end of 90 days, quantities of hydration products in the pastes subjected to sulfate solutions were determined by using the Rietveld method of analysis. In the second part of the program, mortar bars were exposed to sulfate solutions and examined by scanning electron microscopy (SEM) to determine the presence and location of sulfate reaction products namely ettringite, gypsum, and monosulfate. The degree of decalcification undergone by paste located in different zones in the mortar specimens was determined by measuring the CaO/SiO2 (C/S, ratio) using SEM coupled with ‘electron dispersive X-ray analysis’ (EDXA).

Related References:

1. Mehta, P. K. (1986) “Effect of Fly Ash Compositions on Sulfate Resistance of Cement” ACI Materials Journal, Nov-Dec, pp. 994-1000.

2. Tishmack, J.K., Olek, J. and Diamond, S. (1999) “Characterization of High-Calcium Fly Ashes and Their Potential Influence on Ettringite Formation in Cementitious Systems,” Cement, Concrete and Aggregates, Vol. 21, No.1, pp. 82-92.

3. Tikalsky, P.J and Carrasquillo R.L. (1993) Fly Ash Evaluation and Selection for Use in Sulfate–Resistant Concrete, ACI Materials Journal, Vol. 90, No. 6, pp.545-551.

4. Dunstan, E.R. (1980) “A possible method for identifying fly ashes that will improve the sulfate resistance of concretes,” Cement, Concrete and Aggregates, Vol. 2, No.1, pp. 20-30.

5. Thomas M.D.A. (1998) “Delayed ettringite formation in concrete: recent developments and future directions, University of Toronto.

6. Folliard, K. J., and Sandberg, P., “Mechanisms of Concrete Deterioration by Sodium Sulfate Crystallization,” Third International ACI/ CANMET Conference on Concrete Durability, SP-145, American Concrete Institute, Farmington Hills, MI, 1994, pp. 933-946

7. Mehta, P. K. (1973) “Mechanisms of expansion associated with ettringite formation”, Cement and Concrete Research, Vol. 3, pp. 1-6.

8. Tokyay, M., and Hubbard, H. F. (1992) Mineralogical Investigations of High Lime Fly ashes, ACI special publication, SP-132-05, Vol 132, pp. 65-71.

9. Skalny, J., Marchand, J.and Odler, I., (2002) Sulfate attack on concrete, London, Spon Press, 217 pp.

10. Naik, N.N., Jupe, A.C., Stock, S.R., Wilkinson, A.P., Lee, P.L., Kurtis, K.E. (2006) “Sulfate attack monitored by microCT and EDXRD: Influence of cement type, water-to-cement ratio and aggregate”, Cement and Concrete Research, Vol. 36 pp. 144-159.

11. ACI Committee 201, “Guide to Durable Concrete (ACI 201.2R-08),” American Concrete Institute, Farmington Hills, MI, 2008, pp. 1-49.

12. ACI 232.2R-18 (2018) ‘Report on the Use of fly ash in concrete’, American Concrete Institute, Farmington Hills, MI, 2018, pp. 1-60

13. Dhole, R., “Sulfate Resistance of High Calcium Fly Ash Concrete,” PhD thesis, University of New Brunswick, Fredericton, NB, Canada, 2010, pp. 1-307.

14. Drimalas, T., “Laboratory and Field Evaluations of External Sulfate Attack,” PhD thesis, University of Texas at Auston, TX, US, 2007, pp. 1-203.

15. Dhole, R.; Thomas, M. D. A.; Folliard, K. J.; and Drimalas, T., “Sulfate Resistance of Mortar Mixtures of High-Calcium Fly Ashes and Other Pozzolans,” ACI Materials Journal, V. 108, No. 6, Nov.-Dec. 2011, pp. 645-654.

16. Freeman, R. B. and Carrasquillo R.L. (1992) “Optimization of the Physical and compositional characteristics of Fly ash cement for the production of sulfate resistant concrete., “Centre for Transportation Research, University of Texas, Austin, Research Report No. 481-8F, pp.509.

17. Thomas, M.D.A. et al. (1999) “Use of ternary cementitious systems containing silica fume and fly ash in concrete,” Cement and Concrete Research, Vol. 29, (a), pp. 1207-1214.

18. Mehta, P. K. (1987) “Scientific basis for determining the sulfate resistance of blended cements,” Symposium on-Fly Ash and Coal Conversion By-Products: Characterization, Utilization and Disposal IV, Materials Research Society Vol.113, pp. 145-152.

19. Wee, T. H., Suryavanshi, A.K., Wong, S.F., Rahman, A. K. (2000) Sulfate Resistance of Concrete Containing Mineral admixtures, ACI Materials Journal, Vol. 97, No. 5, pp. 536-549.

20. Hanson, W.C., (1976) ‘A discussion on the paper – Scanning Micrographic Studies of Ettringite Formation by P.K. Mehta’, Cement and Concrete Research, Vol. 6, pp. 595-596.

21. Odler and Abdul-Maula, S. (1984) Possibilities of quantitative determination of the AFt-(ettringite) and AFm-(monosulphate) phases in hydrated cement pastes, Cement Concrete Research, Vol 14, no.1, pp. 134 -141.

22. Shashiprakash, S. G. and Thomas, M. D. A. (2001) Sulfate resistance of mortars containing high-calcium fly ashes and combinations of highly reactive pozzolans and fly ash, Seventh CANMET/ACI International Conference on Fly Ash, Silica Fume, Slag, and Natural Pozzolans in Concrete, American Concrete Institute SP 199, Vol.1, pp. 221-231.

23. ASTM C 1012 (2004), “Standard Test Method for Length Change of Hydraulic-Cement Mortars Exposed to a Sulfate Solution,” ASTM International, West Conshohocken, PA.