Investigating the Potential of Limestone and Calcined Clay as a Substitute for Fly Ash in Strain-Hardening Cementitious Composites (SHCC)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Investigating the Potential of Limestone and Calcined Clay as a Substitute for Fly Ash in Strain-Hardening Cementitious Composites (SHCC)

Author(s): Ameer Hamza Ahmed, Marco Liebscher, Cesare Signorini and Viktor Mechtcherine

Publication: Symposium Paper

Volume: 362

Issue:

Appears on pages(s): 321-330

Keywords: calcined clays, fly ash, limestone calcined clay cement (LC3), multiple cracking, polyethylene (PE) fibers, strain-hardening cementitious composites (SHCC), supplementary cementitious materials (SCMs)

DOI: 10.14359/51740893

Date: 6/6/2024

Abstract:
This study focuses on the feasibility of replacing fly ash with limestone and calcined clay in strain-hardening cementitious composites (SHCC). Three types of composites were considered: a reference one containing fly ash and the other containing two distinct calcined clays (moderate and high metakaolin content) as supplementary cementitious materials (SCM). Mixtures utilized portland cement (PC) with clinker factors of 0.4 and 0.3, reinforced with 2 vol.% high-density polyethylene (HDPE) fibers. At first, the R3 bound water test was carried out to explicitly assess the reactivity of fly ash and the two calcined clays. Subsequently, the compressive and direct tensile behavior of the SHCCs after 28 days of curing age was evaluated. The results revealed that the SHCCs incorporating calcined clays outperformed their counterpart in terms of compressive strength, tensile strength, and ultimate strain, owing to their high pozzolanic activities, and physical properties, particularly their distinct morphologies. Crack analysis conducted through digital image correlation (DIC) highlighted that the SHCCs with calcined clays established a stronger fiber/matrix interface. In conclusion, this research provides valuable insights into the design of ductile SHCC with novel limestone calcined clay cement (LC3), for enhanced sustainability and cost-effectiveness.

Related References:

1. Li, V., 1992, “From Micromechanics to Structural Engineering - The Design of Cementitious Composites for Civil Engineering Applications,” J. Struct. Mech. Earthq. Eng., 10(2), pp. 37–48.

2. Li, V. C., 2003, “On Engineered Cementitious Composites (ECC)- A Review of the Material and Its Applications,” 1(3).

3. Yang, E.-H., Yang, Y., and Li, V., 2007, “Use of High Volumes of Fly Ash to Improve ECC Mechanical Properties and Material Greenness,” ACI Mater. J., 104, pp. 620–628.

4. Antoni, M., Rossen, J., Martirena, F., and Scrivener, K., 2012, “Cement Substitution by a Combination of Metakaolin and Limestone,” Cem. Concr. Res., 42(12), pp. 1579–1589.

5. Badogiannis, E., Kakali, G., and Tsivilis, S., 2005, “Metakaolin as Supplementary Cementitious Material: Optimization of Kaolin to Metakaolin Conversion,” J. Therm. Anal. Calorim., 81(2), pp. 457–462.

6. Avet, F., and Scrivener, K., 2018, “Investigation of the Calcined Kaolinite Content on the Hydration of Limestone Calcined Clay Cement (LC3),” Cem. Concr. Res., 107, pp. 124–135.

7. Curosu, I., Liebscher, M., Mechtcherine, V., Bellmann, C., and Michel, S., 2017, “Tensile Behavior of High-Strength Strain-Hardening Cement-Based Composites (HS-SHCC) Made with High-Performance Polyethylene, Aramid and PBO Fibers,” Cem. Concr. Res., 98, pp. 71–81.

8. Gong, T., Ahmed, A. H., Curosu, I., and Mechtcherine, V., 2020, “Tensile Behavior of Hybrid Fiber Reinforced Composites Made of Strain-Hardening Cement-Based Composites (SHCC) and Carbon Textile,” Constr. Build. Mater., 262, p. 120913.

9. Curosu, I., Ahmed, A. H., Gong, T., and Mechtcherine, V., 2021, “On the Tensile Behavior of High-Strength Strain-Hardening Cement-Based Composites (SHCC) Reinforced with Carbon Textile – Influence of Yarn-SHCC Bond,” ACI Symp. Publ., 345.

10. Curosu, I., Muja, E., Ismailov, M., Ahmed, A. H., Liebscher, M., and Mechtcherine, V., 2022, “An Experimental-Analytical Scale-Linking Study on the Crack-Bridging Mechanisms in Different Types of SHCC in Dependence on Fiber Orientation,” Cem. Concr. Res., 152, p. 106650.

11. 2012, “Dyneema® Fact Sheets by EuroFibers - Issuu” Online. Available: https://issuu.com/eurofibers/docs/name8f0d44. Accessed: 17-May-2023.

12. Koutnik, P., 2019, “Comparison Of Kaolin And Kaolinitic Claystones As Raw Materials For Preparing Meta-Kaolinite-Based Geopolymers,” Ceram. - Silik., pp. 110–123.

13. Wang, L., Ur Rehman, N., Curosu, I., Zhu, Z., Beigh, M. A. B., Liebscher, M., Chen, L., Tsang, D. C. W., Hempel, S., and Mechtcherine, V., 2021, “On the Use of Limestone Calcined Clay Cement (LC3) in High-Strength Strain-Hardening Cement-Based Composites (HS-SHCC),” Cem. Concr. Res., 144, p. 106421.

14. Wang, L., Zhu, Z., Hamza Ahmed, A., Liebscher, M., Zhu, X., and Mechtcherine, V., 2023, “Self-Healing Behavior of High-Strength Strain-Hardening Cement-Based Composites (HS-SHCC) Blended with Limestone Calcined Clay Cement (LC3),” Constr. Build. Mater., 370, p. 130633.

15. “Downloads | EP Power Minerals” Online. Available: https://www.eppowerminerals.com/de/downloads. Accessed: 31-Jul-2023.

16. “Mefisto L05 : ČLUZ a.s.” Online.. Available: https://www.cluz.cz/en/mefisto-l05. Accessed: 31-Jul-2023.

17. Ahmed, A. H., Nune, S., Liebscher, M., Köberle, T., Willomitzer, A., Noack, I., Butler, M., and Mechtcherine, V., 2023, “Exploring the Role of Dilutive Effects on Microstructural Development and Hydration Kinetics of Limestone Calcined Clay Cement (LC3) Made of Low-Grade Raw Materials,” J. Clean. Prod., p. 139438.

18. Avet, F., Snellings, R., Alujas Diaz, A., Ben Haha, M., and Scrivener, K., 2016, “Development of a New Rapid, Relevant and Reliable (R3) Test Method to Evaluate the Pozzolanic Reactivity of Calcined Kaolinitic Clays,” Cem. Concr. Res., 85, pp. 1–11.

19. Avet, F., Li, X., Ben Haha, M., Bernal, S. A., Bishnoi, S., Cizer, Ö., Cyr, M., Dolenec, S., Durdzinski, P., Haufe, J., Hooton, D., Juenger, M. C. G., Kamali-Bernard, S., Londono-Zuluaga, D., Marsh, A. T. M., Marroccoli, M., Mrak, M., Parashar, A., Patapy, C., Pedersen, M., Provis, J. L., Sabio, S., Schulze, S., Snellings, R., Telesca, A., Thomas, M., Vargas, F., Vollpracht, A., Walkley, B., Winnefeld, F., Ye, G.,

Zhang, S., and Scrivener, K., 2022, “Report of RILEM TC 267-TRM Phase 2: Optimization and Testing of the Robustness of the R3 Reactivity Tests for Supplementary Cementitious Materials,” Mater. Struct., 55(3), p. 92.

20. Ahmed, A. H., Liebscher, M., and Mechtcherine, V., 2023, “Mechanical Performance of Strain Hardening Limestone Calcined Clay Cementitious Composites (SHLC4) Subject to Wet-Dry Cycles,” Strain Hardening Cementitious Composites, M. Kunieda, T. Kanakubo, T. Kanda, and K. Kobayashi, eds., Springer International Publishing, Cham, pp. 3–12.

21. Swamy, R. N., Ali, S. a. R., and Theodorakopoulos, D. D., 1983, “Early Strength Fly Ash Concrete for Structural Applications,” J Am Concr Inst U. S., 80:5.

22. Zunino, F., and Scrivener, K., 2019, “The Influence of the Filler Effect on the Sulfate Requirement of Blended Cements,” Cem. Concr. Res., 126, p. 105918.

23. Yu, J., and Leung, C. K. Y., 2017, “Strength Improvement of Strain-Hardening Cementitious Composites with Ultrahigh-Volume Fly Ash,” J. Mater. Civ. Eng., 29(9), p. 05017003.

24. Yu, J., Wu, H.-L., and Leung, C. K. Y., 2020, “Feasibility of Using Ultrahigh-Volume Limestone-Calcined Clay Blend to Develop Sustainable Medium-Strength Engineered Cementitious Composites (ECC),” J. Clean. Prod., 262, p. 121343.

25.Wang, S., 2005, Micromechanics Based Matrix Design for Engineered Cementitious Composites, University of Michigan.

26. BS EN 206, 2013, “BS EN 206: Concrete. Specification, Performance, Production and Conformity,” Httpswwwen-Stand. Online.. Available: https://www.en-standard.eu/bs-en-206-2013-a2-2021-concretespecification-performance-production-and-conformity/. Accessed: 13-Jul-2023..

27. Lam, L., Wong, Y. L., and Poon, C. S., 2000, “Degree of Hydration and Gel/Space Ratio of High-Volume Fly Ash/Cement Systems,” Cem. Concr. Res., 30(5), pp. 747–756.

28. Curosu, I., Mechtcherine, V., and Millon, O., 2016, “Effect of Fiber Properties and Matrix Composition on the Tensile Behavior of Strain-Hardening Cement-Based Composites (SHCCs) Subject to Impact Loading,” Cem. Concr. Res., 82, pp. 23–35.

29. Curosu, I., Mechtcherine, V., Forni, D., and Cadoni, E., 2017, “Performance of Various Strain-Hardening Cement-Based Composites (SHCC) Subject to Uniaxial Impact Tensile Loading,” Cem. Concr. Res., 102, pp. 16–28.

30. Huang, B. T., Zhu, J., Weng, K.-F., and Li, V., 2022, “Ultra-High-Strength Engineered/Strain-Hardening Cementitious Composites (ECC/SHCC): Material Design and Effect of Fiber Hybridization,” Cem. Concr. Compos., 129, p. 104464.

31. Ranade, R., Li, V., Stults, M. D., Heard, W., and Rushing, T., 2013, “Composite Properties of High-Strength, High-Ductility Concrete,” ACI Mater. J., 110, pp. 413–422.

32. Berodier, E., and Scrivener, K., 2015, “Evolution of Pore Structure in Blended Systems,” Cem. Concr. Res., 73, pp. 25–35.

33. Zunino, F., and Scrivener, K., 2021, “The Reaction between Metakaolin and Limestone and Its Effect in Porosity Refinement and Mechanical Properties,” Cem. Concr. Res., 140, p. 106307.

34. Leung, C. K. Y., and Geng, Y., 1995, “Effect of Lateral Stresses on Fiber Debonding/Pull-Out,” Compos. Eng., 5(10), pp. 1331–1348.

35.Ma, J., Wang, D., Zhao, S., Duan, P., and Yang, S., 2021, “Influence of Particle Morphology of Ground Fly Ash on the Fluidity and Strength of Cement Paste,” Materials, 14(2), p. 283.

36. Krishnan, S., Dhoopadahalli, G., and Bishnoi, S., 2020, “Why Low-Grade Calcined Clays Are the Ideal for the Production of Limestone Calcined Clay Cement (LC3),” pp. 125–130.

37. Sharma, M., Bishnoi, S., Martirena, F., and Scrivener, K., 2021, “Limestone Calcined Clay Cement and Concrete: A State-of-the-Art Review,” Cem. Concr. Res., 149, p. 106564.