Title: High-Strength Headed Bars in Joints of Special Moment Frames under Cyclic Loading

Author(s): H.-J. Lee, F.-C. Yu, K.-C. Lin, J.-C. Wang, B. L. Worsfold, and J. F. Silva

Publication: Structural Journal

Volume: 121

Issue: 6

Appears on pages(s): 105-120

Keywords: anchorage; beam-column joint; development length; headed bars; high-strength reinforcement; joint shear; reversed cyclic loading

DOI: 10.14359/51740866

Date: 11/1/2024

Abstract:
This paper presents cyclic test results of nine beam-column joints, fabricated with Grades 60, 80, and 100 (Grades 420, 550, and 690) No. 11 (D36) headed bars in joints with matching concrete strengths. With the exception of the joint shear determination, each specimen was designed in accordance with ACI 318-14 provisions for special moment frame joints. The headed bar embedment length was determined using 1.0fy in accordance with ACI 318-14, rather than the ACI 318-19 requirement to use 1.25fy to calculate the development length. Test results demonstrate that the ACI 318-14 development length can be used for closely spaced high-strength No. 11 (D36) headed bars in joints with Code-conforming transverse reinforcement. This paper also aggregates the test data with prior research and compares the data with descriptive equations and breakout methodology for assessing the development length and anchorage strength of headed bars. The results support several design recommendations for the ACI 318 provisions.