Experimental Study on Scale Effect of Eccentrically Compressed Reinforced Concrete Columns Strengthened with Carbon Fiber-Reinforced Polymer

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Study on Scale Effect of Eccentrically Compressed Reinforced Concrete Columns Strengthened with Carbon Fiber-Reinforced Polymer

Author(s): Jianhui Si, Yuan Zhou, Zhaobao Zeng, Kai Li, Jiannan Hu, Zewei Liu, and Xinchao Ding

Publication: Structural Journal

Volume: 121

Issue: 5

Appears on pages(s): 77-87

Keywords: carbon fiber-reinforced polymer (CFRP) strengthened columns; reinforced concrete square column; size effect; small eccentric compression

DOI: 10.14359/51740854

Date: 9/1/2024

Abstract:
Strictly following the similarity principle of specimen size, eccentricity, and carbon fiber-reinforced polymer (CFRP) strengthening layers, three groups of reinforced concrete square columns with different scales were designed. Experimental studies on eccentric compression of unstrengthened columns and CFRP-strengthened columns were carried out. The failure characteristics of specimens of various sizes were obtained, as well as the bearing capacity, ductility coefficient, lateral deflection, CFRP, and steel bar strain were analyzed. The test results showed an improved ductility, stiffness, and bearing capacity of eccentrically compressed reinforced concrete columns, strengthened with CFRP. However, the strengthening effect is inversely proportional to the size of the specimen and has a more obvious size effect.

Related References:

1. Teng, J. G.; Chen, J. F.; Smith, S. T.; and Lam, L., FRP Strengthened RC Structures, John Wiley & Sons, Inc., New York, 2012.

2. Zhou, Y.; Chen, X.; Wang, X.; Sui, L.; Huang, X.; Guo, M.; and Hu, B., “Seismic Performance of Large Rupture Strain FRP Retrofitted RC Columns with Corroded Steel Reinforcement,” Engineering Structures, V. 216, 2020, p. 110744. doi: 10.1016/j.engstruct.2020.110744

3. Wang, D.; Wang, Z.; Smith, S. T.; and Yu, T., “Seismic Performance of CFRP-Confined Circular High-Strength Concrete Columns with High Axial Compression Ratio,” Construction and Building Materials, V. 134, 2017, pp. 91-103. doi: 10.1016/j.conbuildmat.2016.12.108

4. Moghtadernejad, N.; Jamshidi, M.; Maheri, M. R.; and Keong, C. K., “Repair of Post-Heated Short Rectangular Reinforced Concrete Columns with FRP Jackets,” V. 34, Structures, 2021, pp. 4269-4283.

5. Mohammed, A. A.; Manalo, A. C.; Ferdous, W.; Zhuge, Y.; Vijay, P. V.; and Pettigrew, J., “Experimental and Numerical Evaluations on the Behaviour of Structures Repaired Using Prefabricated FRP Composites Jacket,” Engineering Structures, V. 210, 2020.

6. Zhao, J.; Si, C.; Ren, W.; Zhang, X.; and Sun, Y., “Experimental and Numerical Studies on Seismic Performance of Rectangular Concrete Columns Reinforced by CFRP Bars with Different Ratios and Positions,” Structures, V. 32, 2021, pp. 237-253.

7. Yan, L., and Chouw, N., “Natural FRP Tube Confined Fibre Reinforced Concrete under Pure Axial Compression: A Comparison with Glass/Carbon FRP,” Thin-Walled Structures, V. 82, 2014, pp. 159-169. doi: 10.1016/j.tws.2014.04.013

8. Widiarsa, I. B. R., and Hadi, M. N. S., “Performance of CFRP Wrapped Square Reinforced Concrete Columns Subjected to Eccentric Loading,” Procedia Engineering, V. 54, 2013, pp. 365-376.

9. Kusumawardaningsih, Y., and Hadi, M. N. S., “Comparative Behaviour of Hollow Columns Confined with FRP Composites,” Composite Structures, V. 93, No. 1, 2010, pp. 198-205.

10. Nematzadeh, M.; Mousavimehr, M.; Shayanfar, J.; and Omidalizadeh, M., “Eccentric Compressive Behavior of Steel Fiber-Reinforced RC Columns Strengthened with CFRP Wraps: Experimental Investigation and Analytical Modeling,” Engineering Structures, V. 226, 2021, Article No. 111389.

11. Lin, G.; Zeng, J. J.; Teng, J. G.; and Li, L. J., “Behavior of Large-Scale FRP-Confined Rectangular RC Columns under Eccentric Compression,” Engineering Structures, V. 216, 2020, p. 110759. doi: 10.1016/j.engstruct.2020.110759

12. Lam, L.; Huang, L.; Xie, J.-H.; and Chen, J.-F., “Compressive Behavior of Ultra-High Performance Concrete Confined with FRP,” Composite Structures, V. 274, 2021, p. 274.

13. Al-Rousan, R., “Behavior of Circular Reinforced Concrete Columns Confined with CFRP Composites,” Procedia Manufacturing, V. 44, 2020, pp. 623-630. doi: 10.1016/j.promfg.2020.02.247

14. Qiang, W.; Bailin, L. I.; Lu, C.; and Zhang, Z., “Square Column When the Loss of Prestress of Prestressed CFRP Reinforced Concrete,” Building Science, V. 4, No. 3, 2020, pp. 57-64.

15. Feng, L.; Ying, L.; and Lujian, T., “Analysis and Finite Element Simulation of Mechanical Properties of Prestressed Carbon Fiber Reinforced Concrete Rectangular Bias Columns,” Engineering Construction, V. 49, No. 9, 2017, pp. 14-20.

16. Donghui, C., and Yanhong, Y., Journal of Building Science and Engineering, V. 34, No. 4, 2017, pp. 34-40.

17. Lu, C.; Wei, F.; Wang, Q.; Liu, C.; and Li, Z., “Experimental Study on Axial Compression Performance of Reinforced Concrete Short Square Section Columns Reinforced with Prestressed Carbon Fiber Cladding,” Industrial Building, V. 47, No. 5, 2017, pp. 171-178.

18. Donghui, C.; Yannan, Y.; and Xu, Y., Journal of Building Science and Engineering, 2013, V. 30, No. 1, pp. 25-31.

19. Zhai, A.; Sun, M.; Ji, C.; Chen, S.; and Wang, C., Journal of Hydraulic and Building Engineering, 2013, V. 11, No. 1, pp. 31-36.

20. Lu, C.-L.; Xiao, Y.-P.; Wang, Q.; and Zhu, W.-X., “Study on Axial Compressive Properties of RC Square Columns Strengthened with Prestressed CFRP Sheets, Structures, V. 27, 2020, pp. 2011-2024.

21. Wang, Q.; Lv, J.; Lu, C.; and Zhu, W., “Experimental Study on Seismic Performance of Square RC Columns Strengthened with Multi-Layer Prestressed CFRP Fabric,” Journal of Building Engineering, V. 45, 2022, pp. 45.

22. Janke, L.; Czaderski, C.; Ruth, J.; and Motavalli, M., “Experiments on the Residual Load-Bearing Capacity of Prestressed Confined Concrete Columns,” Engineering Structures, V. 31, No. 10, 2009, pp. 2247-2256. doi: 10.1016/j.engstruct.2009.04.006

23. Guo, Y.-C.; Gao, W.-Y.; Zeng, J.-J.; Duan, Z.-J.; Ni, X.-Y.; and Peng, K.-D., “Compressive Behavior of FRP Ring-Confined Concrete in Circular Columns: Effects of Specimen Size and a New Design-Oriented Stress-Strain Model,” Construction and Building Materials, V. 201, 2019, pp. 350-368. doi: 10.1016/j.conbuildmat.2018.12.183

24. Zhou, J.; Bi, F.; Wang, Z.; and Zhang, J., “Experimental Investigation of Size Effect on Mechanical Properties of Carbon Fiber Reinforced Polymer (CFRP) Confined Concrete Circular Specimens,” Construction and Building Materials, V. 127, 2016, pp. 643-652. doi: 10.1016/j.conbuildmat.2016.10.039

25. Zhou, C.; Siha, A.; Qiu, Y.; and Pan, Q., “Experimental Investigation of Axial Compressive Behavior of Large-Scale Circular Concrete Columns Confined by Prestressed CFRP Strips,” Journal of Structural Engineering, ASCE, V. 145, No. 8, 2019, p. 04019070. doi: 10.1061/(ASCE)ST.1943-541X.0002351

26. Wang, D. Y.; Wang, Z. Y.; Smith, S. T.; and Yu, T., “Size Effect on Axial Stress-Strain Behavior of CFRP-Confined Square Concrete Columns,” Construction and Building Materials, V. 118, 2016, pp. 116-126. doi: 10.1016/j.conbuildmat.2016.04.158

27. Jin, L.; Chen, H.; Wang, Z.; and Du, X., “Size Effect on Axial Compressive Failure of CFRP-Wrapped Square Concrete Columns: Tests and Simulations,” Composite Structures, V. 254, 2020, p. 254 doi: 10.1016/j.compstruct.2020.112843

28. GB 50010-2010, “Code for Design of Concrete Structures,” Ministry of Housing and Urban-Rural Development of the People’s Republic of China, Beijing, China, 2010.

29. GB/T 50152-2012, “Standard Test Method for Concrete Structures,” Ministry of Housing and Urban-Rural Development of the People’s Republic of China, Beijing, China, 2012.

30. GB 50608-2010, “Technical Code for Infrastructure Application of FRP Composites,” Ministry of Housing and Urban-Rural Development of the People’s Republic of China, Beijing, China, 2010.

31. Jiaru, Q.; Lirong, C.; and Dongliang, Z., “Concrete Column Stirrup Constraint at the Center of the Compression Performance,” Journal of Tsinghua University, Natural Science Edition, 2002, pp. 1369-1373.


ALSO AVAILABLE IN:

Electronic Structural Journal