Horizontal Shear Capacity of Composite T-Beams Reinforced with Glass Fiber-Reinforced Polymer Interface Shear Reinforcement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Horizontal Shear Capacity of Composite T-Beams Reinforced with Glass Fiber-Reinforced Polymer Interface Shear Reinforcement

Author(s): Moataz Mahmoud, Mohamed Eladawy, Basil Ibrahim, and Brahim Benmokrane

Publication: Structural Journal

Volume: 121

Issue: 4

Appears on pages(s): 225-236

Keywords: analytical equations; composite reinforced concrete T-beam; crack pattern; design codes; glass fiber-reinforced polymer (GFRP) bars; interface shear stress; reinforced concrete; shear reinforcement and connectors; shear stress and slip

DOI: 10.14359/51740718

Date: 7/1/2024

Abstract:
Composite construction has proven to be cost-effective, as this method merges precast and cast-in-place elements while preserving the effectiveness and seamless nature of monolithic construction. There are no experimental research results on the behavior of glass fiber-reinforced polymer (GFRP)-reinforced composite beams in the case of horizontal shear transfer in composite T-beams. This research aims to investigate a novel and sustainable approach using noncorroding GFRP as shear-transfer reinforcement in composite reinforced concrete (RC) T-beams. A total of six fullscale RC T-beams (one monolithic RC beam and five composite RC beams) measuring 4200 mm (165.4 in.) in length, 420 mm (16.5 in.) in depth, and 250 mm (9.8 in.) in width were constructed and tested until failure. The main experimental variables evaluated were shear reinforcement type (GFRP or steel stirrups); ratio (0.32, 0.35, or 0.48%), and shape (stirrups or bent bars). The test results were analyzed in terms of ultimate horizontal shear stress, deflection, slippage, and reinforcement strain. The experimental results indicate that the GFRP shear reinforcement provided adequate shear transfer capacities compared to steel when provided across rough concrete interfaces. Moreover, the test results show that increasing the shear reinforcement ratio enhanced the performance of the composite RC T-beams in terms of horizontal shear capacity and slip. Furthermore, the available equations specified in design provisions, such as CAN/CSA S6-19 (2019) and AASHTO LRFD (2018), exhibited unduly conservative predictions of the interface shear strength of the GFRP bars. The results of this study unequivocally establish the viability and promise of employing GFRP bars as shear connectors in composite T-beam applications.

Related References:

AASHTO, 2018, “AASHTO LRFD Bridge Design Specifications for GFRP-Reinforced Concrete,” second edition, American Association of State Highway Transportation Officials, Washington, DC, 14 pp.

ACI Committee 318, 2019, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19) (Reapproved 2022),” American Concrete Institute, Farmington Hills, MI, 624 pp.

ACI Committee 440, 2015, “Guide for the Design and Construction of Structural Concrete Reinforced with Fiber-Reinforced Polymer (FRP) Bars (ACI 440.1R-15),” American Concrete Institute, Farmington Hills, MI, 88 pp.

ACI Committee 440, 2022, “Building Code Requirements for Structural Concrete Reinforced with Glass Fiber-Reinforced Polymer (GFRP) Bars—Code and Commentary (ACI CODE-440.11-22),” American Concrete Insti­tute, Farmington Hills, MI, 260 pp.

Ali, A. H.; Mohamed, H. M.; and Benmokrane, B., 2020, “Bar Size Effect on Long-Term Durability of Sand-Coated Basalt-FRP Composite Bars,” Composites Part B: Engineering, V. 195, p. 108059. doi: 10.1016/j.compositesb.2020.108059

Aljada, B., and El-Salakawy, E., 2023, “Performance of GFRP Bars as Friction Shear Reinforcement in Concrete Composite Elements,” Proceeding of the Canadian Society of Civil Engineering Annual Conference, Singapore, Springer Nature Singapore.

Alkatan, J., 2016, “FRP Shear Transfer Reinforcement for Composite Concrete Construction,” doctoral dissertation, University of Windsor, Windsor, ON, Canada.

Alruwaili, M. S., 2018, “Shear Transfer Mechanism in FRP Reinforced Composite Concrete Structures,” doctoral dissertation, University of Windsor, Windsor, ON, Canada.

ASTM D7205/D7205M-21, 2021, “Standard Test Method for Tensile Properties of Fiber Reinforced Polymer Matrix Composite Bars,” ASTM International, West Conshohocken, PA, 13 pp.

Bass, R. A.; Carrasquillo, R. L.; and Jirsa, J. O., 1989, “Shear Transfer Across New and Existing Concrete Interfaces,” ACI Structural Journal, V. 86, No. 4, July-Aug., pp. 383-393.

Bazli, M., and Abolfazli, M., 2020, “Mechanical Properties of Fibre Reinforced Polymers Under Elevated Temperatures: An Overview,” Polymers, V. 12, No. 11, p. 2600. doi: 10.3390/polym12112600

Benmokrane, B.; Hassan, M.; Robert, M.; Vijay, P. V.; and Manalo, A., 2020, “Effect of Different Constituent Fiber, Resin, and Sizing Combinations on Alkaline Resistance of Basalt, Carbon, and Glass FRP Bars,” Journal of Composites for Construction, ASCE, V. 24, No. 3, p. 04020010. doi: 10.1061/(ASCE)CC.1943-5614.0001009

Benmokrane, B., and Rahman, H., 1998, Durability of Fiber Reinforced Polymer (FRP) Composites for Construction,” Proceedings of the First International Conference on Durability of FRP Composites for Construction, Sherbrooke, QC, Canada, 706 pp.

Birkeland, P. W., and Birkeland, H. W., 1966, “Connections in Precast Concrete Construction,” ACI Journal Proceedings, V. 63, No. 3, Mar., pp. 345-368.

Bryson, J., and Carpenter, E. F., 1970, “Flexural Behavior of Prestressed Concrete Composite Tee-Beams,” US National Bureau of Standards.

CAN/CSA S6-19, 2019, “Canadian Highway Bridge Design Code,” CSA Group, Toronto, ON, Canada.

CAN/CSA S807-19, 2019, “Specification for Fiber-Reinforced Polymers,” CSA Group, Toronto, ON, Canada.

Cheong, Y. W.; Kwan, H. P.; and Hariyanto, A. D., 2005, “Quality Control in Precast Production, A Case Study on Tunnel Segment Manufacture,” Journal of Architecture and Built Environment, V. 33, No. 2

Connor, A. B., and Kim, Y. H., 2016, “Shear-Transfer Mechanisms for Glass Fiber-Reinforced Polymer Reinforcing Bars,” ACI Structural Journal, V. 113, No. 6, Nov-Dec., pp. 1369-1380. doi: 10.14359/51689034

Duo, Y.; Liu, X.; Liu, Y.; Tafsirojjaman, T.; and Sabbrojjaman, M., 2021, “Environmental Impact on the Durability of FRP Reinforcing Bars,” Journal of Building Engineering, V. 43, p. 102909. doi: 10.1016/j.jobe.2021.102909

Fang, Z.; Jiang, H.; Liu, A.; Feng, J.; and Chen, Y., 2018, “Horizontal Shear Behaviors of Normal Weight and Lightweight Concrete Composite T-Beams,” International Journal of Concrete Structures and Materials, V. 12, No. 1, pp. 1-21. doi: 10.1186/s40069-018-0274-3

Feng, G.; Zhu, D.; Guo, S.; Rahman, M. Z.; Jin, Z.; and Shi, C., 2022, “A Review on Mechanical Properties and Deterioration Mechanisms of FRP Bars Under Severe Environmental and Loading Conditions,” Cement and Concrete Composites, V. 134, p. 104758. doi: 10.1016/j.cemconcomp.2022.104758

Halicka, A., and Jabłoński, Ł., 2016, “Shear Failure Mechanism of Composite Concrete T-Shaped Beams,” Proceedings of the Institution of Civil Engineers – Structures and Buildings, V. 169, No. 1, pp. 67-75. doi: 10.1680/stbu.14.00127

Hanson, N. W., 1960, “Precast-Prestressed Concrete Bridges 2: Horizontal Shear Connections,” Research and Development Laboratories, Portland Cement Association, Skokie, IL, pp. 38-58.

Harries, K. A.; Zeno, G.; and Shahrooz, B., 2012, “Toward an Improved Understanding of Shear-Friction Behavior,” ACI Structural Journal, V. 109, No. 6, Nov.-Dec., pp. 835-844

Lang, M. W., 2011, “Analysis of the AASHTO LFRD Horizontal Shear Strength Equation,” doctoral dissertation, Virginia Polytechnic Institute and State University, Blacksburg, VA.

Mahmoud, M. A.; Elafandy, T. H.; Okail, H. O.; and Abdelrahman, A. A., 2014, “Interfacial Shear Behavior of Composite Flanged Concrete Beams,” HBRC Journal, V. 10, No. 2, pp. 206-214. doi: 10.1016/j.hbrcj.2013.11.001

Manalo, A.; Maranan, G.; Benmokrane, B.; Cousin, P.; Alajarmeh, O.; and Ferdous, W., Liang, R.; andHota, G., 2020, “Comparative Durability of GFRP Composite Reinforcing Bars in Concrete and in Simulated Concrete Environments,” Cement and Concrete Composites, V. 109, p. 103564. doi: 10.1016/j.cemconcomp.2020.103564

Mattock, A. H., 1974, “Shear Transfer in Concrete Having Reinforcement at an Angle to the Shear Plane,” Shear in Reinforced Concrete, SP-42, American Concrete Institute, Farmington Hills, MI, pp. 17-42.

Mattock, A. H.; Li, W. K.; and Wang, T. C., 1976, “Shear Transfer in Lightweight Reinforced Concrete,” PCI Journal, V. 21, No. 1, pp. 20-39. doi: 10.15554/pcij.01011976.20.39

Mohamed, H. M., and Benmokrane, B., 2015, “Torsion Behavior of Concrete Beams Reinforced with Glass Fiber-Reinforced Polymer Bars and Stirrups,” ACI Structural Journal, V. 112, No. 5, Sept.-Oct., pp. 543-552.doi: 10.14359/51687824

Mohamed, H. M., and Benmokrane, B., 2016, “Reinforced Concrete Beams With and Without FRP Web Reinforcement Under Pure Torsion,” Journal of Bridge Engineering, ASCE, V. 21, No. 3, p. 04015070. doi: 10.1061/(ASCE)BE.1943-5592.0000839

Mufti, A.; Onofrei, M.; Benmokrane, B.; Banthia, N.; Boulfiza, M.; Newhook, J.; Bakht, B.; Tadros, G.; and Brett, P., 2005, “Durability of GFRP Reinforced Concrete in Field Structures,” Proceedings of the 7th International Conference on Fiber-Reinforced Polymer Reinforcement for Reinforced Concrete Structures, Kansas City, MO.

Oh, Y. H., and Moon, J. H., 2021, “Evaluation of Design Provisions for Horizontal Shear Strength in Composite Precast Concrete Beams with Different Interface Conditions,” Applied Sciences, Basel, Switzerland, V. 11, No. 9, p. 4246. doi: 10.3390/app11094246

Pan, Y., and Yan, D., 2021, “Study on the Durability of GFRP Bars and Carbon/Glass Hybrid Fiber Reinforced Polymer (HFRP) Bars Aged in Alkaline Solution,” Composite Structures, V. 261, p. 113285. doi: 10.1016/j.compstruct.2020.113285

Patnaik, A. K., 2001, “Behavior of Composite Concrete Beams with Smooth Interface,” Journal of Structural Engineering, ASCE, V. 127, No. 4, pp. 359-366. doi: 10.1061/(ASCE)0733-9445(2001)127:4(359)

Pultrall, 2019, “V-ROD Glass Fiber Reinforced Polymer (GFRP) Technical Data Sheet.” Thetford Mines, Canada, https://fiberglassrebar.com/technical-data-sheets/. (last accessed June 11, 2024)

Solyom, S., and Balázs, G. L., 2020, “Bond of FRP Bars with Different Surface Characteristics,” Construction and Building Materials, V. 264, p. 119839. doi: 10.1016/j.conbuildmat.2020.119839

Tomlinson, D., and Fam, A., 2014, “Experimental Investigation of Precast Concrete Insulated Sandwich Panels with Glass Fiber-Reinforced Polymer Shear Connectors,” ACI Structural Journal, V. 111, No. 3, May-June, pp. 595-606. doi: 10.14359/51686621

Wairaven, J.; Frenay, J.; and Pruijssers, A., 1987, “Influence of Concrete Strength and Load History on the Shear Friction Capacity of Concrete Members,” PCI Journal, V. 32, No. 1, pp. 66-84. doi: 10.15554/pcij.01011987.66.84

Wang, Z.; Zhao, X. L.; Xian, G.; and Wu, G., SinghRaman, S.; Al-Saadi, S.; and Haque, A., 2017, “Long-Term Durability of Basalt-and Glass-Fibre Reinforced Polymer (BFRP/GFRP) Bars in Seawater and Sea Sand Concrete Environment,” Construction and Building Materials, V. 139, pp. 467-489. doi: 10.1016/j.conbuildmat.2017.02.038

Woltman, G.; Tomlinson, D.; and Fam, A., 2013, “Investigation of Various GFRP Shear Connectors for Insulated Precast Concrete Sandwich Wall Panels,” Journal of Composites for Construction, ASCE, V. 17, No. 5, pp. 711-721. doi: 10.1061/(ASCE)CC.1943-5614.0000373

Zhang, B.; Masmoudi, R.; and Benmokrane, B., 2004, “Behaviour of One-Way Concrete Slabs Reinforced with CFRP Grid Reinforcement,” Construction and Building Materials, V. 18, No. 3, pp. 625-635. doi: 10.1016/j.conbuildmat.2004.04.007


ALSO AVAILABLE IN:

Electronic Structural Journal