Experimental Investigation of Dapped Ends with Diagonal Reinforcement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Investigation of Dapped Ends with Diagonal Reinforcement

Author(s): Chathura Rajapakse, Herve Degee, and Boyan Mihaylov

Publication: Structural Journal

Volume: 121

Issue: 4

Appears on pages(s): 35-46

Keywords: dapped-end connections; diagonal reinforcement layout; flexural failures; reentrant corner cracks; shear failures

DOI: 10.14359/51740710

Date: 7/1/2024

Abstract:
Reinforced concrete dapped-end connections are susceptible to formation of inclined cracks at the reentrant corner under service conditions. As these connections also work with high shear stresses, they require a high amount of reinforcement to ensure sufficient load-bearing capacity. To deepen the understanding of this topic, an experimental campaign of eight large-scale dapped-end connections featuring diagonal reinforcement is presented. These specimens, which are among the largest available in the literature, are similar in size to the dapped ends typically used in bridges. The test series captures both flexural and shear failures of dapped ends. The crack displacements, crack patterns, and elongation of main reinforcement are reported, with 56 continuous measurements of deformations. The test results of this study are used in conjunction with a similar study on specimens with orthogonal reinforcement to investigate the impact of reinforcement layout. For the same amount of dapped-end reinforcement, specimens with diagonal reinforcement are considerably stronger than the corresponding connections with orthogonal reinforcement. For both reinforcement layouts, the crack widths exceeded typical code provisions under service conditions.

Related References:

1. Schlaich, J., and Schafer, K., “Design and Detailing of Structural Concrete Using Strut-and-Tie Models,” Structural Engineering, V. 69, No. 6, 1991, pp. 113-125.

2. Desnerck, P.; Lees, J. M.; and Morley, C. T., “Impact of the Reinforcement Layout on the Load Capacity of Reinforced Concrete Half-Joints,” Engineering Structures, V. 127, 2016, pp. 227-239. doi: 10.1016/j.engstruct.2016.08.061

3. Schlaich, J.; Schäfer, K.; and Jennewein, M., “Toward a Consistent Design of Structural Concrete,” PCI Journal, V. 32, No. 3, 1987, pp. 74-150. doi: 10.15554/pcij.05011987.74.150

4. Cook, W. D., and Mitchell, D., “Studies of Disturbed Regions Near Discontinuities in Reinforced Concrete Members,” ACI Structural Journal, V. 85, No. 2, Mar.-Apr. 1988, pp. 206-216. doi: 10.14359/2772

5. Mata-Falcón, J.; Pallarés, L.; and Miguel, P. F., “Proposal and Experimental Validation of Simplified Strut-and-Tie Models on Dapped-End Beams,” Engineering Structures, V. 183, 2019, pp. 594-609. doi: 10.1016/j.engstruct.2019.01.010

6. Muttoni, A.; Fernández Ruiz, M.; Niketic, F.; and Backes, M.-R., “Assessment of Existing Structures Based on Elastic-Plastic Stress Fields - Modelling of Critical Details and Investigation of the In-Plane Shear Transverse Bending Interaction,” Rapport OFROU, V. 680, 2016, 134 pp.

7. Mata-Falcón, J., “Serviceability and Ultimate Behaviour of Dapped-End Beams (in Spanish: Estudio del Comportamiento en Servicio y Rotura de los Apoyos a Media Madera),” PhD dissertation, Universitat Politècnica de València, València, Spain, 2015.

8. Nagy-György, T.; Sas, G.; Dăescu, A. C.; Barros, J. A.; and Stoian, V., “Experimental and Numerical Assessment of the Effectiveness of FRP-Based Strengthening Configurations for Dapped-End RC Beams,” Engineering Structures, V. 44, 2012, pp. 291-303. doi: 10.1016/j.engstruct.2012.06.006

9. Desnerck, P.; Lees, J. M.; and Morley, C. T., “The Effect of Local Reinforcing Bar Reductions and Anchorage Zone Cracking on the Load Capacity of RC Half-Joints,” Engineering Structures, V. 152, 2017, pp. 865-877. doi: 10.1016/j.engstruct.2017.09.021

10. Herzinger, R., “Stud Reinforcement in Dapped Ends of Concrete Beams,” doctoral thesis, University of Calgary, Calgary, AB, Canada, 2008.

11. Zhu, R. R.; Wanichakorn, W.; Hsu, T. T.; and Vogel, J., “Crack Width Prediction Using Compatibility-Aided Strut-and-Tie Model,” ACI Structural Journal, V. 100, No. 4, July-Aug. 2003, pp. 413-421.

12. Nagrodzka-Godycka, K., and Piotrkowski, P., “Experimental Study of Dapped-End Beams Subjected to Inclined Load,” ACI Structural Journal, V. 109, No. 1, Jan.-Feb. 2012, pp. 11-20. doi: 10.14359/51683489

13. Moreno-Martínez, J. Y., and Meli, R., “Experimental Study on the Structural Behavior of Concrete Dapped-End Beams,” Engineering Structures, V. 75, 2014, pp. 152-163. doi: 10.1016/j.engstruct.2014.05.051

14. Mattock, A. H., and Chan, T. C., “Design and Behavior of Dapped-End Beams,” PCI Journal, V. 24, No. 6, 1979, pp. 28-45. doi: 10.15554/pcij.11011979.28.45

15. Lu, W. Y.; Lin, I. J.; Hwang, S. J.; and Lin, Y. H., “Shear Strength of High-Strength Concrete Dapped-End Beams,” Zhongguo Gongcheng Xuekan, V. 26, No. 5, 2003, pp. 671-680. doi: 10.1080/02533839.2003.9670820

16. Lu, W. Y.; Lin, I. J.; and Yu, H. W., “Behaviour of Reinforced Concrete Dapped-End Beams,” Magazine of Concrete Research, V. 64, No. 9, 2012, pp. 793-805. doi: 10.1680/macr.11.00116

17. Mitchell, D.; Marchand, J.; Croteau, P.; and Cook, W. D., “Concorde Overpass Collapse: Structural Aspects,” Journal of Performance of Constructed Facilities, ASCE, V. 25, No. 6, 2011, pp. 545-553. doi: 10.1061/(ASCE)CF.1943-5509.0000183

18. Mitchell, D.; Cook, W. D.; and Peng, T., “Importance of Reinforcement Detailing,” Further Examples for the Design of Structural Concrete with Strut-and-Tie Models, SP-273, K.-H. Reineck and L. C. Novak, eds., American Concrete Institute, Farmington Hills, MI, 2010, pp. 1-16.

19. Rajapakse, C.; Degée, H.; and Mihaylov, B., “Investigation of Shear and Flexural Failures of Dapped-End Connections with Orthogonal Reinforcement,” Engineering Structures, V. 260, 2022, p. 114233. doi: 10.1016/j.engstruct.2022.114233

20. EN 1992-1-1, “Eurocode 2. Design of Concrete Structures Part 1-1: General Rules and Rules for Buildings,” European Committee for Standardization, Brussels, Belgium, 2004, 225 pp.

21. Mihaylov, B.; Rajapakse, C.; and Berger, P. H., “Effect of Steel Fibers on the Ultimate Flexural Behavior of Dapped-End Connections,” Engineering Structures, V. 259, 2022, p. 114147. doi: 10.1016/j.engstruct.2022.114147

22. Fu, Z., “Use of Fibres and Headed Bars in Dapped End Beams,” MSc dissertation, McGill University, Montreal, QC, Canada, 2004.


ALSO AVAILABLE IN:

Electronic Structural Journal