Actual Applications of 3D-Printing: Chapter 7 of the Emerging Technology Report

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Actual Applications of 3D-Printing: Chapter 7 of the Emerging Technology Report

Author(s): Ferron

Publication: Web Session

Volume: ws_F23_Ferron.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 10/29/2023

Abstract:
This presentation highlights some case studies related to 3D-printing of cementitious mixtures and compares and contrasts commonalities among them and lessons learned. In additions, best practices related to soliciting case studies for ACI documents is presented.