Chapter 4: Materials for 3D Printing

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Chapter 4: Materials for 3D Printing

Author(s): Ouellet-Plamondon

Publication: Web Session

Volume: ws_F23_Ouellet-Plamondon.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 10/29/2023

Abstract:
The material development for 3D-printing and additive construction involves the selection of the binder, the aggregates, and the characterization of the fresh properties of the mixture. Examples of materials for 3D printing will be presented, as well as the key experiments and calculations to develop the mixture. Steps are proposed to test materials for 3D printing, according to the design criteria.