Leveraging Machine Learning to Better Understand Structural Behavior of Concrete Components under Extreme Loads

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Leveraging Machine Learning to Better Understand Structural Behavior of Concrete Components under Extreme Loads

Author(s): Paal

Publication: Web Session

Volume: ws_F23_Paal.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 10/29/2023

Abstract:
Existing physics-based modeling approaches for predicting the seismic response of reinforced concrete frames do not have a good compromise between performance and computational efficiency. High-fidelity models have reasonable predictive performance but are very computationally demanding, while more simplified models lose accuracy but maintain computational efficiency. This presentation will cover recent advances in machine learning-informed prediction of RC components as well as a highly accurate and computationally efficient approach to predicting the performance of RC frames.