Reliability-Based Code Development for Carbon Fiber- Reinforced Polymer-Strengthened Circular Reinforced Concrete Columns

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Reliability-Based Code Development for Carbon Fiber- Reinforced Polymer-Strengthened Circular Reinforced Concrete Columns

Author(s): Juscelina Rosiane Ferreira, Peterson Araujo Quadros, and Sofia Maria Carrato Diniz

Publication: Structural Journal

Volume: 121

Issue: 3

Appears on pages(s): 215-230

Keywords: carbon fiber-reinforced polymer (CFRP) confinement; circular cross sections; design codes; existing structures; reinforced concrete (RC); reliability index; short columns; strengthening

DOI: 10.14359/51740490

Date: 5/1/2024

Abstract:
Concrete confinement using fiber-reinforced polymers (FRPs) has been vastly used for strengthening of reinforced concrete (RC) columns. The strengthening of RC columns belongs to the realm of existing structures, which has been recognized as distinct from the design of new structures. Code development efforts for the strengthening of RC columns should follow a reliability-based framework similar to the one used in the code development for new structures. In this process, a number of additional issues arise: the mechanical model of FRP confinement representing existing RC columns, the statistical description of the design variables, and the target reliability to be attained. In this study, the reliability levels of 288 axially loaded, FRP-RC short columns of circular cross sections, strengthened according to ACI 440 guidelines, are assessed. Monte Carlo simulation is used in the probabilistic description of column strength and computation of the probability of failure. An FRP confinement model that explicitly accounts for the presence of transversal steel and attendant model errors associated to the estimation of ultimate stress and ultimate strain are used in the computation of the FRP-RC column capacity. The values of the reliability index are in the range of 3.92 to 4.61, satisfying the target reliability suggested for both new and existing structures. The research findings presented herein provide further support for the efforts of ACI Committee 440 in the development of standards related to the FRP strengthening of RC columns.

Related References:

ACI Committee 318, 2014, “Building Code Requirements for Reinforced Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 520 pp.

ACI Committee 440, 2017, “Guide for the Design and Construction of Externally Bonded FRP Systems for Strengthening Concrete Structures (ACI 440.2R-17),” American Concrete Institute, Farmington Hills, MI, 112 pp.

ACI Committee 440, 2022, “Building Code Requirements for Structural Concrete Reinforced with Glass Fiber-Reinforced Polymer (GFRP) Bars—Code and Commentary (ACI CODE-440.11-22),” American Concrete Institute, Farmington Hills, MI, 260 pp.

ACI Committee 562, 2016, “Code Requirements for Assessment, Repair, and Rehabilitation of Existing Concrete Structures (ACI 562-16) and Commentary,” American Concrete Institute, Farmington Hills, MI, 88 pp.

Ang, A. H.-S., and Tang, W. H., 1984, Probability Concepts in Engineering Planning and Design: Decision, Risk, and Reliability, John Wiley & Sons, Inc., New York.

ASCE, 2021, “ASCE 2021 Report Card for America’s Infrastructure,” American Society of Civil Engineers, Reston, VA, https://infrastructurereportcard.org/cat-item/bridges-infrastructure/. (last accessed Apr. 1, 2024)

Baji, H., 2017, “Calibration of the FRP Resistance Reduction Factor for FRP-Confined Reinforced Concrete Building Columns,” Journal of Composites for Construction, ASCE, V. 21, No. 3, p. 04016107. doi: 10.1061/(ASCE)CC.1943-5614.0000769

Bartlett, F. M., and MacGregor, J. G., 1995, “Equivalent Specified Concrete Strength from Core Test Data,” Concrete International, V. 17, No. 3, Mar., pp. 52-58.

Casas, J. R., and Chambi, J. L., 2014, “Partial Safety Factors for CFRP-Wrapped Bridge Piers: Model Assessment and Calibration,” Composite Structures, V. 118, pp. 267-283. doi: 10.1016/j.compstruct.2014.07.032

Chastre, C., and Silva, M. A. G., 2010, “Monotonic Axial Behavior & Modelling of RC Circular Columns Confined with CFRP,” Engineering Structures, V. 32, No. 8, pp. 2268-2277. doi: 10.1016/j.engstruct.2010.04.001

Cusson, D., and Paultre, P., 1995, “Stress-Strain Model for Confined High-Strength Concrete,” Journal of Structural Engineering, ASCE, V. 121, No. 3, pp. 468-477. doi: 10.1061/(ASCE)0733-9445(1995)121:3(468)

Diniz, S. M. C., 2008, “Structural Reliability: Rational Tools for Design Code Development,” Structures Congress 2008: Crossing Borders, American Society of Civil Engineers, Reston, VA.

Diniz, S. M. C., and Frangopol, D. M., 1997a, “Reliability Bases for High-Strength Concrete Columns,” Journal of Structural Engineering, ASCE, V. 123, No. 10, pp. 1375-1381. doi: 10.1061/(ASCE)0733-9445(1997)123:10(1375)

Diniz, S. M. C., and Frangopol, D. M., 1997b, “Strength and Ductility Simulation of High-Strength Concrete Columns,” Journal of Structural Engineering, ASCE, V. 123, No. 10, pp. 1365-1374. doi: 10.1061/(ASCE)0733-9445(1997)123:10(1365)

Diniz, S. M. C., and Frangopol, D. M., 1998, “Reliability Assessment of High-Strength Concrete Columns,” Journal of Engineering Mechanics, ASCE, V. 124, No. 5, pp. 529-536. doi: 10.1061/(ASCE)0733-9399(1998)124:5(529)

Eid, R., and Paultre, P., 2008, “Analytical Model for FRP-Confined Circular Reinforced Concrete Columns,” Journal of Composites for Construction, ASCE, V. 12, No. 5, pp. 541-552. doi: 10.1061/(ASCE)1090-0268(2008)12:5(541)

Ferreira, J. R., 2017, “Reliability of Short Circular RC Columns Confined by FRP,” PhD thesis, Federal University of Minas Gerais, Belo Horizonte, Brazil.

Ferreira, J. R., and Diniz, S. M. C., 2018, “Model Uncertainty in the Estimation of the Resistance of Circular Reinforced Concrete Columns Confined by Carbon Fiber Reinforced Polymer,” Structure and Infrastructure Engineering, V. 14, No. 1, pp. 68-88. doi: 10.1080/15732479.2017.1328447

Ferreira, J. R.; Quadros, P. A.; and Diniz, S. M. C., 2018, “Extending the Life-Cycle of Reinforced Concrete Columns by FRP Strengthening,” Structures Congress 2018: Bridges, Transportation Structures, and Nonbuilding Structures, American Society of Civil Engineers, Reston, VA.

fib, 2020, Model Code 2020, International Federation for Structural Concrete, Lausanne, Switzerland.

Galambos, T.; Ellingwood, B.; MacGregor, J.; and Cornell, A., 1982, “Probability Based Load Criteria: Assessment of Current Design Practice,” Journal of Structural Division, ASCE, V. 108, No. 5, pp. 959-977.

Ghosn, M.; Frangopol, D. M.; McAllister, T. P.; Shah, M.; Diniz, S. M. C.; Ellingwood, B. R.; Manuel, L.; Biondini, F.; Catbas, N.; Strauss, A.; and Zhao, X. L., 2016, “Reliability-Based Performance Indicators for Structural Members,” Journal of Structural Engineering, ASCE, V. 142, No. 9, p. 04016002. doi: 10.1061/(ASCE)ST.1943-541X.0001546

ISO 13822:2010, 2010, “Basis for Design of Structures – Assessment of Existing Structures,” International Organization for Standardization, Geneva, Switzerland.

ISO 19338:2014, 2014, “Performance and Assessment Requirements for Design Standards on Structural Concrete,” International Organization for Standardization, Geneva, Switzerland.

Lee, J. Y.; Yi, C. K.; Jeong, H. S.; Kim, S. W.; and Kim, J. K., 2010, “Compressive Response of Concrete Confined with Steel Spirals and FRP Composites,” Journal of Composite Materials, V. 44, No. 4, pp. 481-504. doi: 10.1177/0021998309347568

Melchers, R. E., 2001, “Assessment of Existing Structures-Approaches and Research Needs,” Journal of Structural Engineering, ASCE, V. 127, No. 4, pp. 406-411. doi: 10.1061/(ASCE)0733-9445(2001)127:4(406)

Micelli, F., and Modarelli, R., 2013, “Experimental and Analytical Study on Properties Affecting the Behaviour of FRP-Confined Concrete,” Composites. Part B, Engineering, V. 45, No. 1, pp. 1420-1431. doi: 10.1016/j.compositesb.2012.09.055

Mirza, S. A., and MacGregor, J. G., 1979a, “Variations in the Dimensions of Reinforced Concrete Members,” Journal of the Structural Division, ASCE, V. 105, No. 4, pp. 751-766. doi: 10.1061/JSDEAG.0005132

Mirza, S. A., and MacGregor, J. G., 1979b, “Variability of Mechanical Properties of Reinforcing Bars,” Journal of the Structural Division, ASCE, V. 105, No. 5, pp. 921-937. doi: 10.1061/JSDEAG.0005146

Nowak, A., and Szerszen, M., 2003, “Calibration of Design Code for Buildings (ACI 318): Part 1—Statistical Models for Resistance,” ACI Structural Journal, V. 100, No. 3, May-June, pp. 377-382.

Ozbakkaloglu, T.; Lim, J. C.; and Vincent, T., 2013, “FRP-Confined Concrete in Circular Sections: Review and Assessment of Stress–Strain Models,” Engineering Structures, V. 49, pp. 1068-1088. doi: 10.1016/j.engstruct.2012.06.010

Park, R., and Paulay, T., 1975, Reinforced Concrete Structures, John Wiley & Sons, Inc., New York.

Pellegrino, C., and Modena, C., 2010, “Analytical Model for FRP Confinement of Concrete Columns with and without Internal Steel Reinforcement,” Journal of Composites for Construction, ASCE, V. 14, No. 6, pp. 693-705. doi: 10.1061/(ASCE)CC.1943-5614.0000127

Ribeiro, A. B.; Calixto, J. M. F.; and Diniz, S. M. C., 2016, “Assessment of Epistemic Uncertainties in the Shear Strength of Slender Reinforced Concrete Beams,” Engineering Structures, V. 116, pp. 140-147. doi: 10.1016/j.engstruct.2016.02.045

Saatcioglu, M., and Razvi, S., 1992, “Strength and Ductility of Confined Concrete,” Journal of Structural Engineering, ASCE, V. 118, No. 6, pp. 1590-1607. doi: 10.1061/(ASCE)0733-9445(1992)118:6(1590)

Shirmohammadi, F.; Esmaeily, A.; and Kiaeipour, Z., 2015, “Stress-Strain Model for Circular Concrete Columns Confined by FRP and Conventional Lateral Steel,” Engineering Structures, V. 84, pp. 395-405. doi: 10.1016/j.engstruct.2014.12.005

Steenbergen, R. D. J. M.; Sýkora, M.; Diamantidis, D.; Holický, M.; and Vrouwenvelder, T., 2015, “Economic and Human Safety Reliability Levels for Existing Structures,” Structural Concrete, V. 16, No. 3, pp. 323-332. doi: 10.1002/suco.201500022

Szerszen, M., and Nowak, A., 2003, “Calibration of Design Code for Buildings (ACI 318): Part 2—Reliability Analysis and Resistance Factors,” ACI Structural Journal, V. 100, No. 3, May-June, pp. 383-391.

Val, D. V., 2003, “Reliability of Fiber-Reinforced Polymer-Confined Reinforced Concrete Columns,” Journal of Structural Engineering, ASCE, V. 129, No. 8, pp. 1122-1130. doi: 10.1061/(ASCE)0733-9445(2003)129:8(1122)

Wang, N., and Ellingwood, B. R., 2015, “Limit State Design Criteria for FRP Strengthening of RC Bridge Components,” Structural Safety, V. 56, pp. 1-8. doi: 10.1016/j.strusafe.2015.03.004

Wang, W., and Yang, W., 2010, “Statistical Studies on Material Behavior of CFRP Sheets under Uniaxial Loads and its Application in Reliability Analysis,” 5th International Conference on FRP Composites in Civil Engineering, CICE, Beijing, China.

Wang, Z.; Wang, D.; Smith, S. T.; and Lu, D., 2012, “Experimental Testing and Analytical Modeling of CFRP-Confined Large Circular RC Columns Subjected to Cyclic Axial Compression,” Engineering Structures, V. 40, pp. 64-74. doi: 10.1016/j.engstruct.2012.01.004

Zou, Y., and Hong, H. P., 2011, “Reliability Assessment of FRP-Confined Concrete Columns Designed for Buildings,” Structure and Infrastructure Engineering, V. 7, No. 3, pp. 243-258. doi: 10.1080/15732470802416998


ALSO AVAILABLE IN: