Seismic Performance of Gravity-Load-Designed Beam-Column Joints with Strain-Hardened Cementitious Composite

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Seismic Performance of Gravity-Load-Designed Beam-Column Joints with Strain-Hardened Cementitious Composite

Author(s): B.S. Sindu and Saptarshi Sasmal

Publication: Structural Journal

Volume: 121

Issue: 3

Appears on pages(s): 159-172

Keywords: beam-column (BC) joint; energy dissipation; hysteresis behavior; seismic upgradation; strain-hardened cementitious composite (SHCC)

DOI: 10.14359/51740484

Date: 5/1/2024

Abstract:
Beam-column (BC) joints are crucial components for ensuring the safety of structures during earthquakes. Various standards/ codes (Eurocode 8, ACI 352R-02, and IS 13920:1993) prescribe special reinforcement detailing at the joint region to improve the seismic performance. Although extremely important, execution of the same is challenging due to heavy reinforcement congestion. In this regard, an attempt has been made in this study to develop a strain-hardened, high-performance cementitious composite (SHCC) with improved tension-related performance for seismicresistant BC joints, which can potentially reduce the reinforcement demand. The efficacy of SHCC in improving the gravity-loaddesigned (GLD) BC joints without any additional reinforcement required for ductile detailing is investigated. Full-scale BC joint specimens were developed and subjected to reversed cyclic loading, and the critical seismic performance—such as hysteresis behavior, damage pattern, energy dissipation, shear deformation, and strength/stiffness degradation—were evaluated and compared with GLD specimens with normal concrete. It is observed that the GLD specimens with SHCC at the joint region showed remarkable performance. Without any additional confinement in the joint region, energy dissipation is doubled (100%), and shear deformation is only 40% of the GLD under the same drift demand. The findings of this study will help in developing seismic-resistant BC joints with the minimum reinforcement.

Related References:

1. Calvi, G. M.; Magenes, G.; and Pampanin, S., “Relevance of Beam-Column Joint Damage and Collapse in RC Frame Assessment,” Journal of Earthquake Engineering, V. 6, No. sup001, 2002, pp. 75-100. doi: 10.1080/13632460209350433

2. Sasmal, S.; Novák, B.; Rmanjaneyulu, K.; Roehm, C.; Srinivas, V.; Lakshmanan, N.; and Iyer, N. R., “Upgradation of Gravity Load Designed Subassemblages Subjected to Seismic Type Loading,” Composite Structures, V. 93, No. 6, May 2011, pp. 1561-1573. doi: 10.1016/j.compstruct.2011.01.001

3. Suryanto, B.; Tambusay, A.; Suprobo, P.; Bregoli, G.; and Aitken, M. W., “Seismic Performance of Exterior Beam-Column Joints Constructed with Engineered Cementitious Composite: Comparison with Ordinary and Steel Fibre Reinforced Concrete,” Engineering Structures, V. 250, Jan. 2022, Article No. 113377. doi: 10.1016/j.engstruct.2021.113377

4. AbdelAleem, B. H., and Hassan, A. A. A., “Effect of Combining Steel Fibers with Crumb Rubber on Enhancing the Behavior of Beam-Column Joints under Cyclic Loading,” Engineering Structures, V. 182, Mar. 2019, pp. 510-527. doi: 10.1016/j.engstruct.2018.12.089

5. Esmaeeli, E.; Barros, J. A. O.; Sena-Cruz, J.; Fasan, L.; Li Prizzi, F. R.; Melo, J.; and Varum, H., “Retrofitting of Interior RC Beam–Column Joints Using CFRP Strengthened SHCC: Cast-in-Place Solution,” Composite Structures, V. 122, Apr. 2015, pp. 456-467. doi: 10.1016/j.compstruct.2014.12.012

6. Lowes, L. N., and Altoontash, A., “Modeling Reinforced-Concrete Beam-Column Joints Subjected to Cyclic Loading,” Journal of Structural Engineering, ASCE, V. 129, No. 12, Dec. 2003, pp. 1686-1697. doi: 10.1061/(ASCE)0733-9445(2003)129:12(1686)

7. Murty, C. V. R.; Rai, D. C.; Bajpai, K. K.; and Jain, S. K., “Effectiveness of Reinforcement Details in Exterior Reinforced Concrete Beam-Column Joints for Earthquake Resistance,” ACI Structural Journal, V. 100, No. 2, Mar.-Apr. 2003, pp. 149-156.

8. Engindeniz, M.; Kahn, L. F.; and Zureick, A.-H., “Repair and Strengthening of Reinforced Concrete Beam-Column Joints: State of the Art,” ACI Structural Journal, V. 102, No. 2, Mar.-Apr. 2005, pp. 187-197.

9. Filiatrault, A.; Pineau, S.; and Houde, J., “Seismic Behavior of Steel-Fiber Reinforced Concrete Interior Beam-Column Joints,” ACI Structural Journal, V. 92, No. 5, Sept.-Oct. 1995, pp. 543-552.

10. Del Vecchio, C.; Di Ludovico, M.; Balsamo, A.; and Prota, A., “Seismic Retrofit of Real Beam-Column Joints Using Fiber-Reinforced Cement Composites,” Journal of Structural Engineering, ASCE, V. 144, No. 5, May 2018, p. 04018026. doi: 10.1061/(ASCE)ST.1943-541X.0001999

11. Banthia, N., and Gupta, R., “Hybrid Fiber Reinforced Concrete (HyFRC): Fiber Synergy in High Strength Matrices,” Materials and Structures, V. 37, No. 10, Dec. 2004, pp. 707-716. doi: 10.1007/BF02480516

12. Afroughsabet, V.; Biolzi, L.; and Ozbakkaloglu, T., “High-Performance Fiber-Reinforced Concrete: A Review,” Journal of Materials Science, V. 51, No. 14, July 2016, pp. 6517-6551. doi: 10.1007/s10853-016-9917-4

13. Abbas, A. A.; Syed Mohsin, S. M.; and Cotsovos, D. M., “Seismic Response of Steel Fibre Reinforced Concrete Beam-Column Joints,” Engineering Structures, V. 59, Feb. 2014, pp. 261-283. doi: 10.1016/j.engstruct.2013.10.046

14. Abbass, W.; Khan, M. I.; and Mourad, S., “Evaluation of Mechanical Properties of Steel Fiber Reinforced Concrete with Different Strengths of Concrete,” Construction and Building Materials, V. 168, Apr. 2018, pp. 556-569. doi: 10.1016/j.conbuildmat.2018.02.164

15. Alaee, P., and Li, B., “High-Strength Concrete Exterior Beam-Column Joints with High-Yield Strength Steel Reinforcements,” Engineering Structures, V. 145, Aug. 2017, pp. 305-321. doi: 10.1016/j.engstruct.2017.05.024

16. Röhm, C.; Novák, B.; Sasmal, S.; Karusala, R.; and Srinivas, V., “Behavior of Fibre Reinforced Beam-Column Subassemblages under Reversed Cyclic Loading,” Construction and Building Materials, V. 36, Nov. 2012, pp. 319-329. doi: 10.1016/j.conbuildmat.2012.04.114

17. Zhang, R.; Matsumoto, K.; Hirata, T.; Ishizeki, Y.; and Niwa, J., “Application of PP-ECC in Beam-Column Joint Connections of Rigid-Framed Railway Bridges to Reduce Transverse Reinforcements,” Engineering Structures, V. 86, Mar. 2015, pp. 146-156. doi: 10.1016/j.engstruct.2015.01.005

18. Siva Chidambaram, R., and Agarwal, P., “Seismic Behavior of Hybrid Fiber Reinforced Cementitious Composite Beam–Column Joints,” Materials and Design, V. 86, Dec. 2015, pp. 771-781. doi: 10.1016/j.matdes.2015.07.164

19. Zainal, S. M. I. S.; Hejazi, F.; and Rashid, R. S. M., “Enhancing the Performance of Knee Beam-Column Joint Using Hybrid Fibers Reinforced Concrete,” International Journal of Concrete Structures and Materials, V. 15, No. 1, Dec. 2021, Article No. 20. doi: 10.1186/s40069-021-00457-w

20. Said, S. H., and Abdul Razak, H., “Structural Behavior of RC Engineered Cementitious Composite (ECC) Exterior Beam-Column Joints under Reversed Cyclic Loading,” Construction and Building Materials, V. 107, Mar. 2016, pp. 226-234. doi: 10.1016/j.conbuildmat.2016.01.001

21. Sindu, B. S., and Sasmal, S., “On the Development and Studies of Nano- and Micro-Fiber Hybridized Strain Hardened Cementitious Composite,” Archives of Civil and Mechanical Engineering, V. 19, No. 2, June 2019, pp. 348-359. doi: 10.1016/j.acme.2018.11.008

22. Emara, M.; Mohamed, H. A.; Rizk, M. S.; and Hu, J. W., “Behavior of ECC Columns Confined Using Steel Wire Mesh under Axial Loading,” Journal of Building Engineering, V. 43, Nov. 2021, Article No. 102809. doi: 10.1016/j.jobe.2021.102809

23. Li, M., and Li, V. C., “Rheology, Fiber Dispersion, and Robust Properties of Engineered Cementitious Composites,” Materials and Structures, V. 46, No. 3, Mar. 2013, pp. 405-420. doi: 10.1617/s11527-012-9909-z

24. Ranade, R.; Zhang, J.; Lynch, J. P.; and Li, V. C., “Influence of Micro-Cracking on the Composite Resistivity of Engineered Cementitious Composites,” Cement and Concrete Research, V. 58, Apr. 2014, pp. 1-12. doi: 10.1016/j.cemconres.2014.01.002

25. Sindu, B. S.; Thirumalaiselvi, A.; and Sasmal, S., “Investigations on Fracture Related Properties of Strain Hardened Concrete Using Digital Image Correlation and Acoustic Emission Techniques,” European Journal of Environmental and Civil Engineering, V. 26, No. 14, 2022, pp. 6807-6829. doi: 10.1080/19648189.2021.1962411

26. Dehghani, A.; Mozafari, A. R.; and Aslani, F., “Evaluation of the Efficacy of Using Engineered Cementitious Composites in RC Beam-Column Joints,” Structures, V. 27, Oct. 2020, pp. 151-162. doi: 10.1016/j.istruc.2020.05.045

27. Zhang, X., and Li, B., “Seismic Performance of RC Beam–Column Joints Constructed with Engineered Cementitious Composites,” Journal of Structural Engineering, ASCE, V. 146, No. 12, Dec. 2020, p. 04020271. doi: 10.1061/(ASCE)ST.1943-541X.0002824

28. Parra-Montesinos, G., and Wight, J. K., “Seismic Response of Exterior RC Column-to-Steel Beam Connections,” Journal of Structural Engineering, ASCE, V. 126, No. 10, Oct. 2000, pp. 1113-1121. doi: 10.1061/(ASCE)0733-9445(2000)126:10(1113)

29. Fischer, G., and Li, V. C., “Deformation Behavior of Fiber-Reinforced Polymer Reinforced Engineered Cementitious Composite (ECC) Flexural Members under Reversed Cyclic Loading Conditions,” ACI Structural Journal, V. 100, No. 1, Jan.-Feb. 2003, pp. 25-35.

30. Shannag, M. J.; Barakat, S.; and Abdul-Kareem, M., “Cyclic Behavior of HPFRC-Repaired Reinforced Concrete Interior Beam-Column Joints,” Materials and Structures, V. 35, No. 6, July 2002, pp. 348-356. doi: 10.1007/BF02483154

31. Khan, M. I.; Al-Osta, M. A.; Ahmad, S.; and Rahman, M. K., “Seismic Behavior of Beam-Column Joints Strengthened with Ultra-High Performance Fiber Reinforced Concrete,” Composite Structures, V. 200, Sept. 2018, pp. 103-119. doi: 10.1016/j.compstruct.2018.05.080

32. Sharma, R., and Bansal, P. P., “Behavior of RC Exterior Beam Column Joint Retrofitted Using UHP-HFRC,” Construction and Building Materials, V. 195, Jan. 2019, pp. 376-389. doi: 10.1016/j.conbuildmat.2018.11.052

33. Rai, T.; Mukharjee, B. B.; and Barai, S. V., “Beam-Column Joints Made of Self-Compacting Concrete Containing Recycled Coarse Aggregates and Nano-Silica,” International Journal of Sustainable Materials and Structural Systems, V. 4, No. 1, 2020, pp. 91-104. doi: 10.1504/IJSMSS.2020.106420

34. Sindu, B. S., and Sasmal, S., “Multi-Scale Abridged Cement Composite with Enhanced Mechanical Properties,” ACI Materials Journal, V. 117, No. 4, July 2020, pp. 105-117.

35. Sindu, B. S., and Sasmal, S., “Pseudo-Ductile Cementitious Composites by Hierarchical Crack Bridging,” ACI Materials Journal, V. 119, No. 1, Jan. 2022, pp. 145-158.

36. EFNARC, “Specification and Guidelines for Self-Compacting Concrete,” European Federation for Specialist Construction Chemicals and Concrete Systems, Flums, Switzerland, 2002, 32 pp.

37. Ghiassi, B.; Soltani, M.; and Rahnamaye Sepehr, S., “Micromechanical Modeling of Tension Stiffening in FRP-Strengthened Concrete Elements,” Journal of Composite Materials, V. 52, No. 19, Aug. 2018, pp. 2577-2596. doi: 10.1177/0021998317751248

38. Ramanjaneyulu, K.; Novák, B.; Sasmal, S.; Roehm, C.; Lakshmanan, N.; and Iyer, N. R., “Seismic Performance Evaluation of Exterior Beam-Column Subassemblages Designed According to Different Codal Recommendations,” Structure and Infrastructure Engineering, V. 9, No. 8, 2013, pp. 817-833. doi: 10.1080/15732479.2011.625954

39. FEMA 273, “NEHRP Guidelines for the Seismic Rehabilitation of Buildings,” Federal Emergency Management Agency, Washington DC, 1997, 435 pp.

40. Sasmal, S.; Ramanjaneyulu, K.; Novák, B.; and Lakshmanan, N., “Analytical and Experimental Investigations on Seismic Performance of Exterior Beam-Column Subassemblages of Existing RC‐Framed Building,” Earthquake Engineering & Structural Dynamics, V. 42, No. 12, Oct. 2013, pp. 1785-1805. doi: 10.1002/eqe.2298

41. Park, R., and Paulay, T., “Behaviour of Reinforced Concrete External Beam-Column Joints under Cyclic Loading,” Proceedings of the Fifth World Conference on Earthquake Engineering (5WCEE), V. 1, Rome, Italy, 1973, pp. 772-781.

42. Corinaldesi, V.; Letelier, V.; and Moriconi, G., “Behaviour of Beam-Column Joints Made of Recycled-Aggregate Concrete under Cyclic Loading,” Construction and Building Materials, V. 25, No. 4, Apr. 2011, pp. 1877-1882. doi: 10.1016/j.conbuildmat.2010.11.072


ALSO AVAILABLE IN:

Electronic Structural Journal