Experimental Study of Concrete Columns Reinforced with Lap-Spliced Glass Fiber-Reinforced Polymer Bars under Seismic Load

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Study of Concrete Columns Reinforced with Lap-Spliced Glass Fiber-Reinforced Polymer Bars under Seismic Load

Author(s): Bahareh Nader Tehrani, Ahmed Sabry Farghaly, and Brahim Benmokrane

Publication: Structural Journal

Volume: 121

Issue: 3

Appears on pages(s): 69-82

Keywords: Bahareh Nader Tehrani, Ahmed Sabry Farghaly, and Brahim Benmokrane

DOI: 10.14359/51740460

Date: 5/1/2024

Abstract:
While reinforcing bar lap splicing is inevitable in reinforced concrete (RC) structures, it critically affects structural behavior, especially in structures subjected to seismic load. That notwithstanding, current North American design standards do not provide any recommendations or equations for lap-spliced glass fiber-reinforced polymer (GFRP) reinforcing bars under seismic load. This study tested six full-scale RC columns measuring 1850 mm (73 in.) in height and 400 x 400 mm (16 x 16 in.) in cross section under constant axial load and incremental reversed cyclic lateral loading. Four columns were reinforced with GFRP bars, and two were reinforced with steel bars for comparison. The test parameters included lap-splice length and type of reinforcement. The structural performance of the specimens was evaluated based on the cracking behavior, failure mechanism, hysteretic response, load-carrying capacity, dissipated energy, stiffness degradation, and strain behavior. Afterward, available models in North American design standards for the splice length of GFRP reinforcing bars under monotonic loading were evaluated based on the experimental results. According to the results, providing adequate splice length can secure satisfactory structural performance in spliced GFRP-RC columns. The splice length determined based on the North American design standards for monotonic loading cannot, however, be directly used to achieve the required drift capacity in GFRP-RC columns under reversed cyclic lateral loading.

Related References:

Abdallah, A. E., and El-Salakawy, E. F., 2022a, “Effect of Aspect Ratio on Seismic Behavior of Glass Fiber-Reinforced Polymer-Reinforced Concrete Columns,” ACI Structural Journal, V. 119, No. 3, May, pp. 205-219.

Abdallah, A. E., and El-Salakawy, E. F., 2022b, “Seismic Performance of GFRP-RC Circular Columns with Different Aspect Ratios and Concrete Strengths,” Engineering Structures, V. 257, p. 114092. doi: 10.1016/j.engstruct.2022.114092

ACI Committee 318, 2019, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19) (Reapproved 2022),” American Concrete Institute, Farmington Hills, MI, 624 pp.

ACI Committee 374, 2013, “Guide for Testing Reinforced Concrete Structural Elements under Slowly Applied Simulated Seismic Loads (ACI 374.2R-13),” American Concrete Institute, Farmington Hills, MI, 18 pp.

ACI Committee 440, 2015, “Guide for the Design and Construction of Structural Concrete Reinforced with Fiber-Reinforced Polymer Bars (ACI 440.1R-15),” American Concrete Institute, Farmington Hills, MI, 88 pp.

Aly, R.; Benmokrane, B.; and Ebead, U., 2006, “Tensile Lap Splicing of Bundled CFRP Reinforcing Bars in Concrete,” Journal of Composites for Construction, ASCE, V. 10, No. 4, pp. 287-294. doi: 10.1061/(ASCE)1090-0268(2006)10:4(287)

Asadian, A.; Eslami, A.; Farghaly, A. S.; and Benmokrane, B., 2019, “Splice Strength of Staggered and Non-Staggered Bundled Glass Fiber-Reinforced Polymer Reinforcing Bars in Concrete,” ACI Structural Journal, V. 116, No. 4, July, pp. 129-142. doi: 10.14359/51714482

ASTM D7205/D7205M-21, 2021, “Standard Test Method for Tensile Properties of Fiber Reinforced Polymer Matrix Composite Bars,” ASTM International, West Conshohocken, PA, 13 pp.

Baena, M.; Torres, L.; Turon, A.; and Barris, C., 2009, “Experimental Study of Bond Behaviour between Concrete and FRP Bars Using a Pull-Out Test,” Composites Part B: Engineering, V. 40, No. 8, pp. 784-797. doi: 10.1016/j.compositesb.2009.07.003

Basaran, B., and Kalkan, I., 2020, “Investigation on Variables Affecting Bond Strength between FRP Reinforcing Bar and Concrete by Modified Hinged Beam Tests,” Composite Structures, V. 242, p. 112185. doi: 10.1016/j.compstruct.2020.112185

Bournas, D. A., and Triantafillou, T. C., 2011, “Bond Strength of Lap-Spliced Bars in Concrete Confined with Composite Jackets,” Journal of Composites for Construction, ASCE, V. 15, No. 2, pp. 156-167. doi: 10.1061/(ASCE)CC.1943-5614.0000078

CAN/CSA A23.3-19, 2019, “Design of Concrete Structures,” CSA Group, Toronto, ON, Canada, 515 pp.

CAN/CSA S806-12, 2021, “Design and Construction of Building Components with Fiber Reinforced Polymers,” CSA Group, Toronto, ON, Canada, 187 pp.

CAN/CSA S807-19, 2019, “Specification for Fibre-Reinforced Polymers,” CSA Group, Toronto, ON, Canada, 67 pp.

Chaallal, O., and Benmokrane, B., 1993, “Pullout and Bond of Glass-Fibre Rods Embedded in Concrete and Cement Grout,” Materials and Structures, V. 26, No. 3, pp. 167-175. doi: 10.1007/BF02472934

Deng, Z.; Gao, L.; and Wang, X., 2018, “Glass Fiber-Reinforced Polymer-Reinforced Rectangular Concrete Columns under Simulated Seismic Loads,” Journal of the Brazilian Society of Mechanical Sciences and Engineering, V. 40, No. 2, p. 111. doi: 10.1007/s40430-018-1041-8

Elshamandy, M. G.; Farghaly, A. S.; and Benmokrane, B., 2018, “Experimental Behavior of Glass Fiber-Reinforced Polymer-Reinforced Concrete Columns under Lateral Cyclic Load,” ACI Structural Journal, V. 115, No. 2, Mar., pp. 337-349. doi: 10.14359/51700985

Esfahani, M. R.; Rakhshanimehr, M.; and Mousavi, S. R., 2013, “Bond Strength of Lap-Spliced GFRP Bars in Concrete Beams,” Journal of Composites for Construction, ASCE, V. 17, No. 3, pp. 314-323. doi: 10.1061/(ASCE)CC.1943-5614.0000359

Hassanein, A., and Mohamed, N., Sabry Farghaly, A., and Benmokrane, B., 2020, “Effect of Boundary Element Confinement Configuration on the Performance of GFRP-Reinforced Concrete Shear Walls,” Engineering Structures, V. 225, p. 111262. doi: 10.1016/j.engstruct.2020.111262

Kharal, Z., 2019, “Towards Understanding the Seismic Behaviour of GFRP Confined Concrete Columns,” PhD dissertation, University of Toronto, Toronto, ON, Canada

Kim, C.-G.; Park, H.-G.; and Eom, T.-S., 2018, “Seismic Performance of Reinforced Concrete Columns with Lap Splices in Plastic Hinge Region,” ACI Structural Journal, V. 115, No. 1, Jan., pp. 235-245. doi: 10.14359/51701109

Kim, C.-G.; Park, H.-G.; and Eom, T.-S., 2019, “Effects of Type of Bar Lap Splice on Reinforced Concrete Columns Subjected to Cyclic Loading,” ACI Structural Journal, V. 116, No. 2, Mar., pp. 183-194. doi: 10.14359/51711142

Laoubi, K.; El-Salakawy, E.; and Benmokrane, B., 2006, “Creep and Durability of Sand-Coated Glass FRP Bars in Concrete Elements under Freeze/Thaw Cycling and Sustained Loads,” Cement and Concrete Composites, V. 28, No. 10, pp. 869-878. doi: 10.1016/j.cemconcomp.2006.07.014

Lukose, K.; Gergely, P.; and White, R., 1982, “Behavior of Reinforced Concrete Lapped Splices for Inelastic Cyclic Loading,” ACI Journal Proceedings, V. 79, No. 5, Sept.-Oct., pp. 355-365.

Manalo, A.; Maranan, G.; Benmokrane, B.; Cousin, P.; Alajarmeh, O.; Ferdous, W.; Liang, R.; and Hota, G., 2020, “Comparative Durability of GFRP Composite Reinforcing Bars in Concrete and in Simulated Concrete Environments,” Cement and Concrete Composites, V. 109, p. 103564. doi: 10.1016/j.cemconcomp.2020.103564

Mohamed, K.; Benmokrane, B.; and Krall, M., 2020, “Alkali-Silica Reactivity of Sand Used in Sand-Coating Fiber-Reinforced Polymer Bars as Internal Reinforcement for Concrete,” Journal of Composites for Construction, ASCE, V. 24, No. 6, p. 06020002. doi: 10.1061/(ASCE)CC.1943-5614.0001079

Mosley, C. P.; Tureyen, A. K.; and Frosch, R. J., 2008, “Bond Strength of Nonmetallic Reinforcing Bars,” ACI Structural Journal, V. 105, No. 5, Sept.-Oct., pp. 634-642

Naqvi, S., 2016, “Lap Splice in Glass Fiber Reinforced Polymer‐Reinforced Concrete Rectangular Columns Subjected to Cyclic‐Reversed Loads,” MSc thesis, Department of Civil Engineering, University of Manitoba, Winnipeg, MB, Canada

Naqvi, S., and El-Salakawy, E., 2017, “Lap Splice in GFRP-RC Rectangular Columns Subjected to Cyclic-Reversed Loads,” Journal of Composites for Construction, ASCE, V. 21, No. 4, p. 04016117. doi: 10.1061/(ASCE)CC.1943-5614.0000777

Pam, H. J., and Ho, J. C. M., 2010, “Effects of Steel Lap Splice Locations on Strength and Ductility of Reinforced Concrete Columns,” Advances in Structural Engineering, V. 13, No. 1, pp. 199-214. doi: 10.1260/1369-4332.13.1.199

Paulay, T.; Zanza, T.; and Scarpas, A., 1981, “Lapped Splices in Bridge Piers and in Columns of Earthquake Resisting Reinforced Concrete Frames,” Department of Civil Engineering, University of Canterbury, Christchurch, New Zealand.

Pay, A. C.; Canbay, E.; and Frosch, R. J., 2014, “Bond Strength of Spliced Fiber-Reinforced Polymer Reinforcement,” ACI Structural Journal, V. 111, No. 2, Mar.-Apr., pp. 257-266.

Prajapati, G. N.; Farghaly, A. S.; and Benmokrane, B., 2022a, “Behavior of Reinforced Concrete Columns with Hybrid Reinforcement (Steel/Glass Fiber-Reinforced Polymer) under Reversed Cyclic Load,” ACI Structural Journal, V. 119, No. 4, July, pp. 141-155.

Prajapati, G. N.; Farghaly, A. S.; and Benmokrane, B., 2022b, “Performance of Concrete Columns Longitudinally Reinforced with Steel and GFRP Bars and Confined with GFRP Spirals and Cross Ties under Reversed Cyclic Loading,” Engineering Structures, V. 270, p. 114863. doi: 10.1016/j.engstruct.2022.114863

Prajapati, G. N.; Farghaly, A. S.; and Benmokrane, B., 2023, “Behavior of Glass Fiber-Reinforced Polymer- Reinforced Concrete Columns Subjected to Simulated Seismic Load,” ACI Structural Journal, V. 120, No. 1, Jan., pp. 3-16.

Pultrall, 2020, “Data Sheet – Fiberglass and Carbon Reinforcements,” https://fiberglassrebar.com/technical-data-sheets/. (last accessed April 9, 2024)

Robert, M.; Cousin, P.; and Benmokrane, B., 2009, “Durability of GFRP Reinforcing Bars Embedded in Moist Concrete,” Journal of Composites for Construction, ASCE, V. 13, No. 2, pp. 66-73. doi: 10.1061/(ASCE)1090-0268(2009)13:2(66)

Tabatabaei Kashani, A., 2019, “Compression Lap Splices of GFRP Bars in Reinforced Concrete Columns,” PhD thesis, University of Sherbrooke, Sherbrooke, QC, Canada, 171 pp.

Tavassoli, A., 2013, “Behaviour of GFRP Reinforced Concrete Columns under Combined Axial Load and Flexure,” MSc thesis, Department of Civil Engineering, University of Toronto, Toronto, ON, Canada, 214 pp.

Tavassoli, A., 2015, “Behaviour of Circular Concrete Columns Internally Reinforced with Steel and GFRP under Simulated Earthquake Load,” MSc thesis, Department of Civil Engineering, University of Toronto, Toronto, ON, Canada, 193 pp.

Zemour, N.; Asadian, A.; Ahmed, E. A.; Benmokrane, B.; and Khayat, K. H., 2019, “Experimental Study on Splice Strength of Glass Fiber-Reinforced Polymer Reinforcing Bars in Normal and Self-Consolidating Concrete,” ACI Materials Journal, V. 116, No. 3, May, pp. 105-118. doi: 10.14359/51714459


ALSO AVAILABLE IN:

Electronic Structural Journal