Title: 
            Early-Age Cracking Resistance of Reinforced High-Strength Concrete
        
        
            Author(s): 
            Chuyuan Wen, Dejian Shen, Yang Jiao, Ci Liu, and Ming Li
        
        
            
                Publication: 
                Structural Journal
            
            
                Volume: 
                121
            
            
                Issue: 
                3
            
            
                Appears on pages(s): 
                15-24
            
            
                Keywords: 
                cracking resistance; early age; high-strength concrete (HSC); reinforcement; temperature-stress test machine (TSTM)
            
            
                DOI: 
                10.14359/51740456
            
        
        
            Date: 
            5/1/2024
        
        
            Abstract:
            High-strength concrete (HSC) with a low water-cement ratio (w/c)
may experience large autogenous shrinkage (AS). When shrinkage
of concrete is restrained by the subgrade, foundation, or other part
of the structure, HSC is more prone to crack. However, studies
devoted to the early-age cracking resistance of reinforced HSC
under uniaxial restrained conditions and adiabatic conditions are
still lacking. In the current research, the effect of reinforcement
percentage and reinforcement configuration on the temperature
history, shrinkage, stress, and creep behavior of reinforced HSC at
early age was analyzed using the temperature-stress test machine.
Test results showed that reinforcement could effectively restrain the
development of concrete shrinkage and creep. The cracking resistance of HSC increased with increasing reinforcement percentage, evaluated by the integrated criterion. With the same reinforcement percentage, reinforced HSC with distributed reinforcement along with a proper thickness of concrete cover exhibited higher cracking resistance compared with that of central reinforcement.
        
     
    
    
    
            Related References:
                
                        1. Liu, J. H.; Shi, C. J.; Ma, X. W.; Khayat, K. H.; Zhang, J.; and Wang, D. H., “An Overview on the Effect of Internal Curing on Shrinkage of High Performance Cement-Based Materials,” Construction and Building Materials, V. 146, 2017, pp. 702-712. doi: 10.1016/j.conbuildmat.2017.04.154
                    
                        2. Xin, J. D.; Zhang, G. X.; Liu, Y.; Wang, Z. H.; and Wu, Z., “Effect of Temperature History and Restraint Degree on Cracking Behavior of Early-Age Concrete,” Construction and Building Materials, V. 192, 2018, pp. 381-390. doi: 10.1016/j.conbuildmat.2018.10.066
                    
                        3. Klemczak, B., and Knoppik-Wróbel, A., “Analysis of Early-Age Thermal and Shrinkage Stresses in Reinforced Concrete Walls,” ACI Structural Journal, V. 111, No. 2, Mar.-Apr. 2014, pp. 313-322. doi: 10.14359/51686523
                    
                        4. Shariff, M. N.; and Menon, D., “Experimental Studies on Creep and Shrinkage Behavior of Reinforced Concrete Walls,” ACI Structural Journal, V. 117, No. 3, May 2020, pp. 249-260. doi: 10.14359/5172350210.14359
                    
                        5. Shi, N. N.; Ouyang, J. S.; Zhang, R. X.; and Huang, D. H., “Experimental Study on Early-Age Crack of Mass Concrete under the Controlled Temperature History,” Advances in Materials Science and Engineering, 2014, pp. 1-10. doi: 10.1155/2014/671795
                    
                        6. Huang, L. P.; Hua, J. M.; Kang, M.; and Zhang, A. L., “Influence of Reinforcement Configuration on the Shrinkage and Cracking Potential of High-Performance Concrete,” Construction and Building Materials, V. 140, 2017, pp. 20-30. doi: 10.1016/j.conbuildmat.2017.02.074
                    
                        7. Fang, D. P.; Xi, H. F.; Wang, X. M.; and Zhang, C. M., “Influences of Shrinkage, Creep, and Temperature on the Load Distributions in Reinforced Concrete Buildings During Construction,” Tsinghua Science and Technology, V. 14, No. 6, 2009, pp. 756-764. doi: 10.1016/S1007-0214(09)70146-4
                    
                        8. Yoo, D.-Y.; Park, J.-J.; Kim, S.-W.; and Yoon, Y.-S., “Influence of Reinforcing Bar Type on Autogenous Shrinkage Stress and Bond Behavior of Ultra High Performance Fiber Reinforced Concrete,” Cement and Concrete Composites, V. 48, 2014, pp. 150-161. doi: 10.1016/j.cemconcomp.2013.11.014
                    
                        9. Gu, C. P.; Wang, Y. C.; Gao, F.; Yang, Y.; Ni, T. Y.; Liu, J. T.; Lou, X.; and Chen, J., “Early Age Tensile Creep of High Performance Concrete Containing Mineral Admixtures: Experiments and Modeling,” Construction and Building Materials, V. 197, 2019, pp. 766-777. doi: 10.1016/j.conbuildmat.2018.11.218
                    
                        10. Klausen, A. E.; Kanstad, T.; Bjøntegaard, Ø.; and Sellevold, E., “Comparison of Tensile and Compressive Creep of Fly Ash Concretes in the Hardening Phase,” Cement and Concrete Research, V. 95, 2017, pp. 188-194. doi: 10.1016/j.cemconres.2017.02.018
                    
                        11. Garas, V. Y.; Kahn, L. F.; and Kurtis, K. E., “Short-Term Tensile Creep and Shrinkage of Ultra-High Performance Concrete,” Cement and Concrete Composites, V. 31, No. 3, 2009, pp. 147-152. doi: 10.1016/j.cemconcomp.2009.01.002
                    
                        12. Xin, J. D.; Li, J. H.; and Huang, D. H., “Analysis of Effect of Reinforcement on Concrete Creep Behavior,” Proceedings of the International Conference on Advances in Mechanical Engineering and Industrial Informatics, Henan, China, 2015, pp. 1307-1312.
                    
                        13. Altoubat, S. A., and Lange, D. A., “Creep, Shrinkage, and Cracking of Restrained Concrete at Early Age,” ACI Materials Journal, V. 98, No. 4, July-Aug. 2001, pp. 323-331. doi: 10.14359/10401
                    
                        14. Altoubat, S. A., and Lange, D. A., “Tensile Basic Creep: Measurements and Behavior at Early Age,” ACI Materials Journal, V. 98, No. 5, Sept.-Oct. 2001, pp. 386-393. doi: 10.14359/10728
                    
                        15. Schlitter, J. L.; Bentz, D. P.; and Weiss, W. J., “Quantifying Stress Development and Remaining Stress Capacity in Restrained, Internally Cured Mortars,” ACI Materials Journal, V. 110, No. 1, Jan. 2013, pp. 3-11. doi: 10.14359/51684361
                    
                        16. Briffaut, M.; Benboudjema, F.; Torrenti, J. M.; and Nahas, G., “A Thermal Active Restrained Shrinkage Ring Test to Study the Early Age Concrete Behaviour of Massive Structures,” Cement and Concrete Research, V. 41, No. 1, 2011, pp. 56-63. doi: 10.1016/j.cemconres.2010.09.006
                    
                        17. Wen, C. Y.; Shen, D. J.; Luo, Y. Y.; Wang, W. T.; Liu, C.; and Li, M., “Early-Age Autogenous Shrinkage and Tensile Creep of Concrete Reinforced with Polypropylene Macro Fiber,” Journal of Sustainable Cement-Based Materials, V. 12, No. 10, 2023, pp. 1-15. doi: 10.1080/21650373.2023.2214135
                    
                        18. Liu, C.; Shen, D. J.; Yang, X.; Shao, H. Z.; Tang, H. W.; and Cai, L. L., “Early-Age Properties and Shrinkage Induced Stress of Ultra-High-Performance Concrete under Variable Temperature and Uniaxial Restrained Condition,” Construction and Building Materials, V. 384, 2023, p. 131382. doi: 10.1016/j.conbuildmat.2023.131382
                    
                        19. Barrett, T. J.; De la Varga, I.; and Weiss, W. J., “Reducing Cracking in Concrete Structures by Using Internal Curing with High Volumes of Fly Ash,” Structures Congress 2012, J. Carrato and J. Burns, eds., Chicago, IL, 2012, pp. 699-707.
                    
                        20. Raoufi, K.; Schlitter, J.; Bentz, D.; and Weiss, J., “Parametric Assessment of Stress Development and Cracking in Internally Cured Restrained Mortars Experiencing Autogenous Deformations and Thermal Loading,” Advances in Civil Engineering, V. 2011, 2011, pp. 1-16. doi: 10.1155/2011/870128
                    
                        21. Sule, M. S., and van Breugel, K., “The Effect of Reinforcement on Early-Age Cracking Due to Autogenous Shrinkage and Thermal Effects,” Cement and Concrete Composites, V. 26, No. 5, 2004, pp. 581-587. doi: 10.1016/S0958-9465(03)00078-7
                    
                        22. Hua, J. M.; Zhou, F. B.; Huang, L. P.; Chen, Z. S.; Xu, Y. M.; and Xie, Z. L., “Influence of Reinforcement Bars on Concrete Pore Structure and Compressive Strength,” Materials (Basel), V. 13, No. 3, 2020, p. 658. doi: 10.3390/ma13030658
                    
                        23. Balevičius, R., and Augonis, M., “The Effects of Bond, Shrinkage and Creep on Cracking Resistance of Steel and GFRP RC Members,” Composite Structures, V. 187, 2018, pp. 85-101. doi: 10.1016/j.compstruct.2017.12.025
                    
                        24. Gribniak, V.; Kaklauskas, G.; and Bacinskas, D., “Shrinkage in Reinforced Concrete Structures: A Computational Aspect,” Journal of Civil Engineering and Management, V. 14, No. 1, 2008, pp. 49-60. doi: 10.3846/1392-3730.2008.14.49-60
                    
                        25. GB 175-2007/XG3-2018, “Common Portland Cement,” General Administration of Quality Supervision, Inspection and Quarantine of the People’s Republic of China and Standardization Administration of the People’s Republic China, Beijing, China, 2018.
                    
                        26. Kovler, K., “Testing System for Determining the Mechanical Behaviour of Early Age Concrete Under Restrained and Free Uniaxial Shrinkage,” Materials and Structures, V. 27, No. 6, 1994, pp. 324-330. doi: 10.1007/BF02473424
                    
                        27. Kolver, K.; Igarashi, S.; and Bentur, A., “Tensile Creep Behavior of High Strength Concretes at Early Ages,” Materials and Structures, V. 32, No. 5, 1999, pp. 383-387. doi: 10.1007/BF02479631
                    
                        28. Shen, D. J.; Jiang, J. L.; Wang, W. T.; Shen, J. X.; and Jiang, G. Q., “Tensile Creep and Cracking Resistance of Concrete with Different Water-to-Cement Ratios at Early Age,” Construction and Building Materials, V. 146, 2017, pp. 410-418. doi: 10.1016/j.conbuildmat.2017.04.056
                    
                        29. Shen, D. J.; Liu, C.; Li, C. C.; Zhao, X. G.; and Jiang, G. Q., “Influence of Barchip Fiber Length on Early-Age Behavior and Cracking Resistance of Concrete Internally Cured with Super Absorbent Polymers,” Construction and Building Materials, V. 214, 2019, pp. 219-231. doi: 10.1016/j.conbuildmat.2019.03.209
                    
                        30. Lura, P.; van Breugel, K.; and Maruyama, I., “Effect of Curing Temperature and Type of Cement on Early-Age Shrinkage of High-Performance Concrete,” Cement and Concrete Research, V. 31, No. 12, 2001, pp. 1867-1872. doi: 10.1016/S0008-8846(01)00601-9
                    
                        31. Zhang, J.; Hou, D. W.; and Sun, W., “Experimental Study on the Relationship Between Shrinkage and Interior Humidity of Concrete at Early Age,” Magazine of Concrete Research, V. 62, No. 3, 2010, pp. 191-199. doi: 10.1680/macr.2010.62.3.191
                    
                        32. Chu, I.; Kwon, S. H.; Amin, M. N.; and Kim, J.-K., “Estimation of Temperature Effects on Autogenous Shrinkage of Concrete by a New Prediction Model,” Construction and Building Materials, V. 35, 2012, pp. 171-182. doi: 10.1016/j.conbuildmat.2012.03.005
                    
                        33. Hansen, P., and Pedersen, J., “Maturity Computer for Controlled Curing and Hardening of Concrete,” Nordisk Betong, V. 1, 1977, pp. 19-34.
                    
                        34. Shen, D. J.; Liu, K. Q.; Wen, C. Y.; Shen, Y. Q.; and Jiang, G. Q., “Early-Age Cracking Resistance of Ground Granulated Blast Furnace Slag Concrete,” Construction and Building Materials, V. 222, 2019, pp. 278-287. doi: 10.1016/j.conbuildmat.2019.06.028
                    
                        35. Gao, X. J.; Qu, G. B.; and Zhang, A. L., “Influences of Reinforcement on Differential Drying Shrinkage of Concrete,” Journal of Wuhan University of Technology. Materials Science Edition, V. 27, No. 3, 2012, pp. 576-580. doi: 10.1007/s11595-012-0508-1
                    
                        36. Huang, L. P.; Hua, J. M.; Kang, M.; Zhou, F. B.; and Luo, Q. M., “Capillary Tension Theory for Predicting Shrinkage of Concrete Restrained by Reinforcement Bar in Early Age,” Construction and Building Materials, V. 210, 2019, pp. 63-70. doi: 10.1016/j.conbuildmat.2019.03.154
                    
                        37. Li, W. G.; Zhengyu, H.; Hu, G. Q.; Duan, W. H.; and Shah, S. P., “Early-Age Shrinkage Development of Ultra-High-Performance Concrete under Heat Curing Treatment,” Construction and Building Materials, V. 131, 2017, pp. 767-774. doi: 10.1016/j.conbuildmat.2016.11.024
                    
                        38. Sule, M. S., and van Breugel, K., “Effect of Reinforcement on Early-Age Cracking in High Strength Concrete,” Heron, V. 49, No. 2, 2004, pp. 273-292.
                    
                        39. BS 8110-2:1985, “Structural Use of Concrete—Part 2: Code of Practice for Special Circumstances,” British Standards Institution, London, UK, 1985.
                    
                        40. Kang, M., “Research on Restrained Deformation Properties of Reinforced Concrete Members due to Early Shrinkage during Construction,” PhD thesis, Chongqing University, School of Civil Engineering, 2010. (in Chinese)
                    
                        41. Miyazawa, S., and Tazawa, E., “Prediction Model for Shrinkage of Concrete Including Autogenous Shrinkage,” Autogenous Shrinkage of Concrete: Proceedings of the International Workshop, Organized by JCI (Japan Concrete Institute), E.-I. Tazawa, ed., Hiroshima, Japan, 1998, pp. 735-740.
                    
                        42. Xin, J. D.; Lin, S. Q.; Shi, N. N.; Ouyang, J. S.; and Huang, D. H., “Effect of Reinforcement on Early-Age Concrete Temperature Stress: Preliminary Experimental Investigation and Analytical Simulation,” Advances in Materials Science and Engineering, V. 2015, 2015, pp. 1-9. doi: 10.1155/2015/231973
                    
                        43. Wei, Y., and Hansen, W., “Tensile Creep Behavior of Concrete Subject to Constant Restraint at Very Early Ages,” Journal of Materials in Civil Engineering, ASCE, V. 25, No. 9, 2013, pp. 1277-1284. doi: 10.1061/(ASCE)MT.1943-5533.0000671
                    
                        44. Yeon, J. H.; Choi, S.; and Won, M. C., “Evaluation of Zero-Stress Temperature Prediction Model for Portland Cement Concrete Pavements,” Construction and Building Materials, V. 40, 2013, pp. 492-500. doi: 10.1016/j.conbuildmat.2012.10.013
                    
                        45. Sdiri, A.; Kammoun, S.; and Daoud, A., “Numerical Modeling of the Interaction Between Reinforcement and Concrete at Early Age—A Comparison Between Glass Fiber Reinforced Polymer and Steel Rebars,” Structural Concrete, V. 22, No. 1, 2020, pp. 168-182. doi: 10.1002/suco.201900314
                    
                        46. Gosaye, J.; Gardner, L.; Ahmer Wadee, M.; and Ellen, M. E., “Tensile Performance of Prestressed Steel Elements,” Engineering Structures, V. 79, 2014, pp. 234-243. doi: 10.1016/j.engstruct.2014.08.009
                    
                        47. Sun, G. J.; Xue, S. D.; Qu, X. S.; and Zhao, Y. F., “Experimental Investigation of Creep and Shrinkage of Reinforced Concrete with Influence of Reinforcement Ratio,” Advanced Concrete Construction, V. 7, No. 4, Jun. 2019, pp. 211-218. doi: 10.12989/acc.2019.7.4.211
                    
                        48. Tongaroonsri, S., and Tangtermsirikul, S., “Effect of Mineral Admixtures and Curing Periods on Shrinkage and Cracking Age under Restrained Condition,” Construction and Building Materials, V. 23, No. 2, 2009, pp. 1050-1056. doi: 10.1016/j.conbuildmat.2008.05.023
                    
                        49. ASTM C1581/C1581M-18a, “Standard Test Method for Determining Age at Cracking and Induced Tensile Stress Characteristics of Mortar and Concrete Under Restrained Shrinkage,” ASTM International, West Conshohocken, PA, 2018.
                    
                        50. Shen, D. J.; Liu, C.; Feng, Z. Z.; Zhu, S. S.; and Liang, C., “Influence of Ground Granulated Blast Furnace Slag on the Early-Age Anti-Cracking Property of Internally Cured Concrete,” Construction and Building Materials, V. 223, 2019, pp. 233-243. doi: 10.1016/j.conbuildmat.2019.06.149
                    
                        51. Passuello, A.; Moriconi, G.; and Shah, S. P., “Cracking Behavior of Concrete with Shrinkage Reducing Admixtures and PVA Fibers,” Cement and Concrete Composites, V. 31, No. 10, 2009, pp. 699-704. doi: 10.1016/j.cemconcomp.2009.08.004
                    
                        52. Shen, D. J.; Jiang, J. L.; Shen, J. X.; Yao, P. P.; and Jiang, G. Q., “Influence of Prewetted Lightweight Aggregates on the Behavior and Cracking Potential of Internally Cured Concrete at an Early Age,” Construction and Building Materials, V. 99, 2015, pp. 260-271. doi: 10.1016/j.conbuildmat.2015.08.093
                    
                        53. Sule, M. S., and van Breugel, K., “Cracking Behaviour of Reinforced Concrete Subjected to Early-Age Shrinkage,” Materials and Structures, V. 34, No. 5, 2001, pp. 284-292. doi: 10.1007/BF02482208