New Anchorage Technique for GFRP Flexural Strengthening of Concrete Beams Using Bolts-End Anchoring System

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: New Anchorage Technique for GFRP Flexural Strengthening of Concrete Beams Using Bolts-End Anchoring System

Author(s): Djarir Yahiaoui, Abdelaziz Boutrid, Mohamed Saadi, Belgacem Mamen & Tayeb Bouzid

Publication: IJCSM

Volume: 17

Issue:

Appears on pages(s):

Keywords: Tension zone, Bolts-end anchoring, Glass FRP, Bolts, Crack patterns, Failure modes

DOI: 10.1186/s40069-023-00578-4

Date: 7/31/2023

Abstract:
The concept of external glass FRP composite confinement is a current process for strengthening concrete beams subjected to static loads. End anchorage glass FRP composites of 80 mm width and 90–130 mm length with different thicknesses (2.4 and 4.8 mm) have been fixed at the bottom of beams with bolts of various diameters (6 and 10 mm). For this purpose, the behavior of beams strengthened with bolt-end anchoring glass fiber polymer composites (BEGFPC) has been analyzed. It is concluded that the load capacity of the BEGFPC beams is improved by increasing the end-anchorage glass FRP composite thickness (about 98–188%). In addition, the BEGFPC system with bolts of 6 mm diameter has significantly improved the flexibility of beams. In contrast, the 10 mm bolts in diameter give a high ultimate load, whatever their quantity. Therefore, combining bolts with diameters of 6 and 10 mm would be the best solution for increasing the ultimate load and ductility of the retrofitted beams. Depending on the number and bolts' arrangement, there is also an enhancement in the crack patterns by changing from intermediate flexural failure to shear failure in beams.