NEU Material and Technology Validation/Verification Program

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: NEU Material and Technology Validation/Verification Program

Author(s): Mahmut Ekenel

Publication: Web Session

Volume: ws_F23_MahmutEkenel.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 10/29/2023

Abstract:
This presentation will provide an overview of the Validation/Verification program, which is currently being launched by NEU. The NEU Validation/Verification program is conducted impartially by subject matter experts to evaluate the accuracy of relevant technical claims related to reduction of carbon in cement, concrete, and other concrete related products. NEU's Validation/Verification assessments provide guidance in acceptance of the new technologies and their claim about carbon footprint reduction.