“Reasonable Safety” of Existing Structures, Part 3

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: “Reasonable Safety” of Existing Structures, Part 3

Author(s): David G. Tepke, Liying Jiang, Keith E. Kesner, and Stephen S. Szoke

Publication: Concrete International

Volume: 46

Issue: 1

Appears on pages(s): 57-62

Keywords: condition, survey, deterioration, defects

DOI: 10.14359/51740324

Date: 1/1/2024

Abstract:
This is the third of a series of four articles focused on safety of existing structures. It discusses some of the intricacies associated with "reading the structure"--the process of examining the structure, determining the need for focused testing or further evaluation, and then deciding on a path forward.

Related References:

1. Tepke, D.G.; Jiang, L.; Kesner, K.E.; and Szoke, S.S., “Reasonable Safety of Existing Structures, Part 2,” Concrete International, V. 45, No. 12, Dec. 2023, pp. 53-58.

2. Kesner, K.E.; Tepke, D.G.; Jiang, L.; and Szoke, S.S., “Reasonable Safety of Existing Structures, Part 1,” Concrete International, V. 45, No. 11, Nov. 2023, pp. 43-48.

3. ACI Committee 562, “Assessment, Repair, and Rehabilitation of Existing Concrete Structures—Code and Commentary (ACI CODE-562-21),” American Concrete Institute, Farmington Hills, MI, 2021, 88 pp.

4. ACI Committee 364, “Guide for Assessment of Concrete Structures Before Rehabilitation (ACI 364.1R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 20 pp.

5. SEI/ASCE 11-99, “Guideline for Structural Condition Assessment of Existing Buildings,” American Society of Civil Engineers, Reston, VA, 2000, 143 pp.

6. ACI Committee 201, “Guide for Conducting a Visual Inspection of Concrete in Service (ACI 201.1R-08),” American Concrete Institute, Farmington Hills, MI, 2008, 16 pp.

7. ACI Committee 224, “Causes, Evaluation, and Repair of Cracks in Concrete Structures (ACI 224.1R-07),” American Concrete Institute, Farmington Hills, MI, 2007, 22 pp.

8. ACI Committee 224, “Control of Cracking in Concrete Structures (ACI 224R-01) (Reapproved 2008),” American Concrete Institute, Farmington Hills, MI, 2001, 46 pp.

9. ACI Committee 224, “Guide to Design Detailing to Mitigate Cracking (ACI 224.4R-13),” American Concrete Institute, Farmington Hills, MI, 2013, 20 pp.

10. ACI Committee 201, “Durable Concrete—Guide (ACI PRC-201.2-23),” American Concrete Institute, Farmington Hills, MI, 2023, 99 pp.

11. Tepke, D.G., and Isgor, O.B., “Is the Inside of Your Structure Safe from Corrosion?” Concrete International, V. 45, No. 8, Aug. 2023, pp. 31-36.

12. ACI Committee 222, “Guide to Protection of Reinforcing Steel in Concrete against Corrosion (ACI 222R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 60 pp.

13. ACI Committee 228, “Report on Nondestructive Test Methods for Evaluation of Concrete in Structures (ACI 228.2R-13),” American Concrete Institute, Farmington Hills, MI, 2013, 82 pp.

14. ACI Committee 228, “Report on Methods for Estimating In-Place Concrete Strength (ACI 228.1R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 48 pp.

15. ACI Committee 437, “Strength Evaluation of Existing Concrete Buildings (ACI 437R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 28 pp.

16. ACI Committee 214, “Guide to Evaluation of Strength Test Results of Concrete (ACI 214R-11) (Reapproved 2019),” American Concrete Institute, Farmington Hills, MI, 2011, 16 pp.

17. ACI Committee 437, “Load Tests of Concrete Structures: Methods, Magnitude, Protocols, and Acceptance Criteria (ACI 437.1R-07),” American Concrete Institute, Farmington Hills, MI, 2007, 38 pp.

18. ACI Committee 437, “Load Testing of Concrete Structures—Code and Commentary (ACI CODE-437.2-22),” American Concrete Institute, Farmington Hills, MI, 2022, 22 pp.

19. Tepke, D.G.; Firlotte, C.; and Robinson, S.P., “A Decade After Cathodic Protection and Concrete Repairs at Sound of the Sea II Condominiums,” Concrete International, V. 42, No. 11, Nov. 2020, pp. 18-23.

20. Tepke, D.G.; Tribble, N.B.; and Robinson, S.P., “Design for Longevity: A Look Back at Concrete Rehabilitation and Preservation at Shipyard Village Condominiums,” Concrete Repair Bulletin, July-Aug. 2023, pp. 16-23.