Title: Understanding ACI 117 Construction Tolerances and Tools

Author(s): Ahern

Publication: Web Session

Volume: ws_S23_Ahern.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 4/2/2023

Abstract:
This presentation will discuss the main contributions from Bruce to the ACI 117 tolerances committee and some examples of practical tools and best practices related to construction tolerances.