Effective Teaching Methods for Non-destructive Testing Techniques

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effective Teaching Methods for Non-destructive Testing Techniques

Author(s): Armen Amirkhanian and Eleanor Skelton

Publication: Symposium Paper

Volume: 359

Issue:

Appears on pages(s): 69-89

Keywords: resistivity, ultrasonic pulse velocity, UPV, covermeter, experiential learning, non-destructive testing

DOI: 10.14359/51740291

Date: 11/1/2023

Abstract:
This paper presents an introduction to three common non-destructive testing techniques and effective methods to instruct students on the theory, application, advantages, and disadvantages. The document will outline teaching plans for resistivity measurements, ultrasonic pulse velocity measurements, and cover meter measurements. These three methods generally require inexpensive equipment and short preparation times for classroom demonstrations. Additionally, the first two methods have well established ASTM or AASHTO testing procedures that will aid the instructor in presenting the material, even with little to no experience with the techniques. From an instructional standpoint, various experiential learning pedagogies will be discussed to enhance the student learning outcomes. The exercises and lessons presented in the document are the result of many NDT course offerings at various universities. As such, the lessons learned from each exercise will be presented to further guide new instructors to succeed in teaching the material effectively the first time their course is offered.

Related References:

AASHTO (2021). T-358: Standard Method of Test for Surface Resistivity Indication of Concrete’s Ability to Resist Chloride Ion Penetration. https://store.transportation.org/item/publicationdetail/4893

AASHTO (2021). TP-119: Provisional Standard Method of Test for Electrical Resistivity of a Concrete Cylinder Tested in Uniaxial Resistance Test. https://store.transportation.org/item/publicationdetail/4925

Abdulwahed, M., and Nagy, Z. K. (2009). “Applying Kolb’s Experiential Learning Cycle for Laboratory Education.” Journal of Engineering Education, 98(3), 283–294.

Archie, G. E. (1942). “The electrical resistivity log as an aid in determining some reservoir characteristics.” Transactions of the AIME, 146(01), 54–62.

ASTM International. (2016). ASTM C597: Test Method for Pulse Velocity Through Concrete. doi: 10.1520/C0597-16

ASTM International. (2021). ASTM C39: Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens.

ASTM International. (2022). ASTM C469: Test Method for Static Modulus of Elasticity and Poissons Ratio of Concrete in Compression. doi: 10.1520/C0469_C0469M-22

Barneyback, R. S., and Diamond, S. (1981). “Expression and analysis of pore fluids from hardened cement pastes and mortars.” Cement and Concrete Research, 11(2), 279–285.

Bentz, D. P. (2007). “A virtual rapid chloride permeability test.” Cement and Concrete Composites, 29(10), 723–731.

Coyle, A., Spragg, R., Amirkhanian, A., and Weiss, J. (2016). “Measuring the influence of temperature on electrical properties of concrete.” Service Life of Cement-Based Materials and Structures, M. Azenha, I. Gabrijel, D. Schlicke, T. Kanstad, and O. Jensen, eds., Lyngby, Denmark, 211–220.

Coyle, A. T., Spragg, R. P., Suraneni, P., Amirkhanian, A. N., and Weiss, W. J. (2018). “Comparison of Linear Temperature Corrections and Activation Energy Temperature Corrections for Electrical Resistivity Measurements of Concrete.” Advances in Civil Engineering Materials, 7(1), 20170135.

Gu, P., Xie, P., Beaudoin, J. J., and Brousseau, R. (1992). “A.C. impedance spectroscopy (I): A new equivalent circuit model for hydrated portland cement paste.” Cement and Concrete Research, 22(5), 833–840.

Hüblová, S., Cikrle, P., Karel, O., and Kocáb, D. (2019) “Experimental measurement of the diameter and cover depth of steel reinforcement using an electromagnetic concrete cover meter.” IOP Conf. Ser.: Mater. Sci. Eng., 549, 012011.

Kolb, D. (2014). Experiential learning: Experience as the source of learning and development. FT Press.

Komloš, K., Popovics, S., Nürnbergerová, T., Babál, B., Popovics, J.S. (1996) “Ultrasonic pulse velocity test of concrete properties as specified in various standards.” Cement and Concrete Composites, 18(5), 357-364.

Madani, H., Bagheri, A., Parhizkar, T., and Raisghasemi, A. (2014). “Chloride penetration and electrical resistivity of concretes containing nanosilica hydrosols with different specific surface areas.” Cement and Concrete Composites, Elsevier, 53, 18–24.

Philleo, R. E. (1955). “Comparison of Results of Three Methods for Determining Young’s Modulus of Elasticity of Concrete.” ACI Journal Proceedings, 51(1), 461–469.

Randles, J. E. B. (1947). “Kinetics of rapid electrode reactions.” Discussions of the Faraday Society, 1, 11.

Riding, K. A., Poole, J. L., Schindler, A. K., Juenger, M. C. G., and Folliard, K. J. (2008). “Simplified concrete resistivity and rapid chloride permeability test method.” ACI Materials Journal, 105(4), 390–394.

Snyder, K. A., Feng, X., Keen, B. D., and Mason, T. O. (2003). “Estimating the electrical conductivity of cement paste pore solutions from OH-, K+ and Na+ concentrations.” Cement and Concrete Research, 33(6), 793–798.

Spragg, R. P., Castro, J., Nantung, T., Paredes, M., and Weiss, J. (2012). “Variability Analysis of the Bulk Resistivity Measured Using Concrete Cylinders.” Advances in Civil Engineering Materials, 1(1), 104596.

Tumidajski, P. J., Schumacher, A. S., Perron, S., Gu, P., and Beaudoin, J. J. (1996). “On the relationship between porosity and electrical resistivity in cementitious systems.” Cement and Concrete Research, 26(4), 539–544.