ACI PRC-440.2-23: Design and Construction of Externally Bonded Fiber-Reinforced Polymer (FRP) Systems for Strengthening Concrete Structures—Guide

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ACI PRC-440.2-23: Design and Construction of Externally Bonded Fiber-Reinforced Polymer (FRP) Systems for Strengthening Concrete Structures—Guide

Author(s): ACI Committee 440

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 109

Keywords:

DOI:

Date: 11/1/2023

Abstract:
Fiber-reinforced polymer (FRP) systems for strengthening concrete structures are an alternative to traditional strengthening techniques such as steel plate bonding, section enlargement, and external post-tensioning. FRP strengthening systems use FRP composite materials as supplemental externally bonded or near-surface-mounted (NSM) reinforcement. FRP systems offer advantages over traditional strengthening techniques: they are lightweight, relatively easy to install, and noncorroding. Due to the characteristics of FRP systems as well as the behavior of members strengthened with FRP, specific guidance on the use of these systems is needed. This guide provides general information on the history and use of FRP strengthening systems; a description of the material properties of FRP; and recommendations on the engineering, construction, and inspection of FRP systems used to strengthen concrete structures. This guide is based on the knowledge gained from experimental research, analytical work, and field applications of FRP systems used to strengthen concrete structures. Keywords: aramid fibers; basalt fibers; bridges; buildings; carbon fibers; corrosion; cracking; development length; earthquake resistance; fiber-reinforced polymers; glass fibers; structural design.