Title: Concrete Q&A: Effective Depth of Section with More Than One Layer of Tension Reinforcement

Author(s): Weilacher, R.M.; Newsome, J.; and Harrison, G.H.

Publication: Concrete International

Volume: 45

Issue: 12

Appears on pages(s): 103-104

Keywords:

DOI: 10.14359/51740277

Date: 12/1/2023

Abstract:
This month’s Q&A provides an explanation on how to determine an effective depth of a section d when multiple layers of reinforcement are distributed through an entire depth of a reinforced concrete beam.

Related References:

1. ACI Committee 318, “Building Code Requirements for Structural Concrete and Commentary (ACI CODE-318-19) (Reapproved 2022),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.