New Joint ACI and ICRI Guide for Cementitious Repair Material Data Sheet

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: New Joint ACI and ICRI Guide for Cementitious Repair Material Data Sheet

Author(s): Fred R. Goodwin, Benoit Bissonnette, Dave Fuller, Mark Nelson, and Joshua Lloyd

Publication: Concrete International

Volume: 45

Issue: 12

Appears on pages(s): 61-66

Keywords: document, chapter, information, characteristics

DOI: 10.14359/51740271

Date: 12/1/2023

Abstract:
The recently published Guide for Cementitious Repair Material Data Sheet (ACI PRC-364.3-22/ICRI 320.3R-2022) is a result of cooperation between the American Concrete Institute (ACI) and International Concrete Repair Institute (ICRI). This document is a first in the industry to provide this information in a standardized, logical, and consistent format so that repair materials can be appropriately selected and specified.

Related References:

1. ACI Committee 364, “Cementitious Repair Material Data Sheet—Guide (ACI PRC-364.3-22),” American Concrete Institute, Farmington Hills, MI, 2022, 31 pp.

2. ICRI 320.3R-2022, “Cementitious Repair Material Data Sheet—Guide,” International Concrete Repair Institute, Inc., Minneapolis, MN, 2022, 31 pp.

3. Emmons, P.H.; Vaysburd, A.M.; Poston, R.W.; and McDonald, J.E., “Performance Criteria for Concrete Repair Materials, Phase II Field Studies,” Technical Report REMR-CS-60, U.S. Army Corps of Engineers, Washington, DC, Sept. 1998, 98 pp.

4. Vaysburd, A.M.; Emmons, P.H.; McDonald, J.E.; Poston, R.W.; and Kesner, K.E., “Performance Criteria for Concrete Repair Materials, Phase II Summary Report,” Technical Report REMR-CS-62, U.S. Army Corps of Engineers, Washington, DC, Mar. 1999, 72 pp.

5. Vaysburd, A.M.; Carino, N.J.; and Bissonnette, B., “Predicting the Performance of Concrete Repair Materials,” NISTIR 6402, National Institute of Standards and Technology, Gaithersburg, MD, Jan. 2000, 38 pp.

6. SDC, “Vision 2020: A Vision for the Concrete Repair, Protection and Strengthening Industry,” ACI Foundation Strategic Development Council, Farmington Hills, MI, 2006, 29 pp.

7. Shiu, K.N., and Goodwin, F., “Vision 2020—Before and After,” Concrete Repair Bulletin, Sept./Oct. 2014, pp. 34-41.

8. Goodwin, F., “Repair-Material Data-Sheet Protocol,” Concrete Repair Bulletin, Jan./Feb. 2005, pp. 25-27.

9. Earley, W., “ICRI’s New Committee Numbering System,” Concrete Repair Bulletin, Jan./Feb. 2009, pp. 18-19.

10. Goodwin, F.R., and VanGarven, R., “ICRI 320.3, Repair Material Data Sheet Protocol: Going from Good to Better,” Concrete Repair Bulletin, July/Aug. 2010, pp. 16-21.

11. ACI Committee 364, “Guide for Cementitious Repair Material Data Sheet (ACI 364.3R-09),” American Concrete Institute, Farmington Hills, MI, 2009, 12 pp.

12. ACI Committee 546, “Guide to Materials Selection for Concrete Repair (ACI 546.3R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 72 pp.

13. ICRI 320.2R-2018, “Guide for Selecting and Specifying Materials for Repair of Concrete Surfaces,” International Concrete Repair Institute, Inc., Minneapolis, MN, 2018, 44 pp.

14. American Concrete Institute, “ACI Concrete Terminology (ACI CT-23)” ACI, Farmington Hills, MI, 2023, 78 pp.

15. “ICRI Concrete Repair Terminology,” International Concrete Repair Institute, Inc., Minneapolis, MN, 2022, 112 pp.

16. ACI Committee 364, “TechNote: How to Measure pH of a Concrete Surface Prior to Installation of a Floor Covering (ACI 364.17T-18),” American Concrete Institute, Farmington Hills, MI, 2018, 5 pp.

17. CRD-C 164-92, “Standard Test Method for Direct Tensile Strength of Cylindrical Concrete or Mortar Specimens,” U.S. Army Engineer Research and Development Center (ERDC), Vicksburg, MS, 1992, 4 pp.

18. ICRI 210.3R-2022, “Guide for Using In-Situ Tensile Pulloff Tests to Evaluate Concrete Surface Repairs and Bonded Overlays,” International Concrete Repair Institute, Inc., Minneapolis, MN, 2022, 24 pp.

19. CRD-C 39-81, “Test Method for Coefficient of Linear Thermal Expansion of Concrete,” U.S. Army Engineer Research and Development Center (ERDC), Vicksburg, MS, 1981, 2 pp.

20. AASHTO T 259-02(2021), “Standard Method of Test for Resistance of Concrete to Chloride Ion Penetration,” American Association of State Highway and Transportation Officials, Washington, DC, 2002, 4 pp.

21. Butcher, T.G.; Sefcik, D.A.; Warfield, L.; Benham, E.J.; Bowers, S.L.; and Lippa, K.A., “NIST Handbook 133: Checking the Net Contents of Packaged Goods,” National Institute of Standards and Technology, Gaithersburg, MD, 2023, https://www.nist.gov/pml/owm/nist-handbook-133-current-edition.

22. “Consumer Packaging and Labelling Regulations (C.R.C., c. 417),” Department of Justice, Government of Canada, Ottawa, ON, Canada, June 17, 2019, 32 pp.

23. ICRI 310.2R-2013, “Selecting and Specifying Concrete Surface Preparation for Sealers, Coatings, Polymer Overlays, and Concrete Repair,” International Concrete Repair Institute, Inc., Minneapolis, MN, 2013, 54 pp.

24. ICRI 320.5R-2014, “Pictorial Atlas of Concrete Repair Equipment,” International Concrete Repair Institute, Inc., Minneapolis, MN, 2014, 20 pp.