Performance of Quality-Controlled Recycled Concrete Aggregates

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Performance of Quality-Controlled Recycled Concrete Aggregates

Author(s): Amit Kumar, Gyani Jail Singh, Priyanshu Raj, and Rajesh Kumar

Publication: Materials Journal

Volume: 121

Issue: 1

Appears on pages(s): 17-30

Keywords: durability; mechanical properties; mechanical treatment; performance; physical properties; quality control; recycled concrete aggregate (RA)

DOI: 10.14359/51740259

Date: 1/1/2024

Abstract:
This research examines the performance of quality-controlled recycled concrete aggregates (QRAs) with fly-ash-based cement. Compared to concrete made from untreated recycled concrete aggregates (URC), quality-controlled recycled aggregate concrete (QRC) has superior physical, mechanical, and durability properties. Except for sorptivity, the physical, mechanical, and durability properties of QRC are almost identical to those of natural aggregate concrete (NC). The compressive strength, splitting tensile strength, flexural strength, fracture energy, and modulus of elasticity of QRC are higher than those of URC by 18.0%, 16.8%, 60.0%, 27.17%, and 43.46%, respectively. The abrasion resistance of QRC is approximately 60% higher than URC. Scanning electron microscope (SEM) image and energy-dispersive X-ray (EDX) analysis prove that quality control produces denser old interfacial transition zones (OITZ) with fewer microvoids. The QRA improves not only the pore structure but also the weak mortar structure attached to the aggregate. There is also a strong correlation between the compressive strength and splitting tensile strength, flexural strength, fracture energy, and modulus of elasticity of QRC. QRA can be used to compute the mixture proportions for concrete (certainly up to medium-strength concrete) according to either the Indian standard or the international standard. It is challenging to improve the sorptivity of recycled concrete aggregates closer to NC. In addition, QRC has an initial sorptivity of two times (initial) and a final sorptivity of 1.8 times higher than NC, whereas URC has an initial sorptivity of 3.5 times (initial) and a final sorptivity of 2.35 times higher than NC.

Related References:

1. Kim, J., “Influence of Quality of Recycled Aggregates on the Mechanical Properties of Recycled Aggregate Concretes: An Overview,” Construction and Building Materials, V. 328, Apr. 2022, Article No. 127071.

2. Martín-Morales, M.; Zamorano, M.; Ruiz-Moyano, A.; and Valverde-Espinosa, I., “Characterization of Recycled Aggregates Construction and Demolition Waste for Concrete Production Following the Spanish Structural Concrete Code EHE-08,” Construction and Building Materials, V. 25, No. 2, Feb. 2011, pp. 742-748. doi: 10.1016/j.conbuildmat.2010.07.012

3. Duan, Z. H., and Poon, C. S., “Properties of Recycled Aggregate Concrete Made with Recycled Aggregates with Different Amounts of Old Adhered Mortars,” Materials & Design, V. 58, June 2014, pp. 19-29. doi: 10.1016/j.matdes.2014.01.044

4. Adams, M. P., and Jayasuriya, A., “Guideline Development for Use of Recycled Concrete Aggregates in New Concrete (ACI CRC 18.517),” ACI Foundation Concrete Research Council, Farmington Hills, MI, 2019, 89 pp.

5. Neville, A. M., Properties of Concrete, fourth edition, Pearson, London, UK, 1995.

6. Kumar, A., and Singh, G. J., “Improving the Physical and Mechanical Properties of Recycled Concrete Aggregate: A State-of-the-Art Review,” Engineering Research Express, V. 5, No. 1, Mar. 2023, Article No. 012007.

7. Purushothaman, R.; Amirthavalli, R. R.; and Karan, L., “Influence of Treatment Methods on the Strength and Performance Characteristics of Recycled Aggregate Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 27, No. 5, May 2015, p. 04014168.

8. Pandurangan, K.; Dayanithy, A.; and Om Prakash, S., “Influence of Treatment Methods on the Bond Strength of Recycled Aggregate Concrete,” Construction and Building Materials, V. 120, Sept. 2016, pp. 212-221. doi: 10.1016/j.conbuildmat.2016.05.093

9. Ahmad, S.; Maslehuddin, M.; Shameem, M.; Faysal, R. M.; and Adekunle, S. K., “Effect of Abrasion and Chemical Treatment of Recycled Aggregate on the Workability, Strength, and Durability Properties of Concrete,” European Journal of Environmental and Civil Engineering, V. 26, No. 8, 2022, pp. 3276-3291.

10. Alqarni, A. S.; Abbas, H.; Al-Shwikh, K. M.; and Al-Salloum, Y. A., “Treatment of Recycled Concrete Aggregate to Enhance Concrete Performance,” Construction and Building Materials, V. 307, Nov. 2021, Article No. 124960. doi: 10.1016/j.conbuildmat.2021.124960

11. Dilbas, H.; Çakır, Ö.; and Atiş, C. D., “Experimental Investigation on Properties of Recycled Aggregate Concrete with Optimized Ball Milling Method,” Construction and Building Materials, V. 212, July 2019, pp. 716-726. doi: 10.1016/j.conbuildmat.2019.04.007

12. Princigallo, A., “Effective Water in Concrete with Recycled Aggregate,” ACI Materials Journal, V. 115, No. 6, Nov. 2018, pp. 845-854. doi: 10.14359/51706842

13. ACI Committee E701, “Aggregates for Concrete (ACI Education Bulletin E1-07),” American Concrete Institute, Farmington Hills, MI, 2007, 29 pp.

14. Kurda, R.; de Brito, J.; and Silvestre, J. D., “Influence of Recycled Aggregates and High Contents of Fly Ash on Concrete Fresh Properties,” Cement and Concrete Composites, V. 84, Nov. 2017, pp. 198-213. doi: 10.1016/j.cemconcomp.2017.09.009

15. Brand, A. S.; Roesler, J. R.; and Salas, A., “Initial Moisture and Mixing Effects on Higher Quality Recycled Coarse Aggregate Concrete,” Construction and Building Materials, V. 79, Mar. 2015, pp. 83-89. doi: 10.1016/j.conbuildmat.2015.01.047

16. Quattrone, M.; Cazacliu, B.; Angulo, S. C.; Hamard, E.; and Cothenet, A., “Measuring the Water Absorption of Recycled Aggregates, What Is the Best Practice for Concrete Production?” Construction and Building Materials, V. 123, Oct. 2016, pp. 690-703. doi: 10.1016/j.conbuildmat.2016.07.019

17. Mefteh, H.; Kebaïli, O.; Oucief, H.; Berredjem, L.; and Arabi, N., “Influence of Moisture Conditioning of Recycled Aggregates on the Properties of Fresh and Hardened Concrete,” Journal of Cleaner Production, V. 54, Sept. 2013, pp. 282-288. doi: 10.1016/j.jclepro.2013.05.009

18. Poon, C. S.; Shui, Z. H.; Lam, L.; Fok, H.; and Kou, S. C., “Influence of Moisture States of Natural and Recycled Aggregates on the Slump and Compressive Strength of Concrete,” Cement and Concrete Research, V. 34, No. 1, Jan. 2004, pp. 31-36. doi: 10.1016/S0008-8846(03)00186-8

19. Tangchirapat, W.; Buranasing, R.; and Jaturapitakkul, C., “Use of High Fineness of Fly Ash to Improve Properties of Recycled Aggregate Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 22, No. 6, June 2010, pp. 565-571. doi: 10.1061/(ASCE)MT.1943-5533.0000054

20. Kou, S. C.; Poon, C. S.; and Chan, D., “Influence of Fly Ash as Cement Replacement on the Properties of Recycled Aggregate Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 19, No. 9, Sept. 2007, pp. 709-717. doi: 10.1061/(ASCE)0899-1561(2007)19:9(709)

21. Bhasya, V., and Bharatkumar, B. H., “Mechanical and Durability Properties of Concrete Produced with Treated Recycled Concrete Aggregate,” ACI Materials Journal, V. 115, No. 2, Mar. 2018, pp. 209-217. doi: 10.14359/51701239

22. Rashid, K.; Rehman, M. U.; de Brito, J.; and Ghafoor, H., “Multi-

Criteria Optimization of Recycled Aggregate Concrete Mixes,” Journal of Cleaner Production, V. 276, Dec. 2020, Article No. 124316. doi: 10.1016/j.jclepro.2020.124316

23. IS 383:2016, “Coarse and Fine Aggregate for Concrete—Specification,” Bureau of Indian Standards, New Delhi, India, 2016, 21 pp.

24. IS 10262:2019, “Concrete Mix Proportioning—Guidelines,” Bureau of Indian Standards, New Delhi, India, 2019, 44 pp.

25. Mi, R.; Pan, G.; and Kuang, T., “Reducing the Carbonation Zone and Steel Corrosion Zone Widths of Recycled Aggregate Concrete by Optimizing Its Mixing Process,” Journal of Materials in Civil Engineering, ASCE, V. 33, No. 5, May 2021, p. 04021061.

26. IS 516 (Part 1/Sec 1):2021, “Hardened Concrete—Methods of Test: Part 1 – Testing of Strength of Hardened Concrete: Section 1 – Compressive, Flexural and Split Tensile Strength,” Bureau of Indian Standards, New Delhi, India, 2021, 20 pp.

27. ASTM C496/C496M-04, “Standard Test Method for Splitting Tensile Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2004, 5 pp.

28. ASTM C78/C78M-18, “Standard Test Method for Flexural Strength of Concrete (Using Simple Beam with Third-Point Loading),” ASTM International, West Conshohocken, PA, 2018, 5 pp.

29. ASTM C469-02, “Standard Test Method for Static Modulus of Elasticity and Poisson’s Ratio of Concrete in Compression,” ASTM International, West Conshohocken, PA, 2002, 5 pp.

30. RILEM, “Determination of the Fracture Energy of Mortar and Concrete by Means of Three-Point Bend Tests on Notched Beams,” Materials and Structures, V. 18, No. 4, July 1985, pp. 287-290.

31. ASTM C642-97, “Standard Test Method for Density, Absorption, and Voids in Hardened Concrete,” ASTM International, West Conshohocken, PA, 1997, 3 pp.

32. ASTM C1585-04, “Standard Test Method for Measurement of Rate of Absorption of Water by Hydraulic-Cement Concretes,” ASTM International, West Conshohocken, PA, 2004, 6 pp.

33. IS 516 (Part 5):2018, “Hardened Concrete—Methods of Test: Part 5 – Non-destructive Testing of Concrete,” Bureau of Indian Standards, New Delhi, India, 2018.

34. ASTM C1202-19, “Standard Test Method for Electrical Indication of Concrete’s Ability to Resist Chloride Ion Penetration,” ASTM International, West Conshohocken, PA, 2019, 8 pp.

35. IS 15658:2006, “Precast Concrete Blocks for Paving—Specification,” Bureau of Indian Standards, New Delhi, India, 2006, 27 pp.

36. IS 2386 (Part III)-1963, “Methods of Test for Aggregates for Concrete: Part III – Specific Gravity, Density, Voids, Absorption and Bulking (Reaffirmed 2021),” Bureau of Indian Standards, New Delhi, India, 1963, 22 pp.

37. ASTM C597-09, “Standard Test Method for Pulse Velocity Through Concrete,” ASTM International, West Conshohocken, PA, 2009, 4 pp.

38. Singh, G. J.; Kumar, V.; Singh, B. N.; and Kumar, R., “Impact of Drying the Concrete before Its Complete Curing: Plain and Fly Ash–Based Cement Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 34, No. 2, Feb. 2022, p. 04021442. doi: 10.1061/(ASCE)MT.1943-5533.0004290

39. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-08) and Commentary (ACI 318R-08),” American Concrete Institute, Farmington Hills, MI, 2008, 473 pp.

40. Xiao, J.-Z.; Li, J.-B.; and Zhang, C., “On Relationships between the Mechanical Properties of Recycled Aggregate Concrete: An Overview,” Materials and Structures, V. 39, No. 6, July 2006, pp. 655-664. doi: 10.1617/s11527-006-9093-0

41. IS 456:2000, “Plain and Reinforced Concrete—Code of Practice (Reaffirmed 2005),” Bureau of Indian Standards, New Delhi, India, 2000, 114 pp.

42. Zhou, C., and Chen, Z., “Mechanical Properties of Recycled Concrete Made with Different Types of Coarse Aggregate,” Construction and Building Materials, V. 134, Mar. 2017, pp. 497-506.

43. Siregar, A. P. N.; Pasaribu, E. L.; and Suarnita, I. W., “The Effect of Coarse Aggregate Hardness on the Fracture Toughness and Compressive Strength of Concrete,” MATEC Web of Conferences, V. 258, 2019, Article No. 04011.

44. Butler, L.; West, J. S.; and Tighe, S. L., “The Effect of Recycled Concrete Aggregate Properties on the Bond Strength between RCA Concrete and Steel Reinforcement,” Cement and Concrete Research, V. 41, No. 10, Oct. 2011, pp. 1037-1049. doi: 10.1016/j.cemconres.2011.06.004

45. Cabral, A. E. B.; Schalch, V.; Dal Molin, D. C. C.; and Ribeiro, J. L. D., “Mechanical Properties Modeling of Recycled Aggregate Concrete,” Construction and Building Materials, V. 24, No. 4, Apr. 2010, pp. 421-430.

46. Dilbas, H., and Çakır, Ö., “Physical and Mechanical Properties of Treated Recycled Aggregate Concretes: Combination of Mechanical Treatment and Silica Fume,” Journal of Materials in Civil Engineering, ASCE, V. 33, No. 6, June 2021, p. 04021096. doi: 10.1061/(ASCE)MT.1943-5533.0003658

47. Klink, S. A., “Aggregates, Elastic-Modulus, and Poisson’s Ratio of Concrete,” ACI Journal Proceedings, V. 83, No. 6, Nov.-Dec. 1986, pp. 961-965.

48. AASHTO PP 84-17, “Standard Practice for Developing Performance Engineered Concrete Pavement Mixtures,” American Association of State Highway and Transportation Officials, Washington, DC, 2017, 67 pp.

49. Tam, V. W. Y., and Tam, C. M., “Assessment of Durability of Recycled Aggregate Concrete Produced by Two-Stage Mixing Approach,” Journal of Materials Science, V. 42, No. 10, May 2007, pp. 3592-3602. doi: 10.1007/s10853-006-0379-y

50. Liu, J.; Xing, F.; Dong, B.; Ma, H.; and Pan, D., “Study on Surface Permeability of Concrete under Immersion,” Materials (Basel), V. 7, No. 2, Feb. 2014, pp. 876-886. doi: 10.3390/ma7020876

51. Kumar, A.; Singh, G. J.; Kumar, S. B.; and Kumar, R., “Performance-Based Quality Optimization Approach for Mechanically Treated Recycled Concrete Aggregates,” Journal of Materials in Civil Engineering, ASCE, V. 35, No. 9, Sept. 2023, p. 04023315. doi: 10.1061/JMCEE7.MTENG-15284

52. Kumar, A., and Singh G. J., “Recycled Concrete Aggregate Classification Based on Quality Parameters and Performance,” Iranian Journal of Science and Technology, Transactions of Civil Engineering, V. 47, No. 6, Dec. 2023, pp. 3211-3232.

53. Kavitha, O. R.; Shanthi, V. M.; Arulraj, G. P.; and Sivakumar, V. R., “Microstructural Studies on Eco-Friendly and Durable Self-Compacting Concrete Blended with Metakaolin,” Applied Clay Science, V. 124-125, May 2016, pp. 143-149. doi: 10.1016/j.clay.2016.02.011

54. Al-Bayati, H. K. A.; Tighe, S. L.; and Baaj, H., “Effect of Different Treatment Methods on the Interfacial Transition Zone Microstructure to Coarse Recycled Concrete Aggregate,” TAC 2016: Efficient Transportation - Managing the Demand - 2016 Conference and Exhibition of the Transportation Association of Canada, 2016, 29 pp.