Title: ACI CODE-437.2-22: Load Testing of Concrete Structures—Code and Commentary (SI Units)

Author(s): ACI Committee 437

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 26

Keywords:

DOI:

Date: 11/1/2023

Abstract:
This Code provides requirements for test load magnitudes, test protocols, and acceptance criteria for conducting a load test as a means of evaluating the safety and serviceability of concrete structural members and systems of structures. A load test may be conducted as part of a structural evaluation to determine whether a structure requires repair and rehabilitation, or to verify the adequacy of repair and rehabilitation measures. Keywords: acceptance criteria; cyclic loading; load test; monotonic loading; test load magnitude; test protocol.