Response of Reinforced Concrete Shell Elements Subjected to In-Plane and Out-of-Plane Shear

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Response of Reinforced Concrete Shell Elements Subjected to In-Plane and Out-of-Plane Shear

Author(s): Giorgio T. Proestos, Evan C. Bentz, and Michael P. Collins

Publication: Structural Journal

Volume: 121

Issue: 2

Appears on pages(s): 165-180

Keywords: axial stress; experiments; interaction diagrams; moments; shear; shells; three-dimensional; torsion

DOI: 10.14359/51740252

Date: 3/1/2024

Abstract:
This paper investigates the response of reinforced concrete shell elements subjected to all eight stress resultants (in-plane shear, two out-of-plane shears, torsion, two axial loads, and two moments). Twelve new experiments subjected to different combinations of in-plane and out-of-plane loads are presented. The experiments examine the influence of varying quantities of transverse shear reinforcement and concrete strengths. The paper also presents a new nonlinear, high-powered, macro finite element model called Shell II. The Shell II method is a three-layered model based on the equations of the Modified Compression Field Theory and is capable of predicting the full three-dimensional load-deformation response of shell elements subjected to combined loads. Shell II is also used to examine the experimental results in the context of in-plane versus out-of-plane shear-stress interaction diagrams. The results highlight the importance of considering combined loading in predicting the response of shells in three dimensions.

Related References:

1. Vecchio, F. J., and Collins, M. P., “The Modified Compression Field Theory for Reinforced Concrete Elements Subjected to Shear,” ACI Journal Proceedings, V. 83, No. 2, Mar.-Apr. 1986, pp. 219-231.

2. Kaufmann, W., Strength and Deformations of Structural Concrete Subjected to In-Plane Shear and Normal Forces, Birkhäuser Basel, 1998, 149 pp.

3. Kirschner, U., “Investigating the Behaviour of Reinforced Concrete Shell Elements,” PhD thesis, Department of Civil Engineering, University of Toronto, Toronto, ON, Canada, 1986, 208 pp.

4. Polak, M. A., and Vecchio, F. J., “Nonlinear Analysis of Reinforced-Concrete Shells,” Journal of Structural Engineering, ASCE, V. 119, No. 12, 1993, pp. 3439-3462. doi: 10.1061/(ASCE)0733-9445(1993)119:12(3439)

5. Proestos, G. T.; Bae, G. M.; Cho, J. Y.; Bentz, E. C.; and Collins, M. P., “Influence of High-Strength Bars on Shear Response of Containment Walls,” ACI Structural Journal, V. 113, No. 5, Sept.-Oct. 2016, pp. 917-927. doi: 10.14359/51688750

6. Proestos, G. T., “Influence of High-Strength Reinforcing Bars on the Behaviour of Reinforced Concrete Nuclear Containment Structures Subjected to Shear,” MASc thesis, Department of Civil Engineering, University of Toronto, Toronto, ON, Canada, 2014, 155 pp.

7. Adebar, P., and Collins, M. P., “Shear Design of Offshore Structures,” ACI Structural Journal, V. 91, No. 3, May-June 1994, pp. 324-335.

8. Proestos, G. T., “Modelling Reinforced and Prestressed Concrete Structures Subjected to Shear and Torsion,” PhD thesis, University of Toronto, Toronto, ON, Canada, 2018, 332 pp.

9. Ruggiero, D. M., “The Behaviour of Reinforced Concrete Subjected to Reversed Cyclic Shear,” PhD thesis, Department of Civil Engineering, University of Toronto, Toronto, ON, Canada, 2015, 433 pp.

10. Calvi, P. M.; Bentz, E. C.; and Collins, M. P., “Model for Assessment of Cracked Reinforced Concrete Membrane Elements Subjected to Shear and Axial Loads,” ACI Structural Journal, V. 115, No. 2, Mar. 2018, pp. 501-509. doi: 10.14359/51701093

11. Calvi, P. M.; Bentz, E. C.; and Collins, M. P., “Pure Mechanics Crack Model for Shear Stress Transfer in Cracked Reinforced Concrete,” ACI Structural Journal, V. 114, No. 2, Mar.-Apr. 2017, pp. 545-554. doi: 10.14359/51689460

12. Bhide, S. B., and Collins, M. P., “Influence of Axial Tension on the Shear Capacity of Reinforced Concrete Members,” ACI Structural Journal, V. 86, No. 5, Sept.-Oct. 1989, pp. 570-581.

13. Hrynyk, T. D., and Vecchio, F. J., “Capturing Out-of-Plane Shear Failures in the Analysis of Reinforced Concrete Shells,” Journal of Structural Engineering, ASCE, V. 141, No. 12, 2015, p. 04015058.. doi: 10.1061/(ASCE)ST.1943-541X.0001311

14. Hrynyk, T. D., “Behaviour and Modelling of Reinforced Concrete Slabs and Shells Under Static and Dynamic Loads,” PhD thesis, Department of Civil Engineering, University of Toronto, Toronto, ON, Canada, 2013, 436 pp.

15. Vecchio, F. J., “VecTor Suite of Programs,” VecTor Analysis Group, http://www.vectoranalysisgroup.com/. (last accessed Jan. 18, 2024)

16. Vecchio, F. J., “Disturbed Stress Field Model for Reinforced Concrete: Formulation,” Journal of Structural Engineering, ASCE, V. 126, No. 9, 2000, pp. 1070-1077. doi: 10.1061/(ASCE)0733-9445(2000)126:9(1070)

17. CSA A23.3-19, “Design of Concrete Structures,” CSA Group, Toronto, ON, Canada, 2019, 301 pp.

18. AASHTO, “LRFD Bridge Design Specifications and Commentary,” ninth edition, American Association of State Highway Transportation Officials, Washington, DC, 2020, 1914 pp.

19. AS 3600-2018, “Concrete Structures,” Standards Australia, Sydney, NSW, Australia, 2018, 256 pp.

20. Bentz, E. C., “Sectional Analysis of Reinforced Concrete,” PhD thesis, University of Toronto, Department of Civil Engineering, Toronto, ON, Canada, 2000, 316 pp.

21. Vecchio, F. J., “Reinforced Concrete Membrane Element Formulations,” Journal of Structural Engineering, ASCE, V. 116, No. 3, 1990, pp. 730-750. doi: 10.1061/(ASCE)0733-9445(1990)116:3(730)

22. Selby, R. G., “Nonlinear Finite Element Analysis of Reinforced Concrete Solids,” master’s thesis, University of Toronto, Toronto, ON, Canada, 1990, 144 pp.

23. Adebar, P., “Shear Design of Concrete Offshore Structures,” PhD thesis, Department of Civil Engineering, University of Toronto, Toronto, ON, Canada, 1989.

24. Collins, M. P., and Mitchell, D., Prestressed Concrete Structures, Prentice Hall, Englewood Cliffs, NJ, 1991, 766 pp.


ALSO AVAILABLE IN:

Electronic Structural Journal