Shear Strength of Reinforced Concrete Columns with External Post-Tensioned Clamps

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shear Strength of Reinforced Concrete Columns with External Post-Tensioned Clamps

Author(s): Julian D. Rincon, Yu-Mei Chen, Santiago Pujol, Aishwarya Y. Puranam, and Shyh-Jiann Hwang

Publication: Structural Journal

Volume: 121

Issue: 2

Appears on pages(s): 111-125

Keywords: external post-tensioned clamps; lateral prestress; reinforced concrete (RC) columns; retrofit; shear strength

DOI: 10.14359/51740248

Date: 3/1/2024

Abstract:
An alternative method to retrofit reinforced concrete (RC) columns with insufficient shear reinforcement is investigated. The retrofit involves external prestressing of the columns in the transverse direction to increase both shear strength and drift capacity. External post-tensioned clamps, consisting of high-strength steel rods connecting a set of steel angles, were applied around the columns at different spacings and initial post-tensioning stresses. The tension induced in the steel rods exerts lateral confining pressure on the column by bearing of the angles against the corners of the column. Ten RC columns furnished with external post-tensioned clamps were tested under cyclic loads and approximately constant axial loads. In addition, six RC beams with clamps were tested under monotonically increasing loads. Both the column and beam specimens were fabricated with no transverse reinforcement in the form of conventional steel ties. Therefore, the external clamps were the only source of reinforcement resisting shear. The lateral prestress provided by the clamps was observed to increase the shear stress at the formation of the first inclined crack and at failure. As a result, the mode of failure of columns vulnerable in shear changed from shear failure to a more ductile failure dominated by flexure. The observed increase in shear strength is dependent on the lateral prestress and the tensile strength of the concrete. A simple equation, based on the mechanics of materials, is presented to calculate the shear strength of RC columns with external prestressing.




  