Fiber-Reinforced Concrete for Long-Term Durable Structures—Case Studies

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Fiber-Reinforced Concrete for Long-Term Durable Structures—Case Studies

Author(s): Corina-Maria Aldea, Claire Gandee, Beverly Heasley, Heidi Helmink, Carl A. Labbe III, Michael A. Mahoney, Matthew A. Offenberg, and Steve Schaef

Publication: Concrete International

Volume: 45

Issue: 11

Appears on pages(s): 53-59

Keywords: steel, synthetic, durability, project

DOI: 10.14359/51740201

Date: 11/1/2023

Abstract:
Fibers are used to reinforce cementitious materials and to improve their pre- and post-crack behavior. This article highlights the use of fiber reinforcement to enhance durability of concrete structures, as well as benefits of using different types of fibers in projects up to 40 years in service, covering various applications in different geographic locations.

Related References:

1. ACI Committee 544, “Guide for Specifying, Proportioning, and Production of Fiber-Reinforced Concrete (ACI PRC-544.3-08),” American Concrete Institute, Farmington Hills, MI, 2008, 14 pp.

2. ACI Committee 544, “Guide to Design with Fiber-Reinforced Concrete (ACI PRC-544.4-18),” American Concrete Institute, Farmington Hills, MI, 2018, 44 pp.

3. ACI Committee 544, “Report on Fiber Reinforced Concrete (ACI PRC-544.1-96) (Reapproved 2009),” American Concrete Institute, Farmington Hills, MI, 1996, 66 pp.

4. ASTM C1116/C1116M-23, “Standard Specification for Fiber-Reinforced Concrete,” ASTM International, West Conshohocken, PA, 2023, 5 pp.

5. ACI Committee 544, “Report on the Physical Properties and Durability of Fiber-Reinforced Concrete (ACI PRC-544.5-10),” American Concrete Institute, Farmington Hills, MI, 2010, 31 pp.

6. ASTM A820/A820M-22, “Standard Specification for Steel Fibers for Fiber-Reinforced Concrete,” ASTM International, West Conshohocken, PA, 2022, 4 pp.

7. ASTM D7508/D7508M-20, “Standard Specification for Polyolefin Chopped Strands for Use in Concrete,” ASTM International, West Conshohocken, PA, 2020, 4 pp.

8. ASTM C1666/C1666M-08 (Reapproved 2023), “Standard Specification for Alkali Resistant (AR) Glass Fiber for GFRC and Fiber-Reinforced Concrete and Cement,” ASTM International, West Conshohocken, PA, 2023, 4 pp.