Alkali-Silica Reaction Evaluation of Coarse Aggregates from Massachusetts Using Accelerated Tests

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Alkali-Silica Reaction Evaluation of Coarse Aggregates from Massachusetts Using Accelerated Tests

Author(s): J. F. Munoz, C. Balachandran, A. Shastry, R. Mulcahy, J. M. Robertson, and T. S. Arnold

Publication: Materials Journal

Volume: 120

Issue: 6

Appears on pages(s): 129-140

Keywords: alkali-carbonate reaction (ACR); alkali-silica reaction (ASR); alkali threshold (AT); coarse aggregates; miniature concrete prism test (MCPT); Turner-Fairbank Highway Research Center ASR susceptibility test (T-FAST)

DOI: 10.14359/51739152

Date: 12/1/2023

Abstract:
The periodic evaluation of the alkali-silica reaction (ASR) susceptibility of aggregates is a key strategy to eliminate the risk of ASR development in transportation infrastructure. A reliable and practical accelerated ASR test is paramount to improve the frequency and efficiency of the aggregate evaluation campaign. This paper assesses the suitability of the new Turner-Fairbank Highway Research Center ASR susceptibility test (T-FAST) as a costeffective tool to evaluate aggregates. Thirty-eight aggregates of varying mineralogies, including carbonates, were characterized using the T-FAST and AASHTO T 380. The results were compared with historic AASHTO T 303 data. The T-FAST accurately classified the reactivity of the aggregates and was identified as the most sensitive among the three accelerated tests. Additionally, the combination of the T-FAST results with the possibility of accurately determining the alkali thresholds of the aggregates provided a broader understanding of the conditions conducive to triggering ASR in the field.

Related References:

1. Grieco, J., and Mulcahy, R., “The Identification and Prevention of Alkali Silica Reactive (ASR) Aggregates,” 2017 Northeastern States’ Materials Engineers Association (NESMEA) Annual Conference, Hartford, CT, Oct. 17-18, 2017, https://nesmea.engr.uconn.edu/wp-content/uploads/sites/2933/2020/01/Mulcahy-Grieco-Akali-Silica-Reaction-in-Mass.pdf. (last accessed Sept. 26, 2023)

2. Jiang, L.; Sherman, M. R.; and Grieco, J., “Inspection, Risk Assessment, and Management Planning of MassDOT Transportation Structures Affected by Alkali-Silica Reaction,” Transportation Research Board 94th Annual Meeting, Paper No. 15-4927, 2015, 17 pp.

3. AASHTO T 303-00 (2021), “Standard Method of Test for Accelerated Detection of Potentially Deleterious Expansion of Mortar Bars Due to Alkali–Silica Reaction,” American Association of State Highway and Transportation Officials, Washington, DC, 2000, 7 pp.

4. ASTM C295-08, “Standard Guide for Petrographic Examination of Aggregates for Concrete,” ASTM International, West Conshohocken, PA, 2008, 9 pp.

5. Thomas, M. D. A.; Folliard, K. J.; Fournier, B.; Drimalas, T.; and Garber, S. I., “Methods for Preventing ASR in New Construction: Results of Field Exposure Sites,” Report No. FHWA-HIF-14-004, Federal Highway Administration, Washington, DC, 2013, 36 pp.

6. ASTM C1293-20a, “Standard Test Method for Determination of Length Change of Concrete Due to Alkali-Silica Reaction,” ASTM International, West Conshohocken, PA, 2020, 6 pp.

7. Bérubé, M.-A., and Fournier, B., “Canadian Experience with Testing for Alkali-Aggregate Reactivity in Concrete,” Cement and Concrete Composites, V. 15, No. 1-2, 1993, pp. 27-47. doi: 10.1016/0958-9465(93)90037-A

8. Sims, I., and Nixon, P., “RILEM Recommended Test Method AAR-0: Detection of Alkali-Reactivity Potential in Concrete—Outline Guide to the Use of RILEM Methods in Assessments of Aggregates for Potential Alkali-Reactivity,” Materials and Structures, V. 36, No. 7, Aug. 2003, pp. 472-479. doi: 10.1007/BF02481527

9. Thomas, M.; Fournier, B.; Folliard, K.; Ideker, J.; and Shehata, M., “Test Methods for Evaluating Preventive Measures for Controlling Expansion Due to Alkali–Silica Reaction in Concrete,” Cement and Concrete Research, V. 36, No. 10, Oct. 2006, pp. 1842-1856. doi: 10.1016/j.cemconres.2006.01.014

10. AASHTO T 380-19, “Standard Method of Test for Potential Alkali Reactivity of Aggregates and Effectiveness of ASR Mitigation Measures (Miniature Concrete Prism Test, MCPT),” American Association of State Highway and Transportation Officials, Washington, DC, 2019, 10 pp.

11. Latifee, E. R., and Rangaraju, P. R., “Miniature Concrete Prism Test: Rapid Test Method for Evaluating Alkali-Silica Reactivity of Aggregates,” Journal of Materials in Civil Engineering, ASCE, V. 27, No. 7, July 2015, p. 04014215. doi: 10.1061/(ASCE)MT.1943-5533.0001183

12. Konduru, H.; Rangaraju, P.; and Amer, O., “Reliability of Miniature Concrete Prism Test in Assessing Alkali-Silica Reactivity of Moderately Reactive Aggregates,” Transportation Research Record: Journal of the Transportation Research Board, V. 2674, No. 4, Apr. 2020, pp. 23-29. doi: 10.1177/0361198120912247

13. Muñoz, J. F.; Balachandran, C.; and Arnold, T. S., “New Chemical Reactivity Index to Assess Alkali–Silica Reactivity,” Journal of Materials in Civil Engineering, ASCE, V. 33, No. 4, Apr. 2021, p. 04021037. doi: 10.1061/(ASCE)MT.1943-5533.0003640

14. Muñoz, J. F.; Balachandran, C.; and Arnold, T. S., “New Turner-Fairbank Alkali-Silica Reaction Susceptibility Test for Aggregate Evaluation,” Transportation Research Record: Journal of the Transportation Research Board, V. 2675, No. 9, Sept. 2021, pp. 798-808. doi: 10.1177/03611981211004584

15. AASHTO TP 144-21, “Standard Method of Test for Determining the Potential Alkali–Silica Reactivity of Coarse Aggregates (TFHRC-TFAST),” American Association of State Highway and Transportation Officials, Washington, DC, 2021, 10 pp.

16. AASHTO, “Standard Specifications for Transportation Materials and Methods of Sampling and Testing and AASHTO Provisional Standards,” 41st edition, American Association of State Highway and Transportation Officials, Washington, DC, 2021.

17. Muñoz, J. F.; Balachandran, C.; Beyene, M.; and Arnold, T. S., “A Novel Approach for the Assessment of ASR Susceptibility of Concrete Mixtures in Airfield Pavements and Infrastructure,” Report No. FHWA-HRT-21-103, Federal Highway Administration, Washington, DC, 2021, 90 pp.

18. Lindgård, J.; Nixon, P. J.; Borchers, I.; Schouenborg, B.; Wigum, B. J.; Haugen, M.; and Åkesson, U., “The EU ‘PARTNER’ Project—European Standard Tests to Prevent Alkali Reactions in Aggregates: Final Results and Recommendations,” Cement and Concrete Research, V. 40, No. 4, Apr. 2010, pp. 611-635. doi: 10.1016/j.cemconres.2009.09.004

19. Nixon, P., and Fournier, B., “Assessment, Testing and Specification,” Alkali-Aggregate Reaction in Concrete: A World Review, I. Sims and A. Poole, eds., CRC Press, London, UK, 2017, pp. 33-61.

20. Deschenes, R. A. Jr., and Hale, W. M., “Alkali-Silica Reaction in Concrete with Previously Inert Aggregates,” Journal of Performance of Constructed Facilities, ASCE, V. 31, No. 2, Apr. 2017, p. 04016084. doi: 10.1061/(ASCE)CF.1943-5509.0000946

21. Muñoz, J. F.; Balachandran, C.; Lichtenwalner, R. L.; Li, Z.; and Arnold, T. S., “Optimization of Parameters of the New Tuner-Fairbank Alkali-Silica Reactivity Susceptibility Test (T-Fast),” Journal of Testing and Evaluation, V. 51, No. 2, Mar. 2023, 16 pp. doi: 10.1520/JTE20220033

22. Folliard, K. J.; Barborak, R.; Drimalas, T.; Du, L.; Garber, S.; Ideker, J.; Ley, T.; Williams, S.; Juenger, M. C.; Fournier, B.; and Thomas, M. D. A., “Preventing ASR/DEF in New Concrete: Final Report,” Report No. FHWA/TX-06/0-4085-5, Center for Transportation Research, The University of Texas at Austin, Austin, TX, 2006, 266 pp.

23. Ideker, J. H.; Bentivegna, A. F.; Folliard, K. J.; and Juenger, M. C. G., “Do Current Laboratory Test Methods Accurately Predict Alkali-Silica Reactivity?” ACI Materials Journal, V. 109, No. 4, July-Aug. 2012, pp. 395-402.

24. AASHTO R 90-18 (2022), “Standard Practice for Sampling Aggregate Products,” American Association of State Highway and Transportation Officials, Washington, DC, 2018, 6 pp.

25. AASHTO R 76-16 (2020), “Standard Practice for Reducing Samples of Aggregate to Testing Size,” American Association of State Highway and Transportation Officials, Washington, DC, 2016, 8 pp.

26. Kim, T., and Olek, J., “Effects of Sample Preparation and Interpretation of Thermogravimetric Curves on Calcium Hydroxide in Hydrated Pastes and Mortars,” Transportation Research Record: Journal of the Transportation Research Board, V. 2290, No. 1, Jan. 2012, pp. 10-18. doi: 10.3141/2290-02

27. Haxel, G. B.; Hedrick, J. B.; and Orris, G. J., “Rare Earth Elements—Critical Resources for High Technology,” Fact Sheet 087-02, U.S. Geological Survey, Reston, VA, 2002, https://pubs.usgs.gov/fs/2002/fs087-02/. (last accessed Sept. 26, 2023)

28. Kaladharan, G.; Szeles, T.; Stoffels, S. M.; and Rajabipour, F., “Novel Admixtures for Mitigation of Alkali-Silica Reaction in Concrete,” Cement and Concrete Composites, V. 120, July 2021, Article No. 104028. doi: 10.1016/j.cemconcomp.2021.104028

29. Broekmans, M. A. T. M., “Structural Properties of Quartz and Their Potential Role for ASR,” Materials Characterization, V. 53, No. 2-4, Nov. 2004, pp. 129-140. doi: 10.1016/j.matchar.2004.08.010

30. Fernandes, I.; Broekmans, M. A. T. M.; Nixon, P.; Sims, I.; dos Anjos Ribeiro, M.; Noronha, F.; and Wigum, B., “Alkali–Silica Reactivity of Some Common Rock Types. A Global Petrographic Atlas,” Quarterly Journal of Engineering Geology and Hydrogeology, V. 46, No. 2, May 2013, pp. 215-220. doi: 10.1144/qjegh2012-065

31. Rajabipour, F.; Giannini, E.; Dunant, C.; Ideker, J. H.; and Thomas, M. D. A., “Alkali–Silica Reaction: Current Understanding of the Reaction Mechanisms and the Knowledge Gaps,” Cement and Concrete Research, V. 76, Oct. 2015, pp. 130-146. doi: 10.1016/j.cemconres.2015.05.024

32. Tiecher, F.; Florindo, R. N.; Vieira, G. L.; Gomes, M. E. B.; Dal Molin, D. C. C.; and Lermen, R. T., “Influence of the Quartz Deformation Structures for the Occurrence of the Alkali–Silica Reaction,” Materials (Basel), V. 11, No. 9, Sept. 2018, Article No. 1692. doi: 10.3390/ma11091692

33. Fanijo, E. O.; Kolawole, J. T.; and Almakrab, A., “Alkali-Silica Reaction (ASR) in Concrete Structures: Mechanisms, Effects and Evaluation Test Methods Adopted in the United States,” Case Studies in Construction Materials, V. 15, Dec. 2021, Article No. e00563. doi: 10.1016/j.cscm.2021.e00563

34. Katayama, T., “A Critical Review of Carbonate Rock Reactions—Is Their Reactivity Useful or Harmful?” Proceedings of the 9th International Conference on Alkali-Aggregate Reaction, A. B. Poole, ed., London, UK, July 1992, pp. 508-518.

35. Katayama, T., “Modern Petrography of Carbonate Aggregates in Concrete–Diagnosis of So-Called Alkali-Carbonate Reaction and Alkali-Silica Reaction,” Proceedings, Marc-André Bérubé Symposium on Alkali-Aggregate Reactivity in Concrete, Montreal, QC, Canada, May 2006, pp. 423-444.

36. Grattan-Bellew, P. E.; Mitchell, L. D.; Margeson, J.; and Min, D., “Is Alkali–Carbonate Reaction Just a Variant of Alkali–Silica Reaction ACR = ASR?” Cement and Concrete Research, V. 40, No. 4, Apr. 2010, pp. 556-562. doi: 10.1016/j.cemconres.2009.09.002

37. Katayama, T., “The So-Called Alkali-Carbonate Reaction (ACR)—Its Mineralogical and Geochemical Details, with Special Reference to ASR,” Cement and Concrete Research, V. 40, No. 4, Apr. 2010, pp. 643-675. doi: 10.1016/j.cemconres.2009.09.020

38. Gillott, J. E., “Petrology of Dolomitic Limestones, Kingston, Ontario, Canada,” Geological Society of America Bulletin, V. 74, No. 6, 1963, pp. 759-778. doi: 10.1130/0016-7606(1963)74[759:PODLKO]2.0.CO;2

39. Marinoni, N., and Broekmans, M. A. T. M., “Microstructure of Selected Aggregate Quartz by XRD, and a Critical Review of the Crystallinity Index,” Cement and Concrete Research, V. 54, Dec. 2013, pp. 215-225. doi: 10.1016/j.cemconres.2013.08.007

40. Rogers, C. A., “Multi-Laboratory Study of the Accelerated Mortar Bar Test for Alkali-Silica Reaction,” Proceedings of the 10th International Conference on Alkali-Aggregate Reaction, A. Shayan, ed., Melbourne, VIC, Australia, 1996, pp. 362-369.

41. Fournier, B.; Chevrier, R.; DeGrosbois, M.; Lisella, R.; Folliard, K.; Ideker, J. H.; Shehata, M.; Thomas, M.; and Baxter, S., “The Accelerated Concrete Prism Test (60°C): Variability of the Test Method and Proposed Expansion Limits,” Proceedings of the 12th International Conference on Alkali-Aggregate Reaction in Concrete, Beijing, China, Oct. 15-19, 2004.

42. Sims, I., and Nixon, P. J., “Assessment of Aggregates for Alkali–Aggregate Reactivity Potential: RILEM International Recommendations,” Proceedings, 8th CANMET/ACI International Conference on Recent Advances in Concrete Technology, Montreal, QC, Canada, May-June 2006.

43. FHWA-TFHRC Aggregate and Petrography Laboratory, “Petrographic Analyses Report of MassDOT ASR Study Aggregates,” Turner-Fairbank Highway Research Center, Federal Highway Administration, McLean, VA, 2022.

44. Broekmans, M. A. T. M.; Fernandes, I.; and Nixon, P., “A Global Petrographic Atlas of Alkali-Silica Reactive Rock Types: A Brief Review,” Proceedings of the 12th Euroseminar on Microscopy Applied to Building Materials, B. Middendorf, A. Just, D. Klein, A. Glaubitt, and J. Simon, eds., Dortmund, Germany, Sept. 2009, pp. 39-50.

45. CSA A23.1:19/CSA A23.2:19, “Concrete Materials and Methods of Concrete Construction/Test Methods and Standard Practices for Concrete,” CSA Group, Toronto, ON, Canada, 2019.

46. Sibbick, R. G., and Page, C. L., “Threshold Alkali Contents for Expansion of Concretes Containing British Aggregates,” Cement and Concrete Research, V. 22, No. 5, Sept. 1992, pp. 990-994. doi: 10.1016/0008-8846(92)90123-D

47. Lindgård, J.; Andiç-Çakır, Ö.; Fernandes, I.; Rønning, T. F.; and Thomas, M. D. A., “Alkali–Silica Reactions (ASR): Literature Review on Parameters Influencing Laboratory Performance Testing,” Cement and Concrete Research, V. 42, No. 2, Feb. 2012, pp. 223-243. doi: 10.1016/j.cemconres.2011.10.004

48. Thomas, M. D. A.; Fournier, B.; and Folliard, K. J., “Alkali-Aggregate Reactivity (AAR) Facts Book,” Report No. FHWA-HIF-13-019, Office of Pavement Technology, Federal Highway Administration, Washington, DC, 2013, 224 pp.

49. Johnson, S., and Chau, K., “More U.S. Coal-Fired Power Plants are Decommissioning as Retirements Continue,” Today in Energy, U.S. Energy Information Administration, Washington, DC, July 26, 2019, https://www.eia.gov/todayinenergy/detail.php?id=40212. (last accessed Sept. 26, 2023)

50. Kaladharan, G.; Gholizadeh-Vayghan, A.; and Rajabipour, F., “Review, Sampling, and Evaluation of Landfilled Fly Ash,” ACI Materials Journal, V. 116, No. 4, July 2019, pp. 113-122. doi: 10.14359/51716750

51. Al-Shmaisani, S.; Kalina, R.; O’Quinn, K.; Jang, J. K.; Rung, M.; Ferron, R.; and Juenger, M., “Supplementary Cementitious Materials: Assessment of Test Methods for New and Blended Materials,” Report No. FHWA/TX-21/0-6966-1, Center for Transportation Research, The University of Texas at Austin, Austin, TX, 2021, 108 pp.


ALSO AVAILABLE IN:

Electronic Materials Journal