Automated Procedure to Identify Concrete Defects from Impact-Echo Data

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Automated Procedure to Identify Concrete Defects from Impact-Echo Data

Author(s): Zachary W. Coleman and Anton K. Schindler

Publication: Materials Journal

Volume: 120

Issue: 6

Appears on pages(s): 95-106

Keywords: bridge decks; condition assessment; corrosion; delamination; nondestructive testing; voids

DOI: 10.14359/51739149

Date: 12/1/2023

Abstract:
In this study, a procedure for interpreting impact-echo data in an automated, simple manner for detecting defects in concrete bridge decks is presented. Such a procedure is needed because it can be challenging for inexperienced impact-echo users to correctly distinguish between sound and defective concrete. This data interpretation procedure was developed considering the statistical nature of impact-echo data in a manner to allow impact-echo users of all skill levels to understand and implement the procedure. The developed method predominantly relies on conducting segmented linear regression analysis of the cumulative probabilities of an impact-echo data set to identify frequency thresholds distinguishing sound concrete from defective concrete. The accuracy of this method was validated using two case studies of five slab specimens and a full-scale bridge deck, each containing various typical defects. The developed procedure was found to be able to predict the condition of the slab specimens containing shallow delaminations without human assistance within 3.1 percentage points of the maximum attainable accuracy. It was also able to correctly predict the condition of the full-scale bridge deck containing delaminations, voids, corrosion damage, concrete deterioration, and poorly constructed concrete within 3.5 percentage points of the maximum attainable accuracy.

Related References:

ACI Committee 228, 2013, “Report on Nondestructive Test Methods for Evaluation of Concrete in Structures (ACI 228.2R-13),” American Concrete Institute, Farmington Hills, MI, 82 pp.

ASTM C1383-15, 2015, “Standard Test Method for Measuring the P-Wave Speed and the Thickness of Concrete Plates Using the Impact-Echo Method,” ASTM International, West Conshohocken, PA, 11 pp.

Azari, H., and Lin, S., 2019, “Evaluation of the Impact Echo Method for Concrete Bridge Decks with Asphalt Overlays,” Transportation Research Record: Journal of the Transportation Research Board, V. 2673, No. 2, Feb., pp. 436-444. doi: 10.1177/0361198119828676

Carino, N. J., 2001, “The Impact-Echo Method: An Overview,” Structures 2001: Proceedings of the 2001 Structures Congress and Exposition, P. C. Chang, ed., Washington, DC, 18 pp.

Cheng, C., and Sansalone, M., 1993, “The Impact-Echo Response of Concrete Plates Containing Delaminations: Numerical, Experimental and Field Studies,” Materials and Structures, V. 26, No. 5, June, pp. 274-285. doi: 10.1007/BF02472949

Coleman, Z. W., 2021, “Evaluation of Nondestructive Test Methods for Concrete Bridge Deck Condition Assessment,” master’s thesis, Auburn University, Auburn, AL, 389 pp.

Coleman, Z. W., and Schindler, A. K., 2022, “Investigation of Ground-Penetrating Radar, Impact Echo, and Infrared Thermography Methods to Detect Defects in Concrete Bridge Decks,” Transportation Research Record: Journal of the Transportation Research Board, pre-print, 14 pp. doi: 10.1177/03611981221101027

Coleman, Z. W.; Jetzel, C. M.; and Schindler, A. K., 2022, “Evaluation of Nondestructive Test Methods to Assess the In-Place Condition of Concrete Structures,” ALDOT Research Report ALDOT 930-951, Highway Research Center, Auburn University, Auburn, AL, 244 pp.

Coleman, Z. W.; Schindler, A. K.; and Jetzel, C. M., 2021, “Impact-Echo Defect Detection in Reinforced Concrete Bridge Decks without Overlays,” Journal of Performance of Constructed Facilities, ASCE, V. 35, No. 5, Oct., p. 04021058. doi: 10.1061/(ASCE)CF.1943-5509.0001638

Dorafshan, S., and Azari, H., 2020, “Deep Learning Models for Bridge Deck Evaluation Using Impact Echo,” Construction and Building Materials, V. 263, Dec., Article No. 120109. doi: 10.1016/j.conbuildmat.2020.120109

Gibson, A., and Popovics, J. S., 2005, “Lamb Wave Basis for Impact-Echo Method Analysis,” Journal of Engineering Mechanics, ASCE, V. 131, No. 4, Apr., pp. 438-443. doi: 10.1061/(ASCE)0733-9399(2005)131:4(438)

Gucunski, N.; Imani, A.; Romero, F.; Nazarian, S.; Yuan, D.; Wiggenhauser, H.; Shokouhi, P.; Taffe, A.; and Kutrubes, D., 2013, “Nondestructive Testing to Identify Concrete Bridge Deck Deterioration,” Strategic Highway Research Program 2 (SHRP 2) Report S2-R06A-RR-1, Transportation Research Board, Washington, DC, 96 pp.

Gucunski, N.; Slabaugh, G.; Wang, Z.; Fang, T.; and Maher, A., 2008, “Impact Echo Data from Bridge Deck Testing: Visualization and Interpretation,” Transportation Research Record: Journal of the Transportation Research Board, V. 2050, No. 1, Jan., pp. 111-121. doi: 10.3141/2050-11

Gumbel, E. J., 1954, “Statistical Theory of Extreme Values and Some Practical Applications: A Series of Lectures,” Applied Mathematics Series, V. 33, National Bureau of Standards, Washington, DC, 60 pp.

Hashimoto, K.; Shiotani, T.; and Ohtsu, M., 2020, “Application of Impact-Echo Method to 3D SIBIE Procedure for Damage Detection in Concrete,” Applied Sciences, V. 10, No. 8, Article No. 2729.

Lin, J.-M., and Sansalone, M., 1996, “Impact-Echo Studies of Interfacial Bond Quality in Concrete: Part 1—Effects of Unbonded Fraction of Area,” ACI Materials Journal, V. 93, No. 3, May-June, pp. 223-231.

Lin, S.; Meng, D.; Choi, H.; Shams, S.; and Azari, H., 2018, “Laboratory Assessment of Nine Methods for Nondestructive Evaluation of Concrete Bridge Decks with Overlays,” Construction and Building Materials, V. 188, Nov., pp. 966-982. doi: 10.1016/j.conbuildmat.2018.08.127

Muggeo, V. M. R., 2003, “Estimating Regression Models with Unknown Break-Points,” Statistics in Medicine, V. 22, No. 19, pp. 3055-3071. doi: 10.1002/sim.1545

Muggeo, V. M. R., 2022, “Package ‘Segmented’: Regression Models with Break-Points/Change-Points (with Possibly Random Effects) Estimation,” The Comprehensive R Archive Network (CRAN), https://cran.r-project.org/web/packages/segmented/index.html. (last accessed Sept. 21, 2023)

Nowak, A. S., and Collins, K. R., 2013, Reliability of Structures, CRC Press, Boca Raton, FL, 407 pp.

Ohtsu, M., and Watanabe, T., 2002, “Stack Imaging of Spectral Amplitudes Based on Impact-Echo for Flaw Detection,” NDT & E International, V. 35, No. 3, Apr., pp. 189-196. doi: 10.1016/S0963-8695(01)00045-7

Ohtsu, M.; Yamada, M.; and Sonoda, T., 2013, “Quantitative Evaluation of SIBIE Procedure and Case Studies,” Construction and Building Materials, V. 48, Nov., pp. 1248-1254. doi: 10.1016/j.conbuildmat.2012.12.003

Olson, L. D.; Tinkey, Y.; and Miller, P., 2011, “Concrete Bridge Condition Assessment with Impact Echo Scanning,” Emerging Technologies for Material, Design, Rehabilitation, and Inspection of Roadway Pavements: Proceedings of GeoHunan 2011 International Conference, D.-H. Chen, J.-R. Chang, M. Zaman, C. Zhao, and Z. Yao, eds., Hunan, China, pp. 59-66.

Pratt, D., and Sansalone, M., 1992, “Impact-Echo Signal Interpretation Using Artificial Intelligence,” ACI Materials Journal, V. 89, No. 2, Mar.-Apr., pp. 178-187.

Sansalone, M., 1997, “Impact-Echo: The Complete Story,” ACI Structural Journal, V. 94, No. 6, Nov.-Dec., pp. 777-785.

Sansalone, M., and Carino, N. J., 1989, “Detecting Delaminations in Concrete Slabs with and without Overlays Using the Impact-Echo Method,” ACI Materials Journal, V. 86, No. 2, Mar.-Apr., pp. 175-184.

Sansalone, M., and Street, W. B., 1997, Impact-Echo: Nondestructive Evaluation of Concrete and Masonry, Bullbrier Press, Jersey Shore, PA, 339 pp.

Sengupta, A.; Guler, S. I.; and Shokouhi, P., 2021, “Interpreting Impact Echo Data to Predict Condition Rating of Concrete Bridge Decks: A Machine-Learning Approach,” Journal of Bridge Engineering, ASCE, V. 26, No. 8, Aug., p. 04021044. doi: 10.1061/(ASCE)BE.1943-5592.0001744

Tawhed, W. F., and Gassman, S. L., 2002, “Damage Assessment of Concrete Bridge Decks Using Impact-Echo Method,” ACI Materials Journal, V. 99, No. 3, May-June, pp. 273-281.

Tinkey, Y., and Olson, L. D., 2007, “Impact-Echo Scanning for Grout Void Detection in Post-Tensioned Bridge Ducts — Findings from a Research Project and a Case History,” New Horizons and Better Practices: Proceedings of the 2007 Structures Congress, R. Lyons, ed., Long Beach, CA, 13 pp.

Xie, Z.; Zhang, Y.; and Wu, H. F., 2012, “Automated Data Fusion and Visualization for Impact-Echo Testing of Concrete Structures,” IEEE Sensors Journal, V. 12, No. 12, Dec., pp. 3446-3453. doi: 10.1109/JSEN.2012.2210705

Yamada, M.; Yagi, Y.; and Ohtsu, M., 2017, “Identification of Delamination in Concrete Slabs by SIBIE Procedure,” Proceedings, 12th International Conference on Damage Assessment of Structures, Kitakyushu, Japan, 6 pp.

Zhang, Y.; Wei, X.; Tsai, Y.-T.; Zhu, J.; Fetrat, F. A.; and Gucunski, N., 2012, “Multisensor Data Fusion for Impact-Echo Testing of Concrete Structures,” Smart Materials and Structures, V. 21, No. 7, July, Article No. 075021. doi: 10.1088/0964-1726/21/7/075021

Zou, C.; Chen, Z.; Dong, P.; Chen, C.; and Cheng, Y., 2016, “Experimental and Numerical Studies on Nondestructive Evaluation of Grout Quality in Tendon Ducts Using Impact-Echo Method,” Journal of Bridge Engineering, ASCE, V. 21, No. 2, Feb., p. 04015040. doi: 10.1061/(ASCE)BE.1943-5592.0000759


ALSO AVAILABLE IN:

Electronic Materials Journal