Family of Thermal Nomograms for Mass Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Family of Thermal Nomograms for Mass Concrete

Author(s): J. Brown, L. E. Al-Hasani, J. Park, K. E. Kurtis, R. Gentry, and Y. K. Cho

Publication: Materials Journal

Volume: 120

Issue: 6

Appears on pages(s): 81-94

Keywords: mass concrete; nomograms; thermal management

DOI: 10.14359/51739148

Date: 12/1/2023

Abstract:
Thermal management of mass concrete can adversely impact a project’s cost and schedule, both during planning and in execution. Nomograms are presented as aids to quickly identifying and making tradeoffs among promising thermal management options. First, the temperature of fresh concrete and a worst-case adiabatic temperature estimate is provided by a nomogram based on simple physical models. A subsequent nomogram accounts for the impact of size, shape, and environment and is based on a surrogate model generated from many three-dimensional (3-D) finite element simulations without postcooling. Finally, nomograms for postcooling are given, similarly founded on finite element-derived surrogate models, for two classes of cooling pipe layouts. The use of these nomograms, with an awareness of their estimated error, is discussed for the initial development of mass concrete thermal management plans.

Related References:

1. ACI Committee 207, “Guide to Mass Concrete (ACI 207.1R-05),” American Concrete Institute, Farmington Hills, MI, 2006, 30 pp.

2. ACI Committee 207, “Report on Thermal and Volume Change Effects on Cracking of Mass Concrete (ACI 207.2R-07),” American Concrete Institute, Farmington Hills, MI, 2007, 28 pp.

3. Collepardi, M., “A State-of-the-Art Review on Delayed Ettringite Attack on Concrete,” Concrete Durability, V. 25, No. 4, 2003, pp. 401-407. doi: 10.1016/S0958-9465(02)00080-X

4. American Concrete Institute, “ACI Concrete Terminology (ACI CT-21),” ACI, Farmington Hills, MI, 2021, 80 pp.

5. ACI Committee 207, “Cooling and Insulating Systems for Mass Concrete (ACI 207.4R-20),” American Concrete Institute, Farmington Hills, MI, 2020, 20 pp.

6. Evesham, H. A., The History and Development of Nomography, Docent Press, LLC, Boston, MA, 1982.

7. Hankins, T. L., “Blood, Dirt, and Nomograms: A Particular History of Graphs,” Isis, V. 90, No. 1, 1999, pp. 50-80. doi: 10.1086/384241

8. Brodetsky, S., A First Course in Nomography, George Bell & Sons, London, UK, 1920.

9. Balachandran, V. P.; Gonen, M.; Smith, J. J.; and DeMatteo, R. P., “Nomograms in Oncology: More Than Meets the Eye,” The Lancet. Oncology, V. 16, No. 4, 2015, pp. e173-e180. doi: 10.1016/S1470-2045(14)71116-7

10. Kosmatka, S. H., Design and Control of Concrete Mixtures, 13th edition, Portland Cement Association, Skokie, IL, 1992.

11. Silva, W. R. L., and Šmilauer, V., “Nomogram for Maximum Temperature of Mass Concrete,” Concrete International, V. 37, No. 5, May 2015, pp. 30-36.

12. Nguyen, T.-C.; Nguyen, V.-Q.; Aniskin, N.; Phung, B.-T.; and Hoang, Q.-L., “Building a Nomogram to Predict Maximum Temperature in Mass Concrete at an Early Age,” E3S Web Conference, V. 263, 2021, 10 pp.

13. Roschier, L., and Boulet, D., “pyNomo,” 2020.

14. Riding, K. A.; Poole, J. L.; and Folliard, K. J.; Juenger, M. C. G.; and Schindler, A. K., “New Model for Estimating Apparent Activation Energy of Cementitious Systems,” ACI Materials Journal, V. 108, No. 5, Sept.-Oct. 2011, pp. 550-557.

15. Riding, K. A.; Poole, J. L.; and Folliard, K. J.; Juenger, M. C. G.; and Schindler, A. K., “Modeling Hydration of Cementitious Systems,” ACI Materials Journal, V. 109, No.  2, Mar.-Apr. 2012, pp. 225-234.

16. Xu, Q.; Wang, K.; Medina, C.; and Engquist, B., “A Mathematical Model to Predict Adiabatic Temperatures from Isothermal Heat Evolutions with Validation for Cementitious Materials,” International Journal of Heat and Mass Transfer, V. 89, 2015, pp. 333-338. doi: 10.1016/j.ijheatmasstransfer.2015.05.035

17. Al-Hasani, L. E.; Park, J.; Perez, G.; Herndon, H. N.; Brown, J. B.; Cho, Y. K.; Gentry, T. R.; and Kurtis, K. E., “Quantifying Concrete Adiabatic Temperature Rise Based on Temperature-Dependent Isothermal Calorimetry; Modeling and Validation,” Materials and Structures, V. 55, No. 7, 2022, p. 191. doi: 10.1617/s11527-022-02023-6

18. Cervera, M.; Oliver, J.; and Prato, T., “Thermo-Chemo-Mechanical Model for Concrete. I: Hydration and Aging,” Journal of Engineering Mechanics, ASCE, V. 125, No. 9, 1999, pp. 1018-1027. doi: 10.1061/(ASCE)0733-9399(1999)125:9(1018)

19. Scrivener, K.; Ouzia, A.; Juilland, P.; and Kunhi Mohamed, A., “Advances in Understanding Cement Hydration Mechanisms,” Cement and Concrete Research, V. 124, 2019, p. 105823. doi: 10.1016/j.cemconres.2019.105823

20. Zhou, W.; Feng, C.; Liu, X.; Liu, S.; and Zhang, C., “A Macro–Meso Chemo-Physical Analysis of Early-Age Concrete Based on a Fixed Hydration Model,” Magazine of Concrete Research, V. 68, No. 19, 2016, pp. 981-994. doi: 10.1680/jmacr.15.00321

21. Zhou, W.; Tian, W.; Qi, T.; Liu, S.; Feng, C.; Ma, G.; and Chang, X., “Investigation on Hydration and Mechanical Properties of Mortar Containing Limestone Powder and Fly Ash Based on the Coupled Chemical–Thermal–Mechanical Method,” Materials (Basel), V. 13, No. 19, 2020, p. 4387. doi: 10.3390/ma13194387

22. Logg, A.; Kent-Andre, M.; and Wells, G. N., Automated Solution of Differential Equations by the Finite Element Method, Springer, New York, 2012.

23. Alnæs, M. S.; Blechta, J.; Hake, J.; Johansson, A.; Kehlet, B.; Logg, A.; Richardson, C.; Ring, J.; Rognes, M. E.; and Wells, G. N., “The FEniCS Project version 1.5,” Archive of Numerical Software, V. 3, 2015.

24. Buckingham, E., “On Physically Similar Systems; Illustrations of the Use of Dimensional Equations,” Physical Review, V. 4, No. 4, 1914, pp. 345-376. doi: 10.1103/PhysRev.4.345

25. Sonin, A., “A Generalization of the Pi-Theorem and Dimensional Analysis,” Proceedings of the National Academy of Sciences of the United States of America, V. 101, No. 23, 2004, pp. 8525-8526. doi: 10.1073/pnas.0402931101

26. Seabold, S., and Perktold, J., “Statsmodels: Econometric and Statistical Modeling with Python,” 9th Python in Science Conference, Austin, TX, 2010.

27. Myers, T. G.; Fowkes, N. D.; and Ballim, Y., “Modeling the Cooling of Concrete by Piped Water,” Journal of Engineering Mechanics, ASCE, V. 135, No. 12, 2009, pp. 1375-1383. doi: 10.1061/(ASCE)EM.1943-7889.0000046

28. Incropera, F. P., and DeWitt, D. P., Introduction to Heat Transfer, John Wiley & Sons, Inc., New York, 1990.

29. Saleh, J. M., “Heat Transfer in Pipe Flow,” Fluid Flow Handbook, first edition, McGraw-Hill Education, New York, 2002.

30. Silcox, G. D.; Noble, J. J.; Sarofim, A. F.; Wankat, P. C.; and Knaebel, K. S., “Heat Transfer by Convection,” D. W. Green and M. Z. Southard, eds., Perry’s Chemical Engineers’ Handbook, ninth edition, McGraw-Hill Education, New York, 2019.

31. Burns, K. J.; Vasil, G. M.; Oishi, J. S.; Lecoanet, D.; and Brown, B. P., “Dedalus: A Flexible Framework for Numerical Simulations with Spectral Methods,” Physical Review Research, V. 2, No. 2, 2020, p. 023068. doi: 10.1103/PhysRevResearch.2.023068

32. Giunta, A.; Wojtkiewicz, S.; and Eldred, M., “Overview of Modern Design of Experiments Methods for Computational Simulations (Invited),” 41st Aerospace Sciences Meeting and Exhibit, American Institute of Aeronautics and Astronautics, Reston, VA, 2003.

33. Viana, F. A. C., “A Tutorial on Latin Hypercube Design of Experiments,” Quality and Reliability Engineering International, V. 32, No. 5, 2016, pp. 1975-1985. doi: 10.1002/qre.1924

34. Haji-Sheikh, A., “Temperature and Heat Flux Solutions in Two-Layer Concentric Hollow Cylinders with Prescribed Surface Conditions and Volumetric Heat Sources,” Technical Report, University of Nebraska-Lincoln, Lincoln, NE, Sept. 2014, https://mme-exact.unl.edu/. (last accessed Oct. 19, 2023)


ALSO AVAILABLE IN:

Electronic Materials Journal