Pyrrhotite in Concrete Aggregates

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Pyrrhotite in Concrete Aggregates

Author(s): Anthony F. Bentivegna, April Snyder, and Stephen M. Stacey

Publication: Concrete International

Volume: 45

Issue: 8

Appears on pages(s): 37-44

Keywords: mineral, sulfide, deterioration, reaction

DOI: 10.14359/51739100

Date: 8/1/2023

Abstract:
Concrete aggregates produced in two regions in North America have been identified as the cause of deterioration to tens of thousands of residential and light commercial concrete foundations. The article provides an overview of the deterioration mechanism, manifestations of the reaction in North America, current state of knowledge for identification and quantification, and current and proposed legislation.

Related References:

1. Substitute House Bill No. 6646, Connecticut Public Act No. 21-120: “An Act Concerning Crumbling Concrete Foundations,” State of Connecticut, July 6, 2021, 10 pp., www.cga.ct.gov/2021/act/Pa/pdf/2021PA-00120-R00HB-06646-PA.PDF.

2. Massachusetts Senate Bill No. 548, “An Act Relative to Crumbling Concrete Foundations,” The Commonwealth of Massachusetts, Feb. 18, 2021, 7 pp., https://malegislature.gov/Bills/192/S548.

3. Rodrigues, A.; Duchesne, J.; Fournier, B.; Durand, B.; Rivard, P.; and Shehata, M., “Mineralogical and Chemical Assessment of Concrete Damaged by the Oxidation of Sulfide-Bearing Aggregates: Importance of Thaumasite Formation on Reaction Mechanisms,” Cement and Concrete Research, V. 42, No. 10, Oct. 2012, pp. 1336-1347.

4. ASTM C295/C295M-19, “Standard Guide for Petrographic Examination of Aggregates for Concrete,” ASTM International, West Conshohocken, PA, 2019, 9 pp.

5. MNL-117-13, “Manual for Quality Control for Plants and Production of Architectural Precast Concrete Products,” fourth edition, Precast/Prestressed Concrete Institute, Chicago, IL, 2013, 334 pp.

6. Belzile, N.; Chen, Y.; Cai, M.; and Li, Y., “A Review on Pyrrhotite Oxidation,” Journal of Geochemical Exploration, V. 84, No. 2, Sep. 2004, pp. 65-76.

7. Blowes, D.W.; Ptacek, C.J.; Jambor, J.L.; and Weisener, C.G., “The Geochemistry of Acid Mine Drainage,” Treatise on Geochemistry, V. 9, B. Sherwood Loilar, ed., H.D. Holland and K.K. Turekian, executive eds., Elsevier, Amsterdam, the Netherlands, 2003, pp. 149-204.

8. Grattan-Bellew, P.E., and Eden, W.J., “Concrete Deterioration and Floor Heave Due to Biogeochemical Weathering of Underlying Shale,” Canadian Geotechnical Journal, V. 12, No. 3, Aug. 1975, pp. 372-378.

9. Shayan, A., “Deterioration of a Concrete Surface due to the Oxidation of Pyrite Contained in Pyritic Aggregates,” Cement and Concrete Research, V. 18, No, 5, Sept. 1988, pp. 723-730.

10. Casanova, I.; Agullo, L.; and Aguado, A., “Aggregate Expansivity Due to Sulfide Oxidation—I. Reaction System and Rate Model,” Cement and Concrete Research, V. 26, No. 7, July 1996, pp. 993-998.

11. “Solving the Pyrrhotite Issue in Canada,” National Research Council of Canada, Ottawa, ON, Canada, May 2019, https://nrc.canada.ca/en/certifications-evaluations-standards/codes-canada/construction-innovation/solving-pyrrhotite-issue-canada.

12. “Crumbling Foundations,” Connecticut State Department of Housing, Hartford, CT, https://portal.ct.gov/DOH/DOH/Programs/Crumbling-Foundations, accessed May 24, 2023.

13. U.S. Government Accountability Office, “Crumbling Foundations: Extent of Homes with Defective Concrete Is Not Fully Known and Federal Options to Aid Homeowners Are Limited,” July 2020, https://www.gao.gov/products/gao-20-649.

14. Mauk, J.L.; Crafford, T.C.; Horton, J.D.; San Juan, C.A.; and Robinson, G.R. Jr., “Pyrrhotite Distribution in the Conterminous United States,” U.S. Geological Survey Fact Sheet 2020-3017, Mar. 2020, 4 pp. doi:10.3133/fs20203017

15. CSA A23.1:19/CSA A23.2:19, “Concrete Materials and Methods of Concrete Construction / Test Methods and Standard Practices for Concrete,” CSA Group, Toronto, ON, Canada, Jan. 2019, 882 pp.

16. Duchesne, J.; Rodriques, A.; and Fournier, B., “Concrete Damage due to Oxidation of Sulfide-Bearing Aggregate: A Review,” RILEM Technical Letters, V. 6, July 2021, pp. 82-92.

17. ASTM C33/C33M-18, “Standard Specification for Concrete Aggregates,” ASTM International, West Conshohocken, PA, 2018, 8 pp.

18. ACI Committee 201, “Guide to Durable Concrete Reference (201.2R-16),” American Concrete Institute, Farmington Hills, MI, 2016, 84 pp.

19. BS EN 12620:2013, “Aggregates for Concrete (Withdrawn),” British Standards Institution, London, UK, 2013, 54 pp.

20. Chinchón-Payá, S.; Aguado, A.; and Chincón, S., “A Comparative Investigation of the Degradation of Pyrite and Pyrrhotite Under Simulated Laboratory Conditions,” Engineering Geology, V. 127, Feb. 2012, pp. 75-80.

21. Marcelino, A.; Calixto, J.M.; Gumieri, A.G.; Ferreira, M.C.; Caldeira, C.; Silva, M.V.; and Costa, A.L., “Evaluation of Pyrite and Pyrrhotite in Concretes,” Revista IBRACON de Estruturas e Materiais, V. 9, No. 3, June 2016, pp. 484-493.

22. Ideker, J.H.; Bentivegna, A.F.; Folliard, K.J.; and Juenger, M.C.G., “Do Current Laboratory Test Methods Accurately Predict Alkali-Silica Reactivity?” ACI Materials Journal, V. 109, No. 4, July-Aug. 2012, pp. 395-402.

23. ASTM E1621-22, “Standard Guide for Elemental Analysis by Wavelength Dispersive X-Ray Fluorescence Spectrometry,” ASTM International, West Conshohocken, PA, 2022, 9 pp.

24. ASTM D4239-18e1, “Standard Test Method for Sulfur in the Analysis Sample of Coal and Coke Using High-Temperature Tube Furnace Combustion,” ASTM International, West Conshohocken, PA, 2018, 8 pp.

25. ASTM E1915-20, “Standard Test Methods for Analysis of Metal Bearing Ores and Related Materials for Carbon, Sulfur, and Acid-Base Characteristics,” ASTM International, West Conshohocken, PA, 2020, 24 pp.

26. ASTM C1293-20a, “Standard Test Method for Determination of Length Change of Concrete Due to Alkali-Silica Reaction,” ASTM International, West Conshohocken, PA, 2020, 6 pp.

27. ASTM C227-10, “Standard Test Method for Potential Alkali Reactivity of Cement-Aggregate Combinations (Mortar-Bar Method) (Withdrawn 2018),” ASTM International, West Conshohocken, PA, 2010, 6 pp.