Assessment of Deflection Prediction Models for Cracked Prestressed Concrete Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Assessment of Deflection Prediction Models for Cracked Prestressed Concrete Beams

Author(s): Wassim Nasreddine, Adi Obeidah, Peter H. Bischoff, and Hani Nassif

Publication: Structural Journal

Volume: 120

Issue: 6

Appears on pages(s): 167-179

Keywords: deflection; effective moment of inertia; partially prestressed; prestressed concrete

DOI: 10.14359/51739094

Date: 11/1/2023

Abstract:
Variability of deflection prediction models is assessed for cracked prestressed concrete flexural members with bonded steel tendons. Current models for computing deflection are based on an effective moment of inertia (with or without an offset moment for the cracked section response) or a bilinear moment-deflection response using the moment of inertia of the uncracked section before cracking and moment of inertia of the cracked section after cracking. The accuracy of the approaches provided in ACI 318-19, the PCI Design Handbook, and elsewhere are examined for computing immediate deflection using a large database of 180 fully prestressed as well as partially prestressed beams. Parameters considered in the analysis include the effect of tension-stiffening, reinforcement ratio, prestressing type (fully or partially prestressed), cracking moment, concrete elastic modulus, modulus of rupture, and the use of transformed or gross section properties. Results highlight the need for a rational model that can be universally applied to reinforced as well as prestressed concrete flexural members.

Related References:

Abdelrahman, A. A., 1995, “Serviceability of Concrete Beams Prestressed by Fiber Reinforced Plastic Tendons,” PhD thesis, University of Manitoba, Winnipeg, MB, Canada.

ACI Committee 318, 2019, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 624 pp.

ACI Committee 435, 2000, “Control of Deflection in Concrete Structures (ACI 435R-95) (Reapproved 2000), American Concrete Institute, Farmington Hills, MI, 77 pp.

Alkokani, A. F., 1982, “Behavior and Design of Partially Prestressed Concrete Beams,” PhD thesis, The Pennsylvania State University, University Park, PA.

Billet, D. F., 1953, “Study of Prestressed Concrete Beams Failing in Flexure,” MS thesis, University of Illinois, Engineering Experiment Station, Urbana, IL.

Bischoff, P. H., 2005, “Reevaluation of Deflection Prediction for Concrete Beams Reinforced with Steel and Fiber Reinforced Polymer Bars,” Journal of Structural Engineering, ASCE, V. 131, No. 5, May, pp. 752-767. doi: 10.1061/(ASCE)0733-9445(2005)131:5(752)

Bischoff, P. H., 2020, “Comparison of Existing Approaches for Computing Deflection of Reinforced Concrete,” ACI Structural Journal, V. 117, No. 1, Jan., pp. 231-240. doi: 10.14359/51718072

Bischoff, P. H., 2022, “Deformation Model for Reinforced and Cracked Prestressed Concrete,” ACI Structural Journal, V. 119, No. 1, Jan., pp. 243-254. doi: 10.14359/51733138

Bischoff, P. H.; Naito, C. J.; and Ingaglio, J. P., 2018, “Immediate Deflection of Partially Prestressed Concrete Flexural Members,” ACI Structural Journal, V. 115, No. 6, Nov., pp. 1683-1693. doi: 10.14359/51702381

Bischoff, P. H., and Scanlon, A., 2007, “Effective Moment of Inertia for Calculating Deflections of Concrete Members Containing Steel Reinforcement and Fiber-Reinforced Polymer Reinforcement,” ACI Structural Journal, V. 104, No. 1, Jan.-Feb., pp. 68-75.

Branson, D. E., 1965, “Instantaneous and Time-Dependent Deflections of Simple and Continuous Reinforced Concrete Beams,” HPR Report No. 7, Part 1, Alabama Highway Department, Bureau of Public Roads, Montgomery, AL, 78 pp.

Branson, D. E., 1977, Deformation of Concrete Structures, McGraw-Hill, New York, NY, 546 pp.

Branson, D. E.; Meyers, B. L.; and Kripanarayanan, K. M., 1970, “Loss of Prestress, Camber, and Deflection of Noncomposite and Composite Structures Using Different Weight Concretes,” Report No. 70-6, Department of Civil Engineering, University of Iowa, Iowa City, IA.

Branson, D. E., and Trost, H., 1982a, “Unified Procedures for Predicting the Deflection and Centroidal Axis Location of Partially Cracked Non-Prestressed and Prestressed Concrete Members,” ACI Journal Proceedings, V. 79, No. 2, Mar.-Apr., pp. 119-130.

Branson, D. E., and Trost, H., 1982b, “Application of the I-Effective Method in Calculating Deflections of Partially Prestressed Members,” PCI Journal, V. 27, No. 5, Sept.-Oct., pp. 62-77. doi: 10.15554/pcij.09011982.62.77

Chen, C. I., 1973, “Integrated Procedures for Predicting the Initial and Time-Dependent Deformation of ‘Reinforced’ Concrete Structures,” PhD thesis, University of Iowa, Iowa City, IA.

Elzanaty, A. H.; Nilson, A. H.; and Slate, F. O., 1986, “Shear Capacity of Prestressed Concrete Beams Using High-Strength Concrete,” ACI Journal Proceedings, V. 83, No. 3, May-June, pp. 359-368.

Founas, M., 1989, “Deformations and Deflections of Partially Prestressed Concrete T-Beams under Static and Random Amplitude Fatigue Loading,” PhD thesis, University of Michigan, Ann Arbor, MI.

Gowripalan, N., and Zou, X. W., 1999, “Flexural Behavior and Ductility of Prestressed Beams with High-Strength Concrete,” High Performance Concrete—Proceedings: ACI International Conference, Malaysia, 1997, SP-172, V. M. Malhotra, ed., American Concrete Institute, Farmington Hills, MI, pp. 573-600.

Hanson, J. M., 1964, “Ultimate Shear Strength of Prestressed Concrete Beams with Web Reinforcement,” PhD thesis, Lehigh University, Bethlehem, PA.

Hanson, J. M., and Hulsbos, C. L., 1963, “Overload Behavior of Prestressed Concrete Beams with Web Reinforcement,” Fritz Engineering Laboratory Report No. 223.25, Lehigh University, Bethlehem, PA.

Harajli, M., and Naaman, A. E., 1984, “Deformation and Cracking of Partially Prestressed Concrete Beams under Static and Cyclic Fatigue Loading,” Report No. UMEE 84R1, Department of Civil Engineering, University of Michigan, Ann Arbor, MI.

Hernandez, G., 1958, “Strength of Prestressed Concrete Beams with Web Reinforcement,” PhD thesis, University of Illinois, Engineering Experiment Station, Urbana, IL.

Huang, P. T., 1975, “Serviceability Behavior and Crack Control in Pretensioned Prestressed Concrete I- and T-Beams,” PhD thesis, Rutgers, the State University of New Jersey, New Brunswick–Piscataway, NJ.

Janney, J. R.; Hognestad, E.; and McHenry, D., 1956, “Ultimate Flexural Strength of Prestressed and Conventionally Reinforced Concrete Beams,” ACI Journal Proceedings, V. 52, No. 2, Feb., pp. 601-620.

Jiang, Q.; Wang, H.; Chong, X.; Feng, Y.; and Ye, X., 2021, “Flexural Behavior of High-Strength, Steel Reinforced and Prestressed Concrete Beams,” Frontiers of Structural and Civil Engineering, V. 15, No. 1, pp. 227-243. doi: 10.1007/s11709-020-0687-3

Kassian, W., 2016, Prestressed Concrete, Concrete Design Handbook, fourth edition, Cement Association of Canada, Ottawa, ON, Canada, pp. 10-1 – 10-78.

Krishna Mohan Rao, S. V., and Dilger, W. H., 1992, “Evaluation of Short-Term Deflections of Partially Prestressed Concrete Members,” ACI Structural Journal, V. 89, No. 1, Jan.-Feb., pp. 71-78.

Martinez, S.; Nilson, A. H.; and Slate, F. O., 1984, “Spirally Reinforced High-Strength Concrete Columns,” ACI Journal Proceedings, V. 81, No. 5, May, pp. 431-442.

Mast, R. F., 1998, “Analysis of Cracked Prestressed Concrete Sections: A Practical Approach,” PCI Journal, V. 43, No. 4, July-Aug., pp. 80-91. doi: 10.15554/pcij.07011998.80.91

Naaman, A. E., 1982, Prestressed Concrete Analysis and Design: Fundamentals, McGraw-Hill Book Company, New York, 670 pp.

Nasreddine, W., 2022, “Flexural Behavior of Continuous and Simply Supported Beams Prestressed with Hybrid (CFRP and Steel) Tendons,” PhD thesis, Rutgers, the State University of New Jersey, New Brunswick–Piscataway, NJ.

Nilson, A. H., 1976, “Flexural Stresses after Cracking in Partially Prestressed Beams,” PCI Journal, V. 21, No. 4, July-Aug., pp. 72-81. doi: 10.15554/pcij.07011976.72.81

Obeidah, A., and Nassif, H., 2022, “Serviceability of Beams Prestressed with Hybrid (Steel/Carbon Fiber-Reinforced Polymer) Tendons,” ACI Structural Journal, V. 119, No. 3, May, pp. 179-190. doi:10.14359/51734437

Oukaili, N. K. A., and Khattab, M. M., 2018, “Strength and Serviceability of Partially Prestressed Concrete Beams Exposed to Limited Repeated Loading,” Proceedings, 5th International fib Congress, Oct. 7-11, 2018, Melbourne, Australia.

PCI Committee on Allowable Stresses in Prestressed Concrete Design, 1970, “Allowable Tensile Stresses for Prestressed Concrete,” PCI Journal, V. 15, No. 1, Feb., pp. 37-42.

Precast/Prestressed Concrete Institute (PCI), 2017, PCI Design Handbook: Precast and Prestressed Concrete (MNL-120-17), eighth edition, PCI, Chicago, IL.

Scanlon, A., and Bischoff, P. H., 2008, “Shrinkage Restraint and Loading History Effects on Deflections of Flexural Members,” ACI Structural Journal, V. 105, No. 4, July-Aug., pp. 498-506.

Shaikh, A. F., and Branson, D. E., 1970, “Non-Tensioned Steel in Prestressed Concrete Beams,” PCI Journal, V. 15, No. 1, Feb., pp. 14-36. doi: 10.15554/pcij.02011970.14.36

Shi, C., 2003, “Static and Fatigue Behaviour of Prestressed Concrete Beams Strengthened with Prestressed CFRP Sheets,” PhD thesis, Queens University, Kingston, ON, Canada.

Slepetz, J. M., 1968, “Behavior of Rectangular Prestressed Concrete Beams Subjected to Heavy Repeated Loads,” PhD thesis, Department of Civil Engineering, Duke University, Durham, NC.

Tadros, M. K., 1982, “Expedient Service Load Analysis of Cracked Prestressed Concrete Sections,” PCI Journal, V. 27, No. 6, Nov.-Dec., pp. 86-111. See also Reader Comment, PCI Journal, V. 28, No. 6, pp. 137-158.

Tadros, M. K.; Ghali, A.; and Meyer, A. W., 1985, “Prestressed Loss and Deflection of Precast Concrete Members,” PCI Journal, V. 30, No. 1, Jan.-Feb., pp. 114-141. doi: 10.15554/pcij.01011985.114.141

Warwaruk, J., 1957, “Strength in Flexure of Bonded and Unbonded Prestressed Concrete Beams,” MS thesis, University of Illinois, Engineering Experiment Station, Urbana, IL.

Warwaruk, J.; Sozen, M. A.; and Siess, C. P., 1962, “Strength and Behavior in Flexure of Prestressed Concrete Beams,” Investigation of Prestressed Reinforced Concrete for Highway Bridges, Part III, University of Illinois, Engineering Experiment Station, Urbana, IL.

Zou, P. X. W., 2003, “Flexural Behavior and Deformability of Fiber Reinforced Polymer Prestressed Concrete Beams,” Journal of Composites for Construction, ASCE, V. 7, No. 4, Nov., pp. 275-284. doi: 10.1061/(ASCE)1090-0268(2003)7:4(275)

Zwoyer, E. M., 1953, “Shear Strength of Simply Supported Prestressed Concrete Beams,” PhD thesis, University of Illinois, Engineering Experiment Station, Urbana, IL.


ALSO AVAILABLE IN:

Electronic Structural Journal