Experimental Fatigue Analysis of Stresses Caused by Superloads on Concrete Pavements

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Fatigue Analysis of Stresses Caused by Superloads on Concrete Pavements

Author(s): Nathanial Buettner and Julie Vandenbossche

Publication: Structural Journal

Volume: 120

Issue: 6

Appears on pages(s): 63-72

Keywords: damage; fatigue; nonlinear; overload; pavement; superload

DOI: 10.14359/51739086

Date: 11/1/2023

Abstract:
Superloads, defined as vehicles with a gross vehicle weight of over 890 kN, are believed to overload jointed plain concrete pavements (JPCPs) and have the potential to cause significantly more fatigue damage than typical truck traffic. It is anticipated that the fatigue damage is greater when the superload is applied later in the life of the JPCP. In this study, the stress pulses generated by superloads on JPCPs were characterized using finite element modeling and related to fatigue damage through the fatigue testing of concrete beams. Concrete beams subjected to loading profiles that simulate those of a superload were observed to accumulate fatigue damage at an accelerated rate when applied after 70% of the fatigue life of the concrete was consumed. Moreover, through the collection of fatigue life and beam response data, the effects of stress ratio, stress range, flexural strength, and damage state at the time of loading on the fatigue damage imposed by a superload movement were elucidated.

Related References:

1. Papagiannakis, A., “Practices for Permitting Superheavy Load Movements on Highway Pavements,” NCHRP Synthesis 476, The National Academies Press, Washington, DC, 2015, 253 pp.

2. ARA, Inc., “Guide for Mechanistic–Empirical Design of New and Rehabilitated Pavement Structures,” Final Report NCHRP 1-37A, Transportation Research Board of the National Academies, Washington, DC, 2004.

3. AASHTO, “AASHTO Guide for the Design of Pavement Structures,” American Association of State Highway and Transportation Officials, Washington, DC, 1993.

4. Miner, M. A., “Cumulative Damage in Fatigue,” Journal of Applied Mechanics, V. 12, No. 3, 1945, pp. 159-169. doi: 10.1115/1.4009458

5. Holmen, J. O., “Fatigue of Concrete by Constant and Variable Amplitude Loading,” Fatigue of Concrete Structures, SP-75, American Concrete Institute, Farmington Hills, MI, 1982, pp. 71-110.

6. Oh, B. H., “Cumulative Damage Theory of Concrete under Variable-Amplitude Fatigue Loadings,” ACI Materials Journal, V. 88, No. 1, Jan.-Feb. 1991, pp. 41-48.

7. Grzybowski, M., and Meyer, C., “Damage Accumulation in Concrete with and without Fiber Reinforcement,” ACI Materials Journal, V. 90, No. 6, Nov.-Dec. 1993, pp. 594-604.

8. Buettner, N.; Zhang, Q.; Vandenbossche, J. M.; and Oswalt, J., “Investigating the Effects of Superloads on Fatigue Performance in Jointed Plain Concrete Pavements,” 12th International Conference on Concrete Pavements, Sept. 27-Oct. 1, 2021.

9. Buettner, N., “Investigation of the Fatigue Damage Imposed by Superloads on Damaged Jointed Plain Concrete Pavements,” MS thesis, University of Pittsburgh, Pittsburgh, PA, 2022.

10. Khazanovich, L.; Yu, T.; Rao, S.; Galasova, E.; Shats, E.; and Jones, R., “ISLAB2000 – Finite Element Analysis Program for Rigid and Composite Pavements User’s Guide,” ERES Consultants, Champaign, IL, 2000.

11. Cornelissen, H. A. W., “Fatigue Failure of Concrete in Tension,” HERON, V. 29, No. 4, 1984, pp. 1-68.

12. Zhang, B.; Phillips, D. V.; and Wu, K., “Effects of Loading Frequency and Stress Reversal on Fatigue Life of Plain Concrete,” Magazine of Concrete Research, V. 48, No. 177, 1996, pp. 361-375. doi: 10.1680/macr.1996.48.177.361

13. Hsu, T. T., “Fatigue of Plain Concrete,” ACI Journal Proceedings, V. 78, No. 4, July-Aug. 1981, pp. 292-305.

14. Chatti, K.; Manik, A.; Salama, H.; Brake, N.; Haider, S. W.; Mohtar, C. E.; and Lee, H. S., “Effect of Michigan Multi-Axle Trucks on Pavement Distress (Volume III),” Report No. RC-1504, Michigan Department of Transportation, Lansing, MI, 2009, 121 pp.

15. ASTM C78/C78M-21, “Standard Test Method for Flexural Strength of Concrete (Using Simple Beam with Third-Point Loading),” ASTM International, West Conshohocken, PA, 2021.

16. ASTM C39/C39M-21, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2021.

17. ACI Committee 330, “Guide for the Design and Construction of Concrete Parking Lots (ACI 330R-08),” American Concrete Institute, Farmington Hills, MI, 2008, 36 pp.

18. PennDOT, “Materials Specifications (Publication 408/2020),” Pennsylvania Department of Transportation, Harrisburg, PA, 2020.

19. ASTM C192/C192M-19, “Standard Practice for Making and Curing Concrete Test Specimens in the Laboratory,” ASTM International, West Conshohocken, PA, 2019.

20. Murdock, J. W., and Kesler, C. E., “Effect of Range of Stress on Fatigue Strength of Plain Concrete Beams,” ACI Journal Proceedings, V. 55, No. 8, Aug. 1958, pp. 221-231.

21. Tepfers, R., “Tensile Fatigue Strength of Plain Concrete,” ACI Journal Proceedings, V. 76, No. 8, Aug. 1979, pp. 919-934.

22. Darter, M. I., “Design of a Zero-Maintenance Plain Jointed Concrete Pavement, Volume One—Development of Design Procedures,” Report No. FHWA-RD-77-111, Federal Highway Administration, Washington, DC, 1977, 261 pp.

23. Packard, R. G., and Tayabji, S. D., “New PCA Thickness Design Procedure for Concrete Highway and Street Pavements,” Proceedings of the 3rd International Conference on Concrete Pavement Design and Rehabilitation, Purdue University, West Lafayette, IN, 1985, pp. 225-236.


ALSO AVAILABLE IN:

Electronic Structural Journal