Corrosion in CSA and Other ACM Reinforced Concrete Systems

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Corrosion in CSA and Other ACM Reinforced Concrete Systems

Author(s): Berke

Publication: Web Session

Volume: ws_S23_Berke.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 4/2/2023

Abstract:
One of the outstanding questions regarding use of alternative cements in concrete infrastructure systems is the corrosion potential of these systems. This study investigated a variety of commercially available alternative concrete systems, including two calcium sulfoaluminate-based systems, tracking changes in conductivity, microcell current, chloride infiltration, and initiation and propagation of corrosion through cracked and uncracked concrete and mortar specimens to provide a comparison of corrosion-related behavior between ACM and OPC systems.