An Extrusion Based System for Additive Manufacturing of FRC Tunnel Linings: Validation via Non-Destructive and Destructive Tests

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: An Extrusion Based System for Additive Manufacturing of FRC Tunnel Linings: Validation via Non-Destructive and Destructive Tests

Author(s): Andrea Marcucci

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 4/2/2023

Abstract:
Recent years have brought many advancements in the novel use of fiber reinforced concretes including uses of: • “Smart” concretes made with “sensing” FRCs or fibers with time-changing properties • Use of various types of nano fibers such as carbon tubes, bio-nanofibers, etc. in conventional as well as UHPC concretes • 3D printing applications using FRCs • Extruded FRCs • Lower CO2 footprint concretes made with FRCs • CO2 neutral steel fibers The objective of the session is to bring together leading experts in this field, showcase the state-of-the-art and provide a platform for discussion on future directions and opportunities for implementation of these advanced technologies in concrete infrastructure.