Demonstration of Environmental Impact of Concrete Pavement Full Life Cycle Using Caltrans eLCAP Software

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Demonstration of Environmental Impact of Concrete Pavement Full Life Cycle Using Caltrans eLCAP Software

Author(s): Ali Butt

Publication: Web Session

Volume: ws_S23_AliButt.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 4/2/2023

Abstract:
Supplementary cementitious materials (SCMs) reduce clinker content in concrete and thus have the promise of reducing the overall greenhouse gas emissions of concrete. However, traditional SCMs such as fly ash and slag are increasingly imported or transported from certain locations in the US; thus, long-distance shipping and transportation adds to the overall GHG emissions of concrete. In this presentation, we present the use of locally available alternative SCMs in California, such as agricultural ashes (rice hull ash) and biomass ashes and natural pozzolans (volcanic ash, perlite, diatomaceous earth, etc.) and compare the global warming potential over the complete life cycle of the concrete pavement.