Concrete Pavement Design Optimization Provides Cost-Effective Pavement with Improved Long-Term Performance

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete Pavement Design Optimization Provides Cost-Effective Pavement with Improved Long-Term Performance

Author(s): Juan Pablo Covarrubias

Publication: Web Session

Volume: ws_S23_JuanCovarrubias.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 4/2/2023

Abstract:
The evolution of concrete pavement design has progressed significantly in recent years, more specifically with the advent of mechanistic-empirical (ME) pavement design methods. These more sophisticated design methods highlight the importance of holistically considering all factors that influence concrete pavement performance. Including loading & design life, subgrade support, flexural strength, thickness & joint spacing, edge support & joint stability, and humidity & ambient effects, all of which cannot be considered independently of each other. This presentation will discuss the evolution of concrete pavement design and how optimized designs can provide cost-effective pavement with improved long-term performance using ME design procedures.