Title: Development of Beneficial Use and Sustainable Materials Courses ENV6932 and CGN 6525

Author(s): Christopher Ferraro

Publication: Web Session

Volume: ws_S23_ChristopherFerraro2.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 4/2/2023

Abstract:
This presentation involves the creation of course content for a graduate level Beneficial Reuse Course currently being taught at the University of Florida (ENV 6932).