ACI PRC-522-23: Pervious Concrete—Report

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ACI PRC-522-23: Pervious Concrete—Report

Author(s): ACI Committee 522

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 56

Keywords:

DOI:

Date: 6/1/2023

Abstract:
This report provides technical information on pervious concrete’s application, design methods, materials, properties, mixture proportioning, construction methods, testing, and inspection. The term “pervious concrete” typically describes a near-zero-slump, open-graded material consisting of portland cement, coarse aggregate, little or no fine aggregate, admixtures, and water. The combination of these ingredients will produce a hardened material with connected pores, ranging in size from 0.08 to 0.32 in. (2 to 8 mm), that allow water to pass through easily. The void content can range from 15 to 35%, with typical compressive strengths of 400 to 4000 psi (2.8 to 28 MPa). The drainage rate of pervious concrete pavement will vary with aggregate size and density of the mixture but will generally fall into the range of 2 to 18 gal./min/ft2 (81 to 730 L/min/m2). Pervious concrete is widely recognized as a sustainable building material, as it reduces stormwater runoff, improves stormwater quality, may recharge groundwater supplies, and can reduce the impact of the urban heat island effect. Keywords: construction; design; drainage; green building; LEED® credit; permeability; pervious concrete pavement; stormwater; sustainability; testing.