NEx insights: User Experience and Success Stories with FRP-Reinforced Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: NEx insights: User Experience and Success Stories with FRP-Reinforced Concrete

Author(s):

Publication: Concrete International

Volume: 45

Issue: 6

Appears on pages(s): 32-33

Keywords:

DOI: 10.14359/51738859

Date: 6/1/2023

Abstract:
Sales of fiber-reinforced polymer (FRP) reinforcement and its use in concrete construction applications have been steadily increasing worldwide in recent years. To shed light on this growing trend, the second NEx workshop at the ACI Concrete Convention in San Francisco, CA, USA, was organized to build on the success of the first workshop that focused on designing with glass fiber-reinforced polymer (GFRP) reinforced concrete using ACI CODE-440.11-22, “Building Code Requirements for Structural Concrete Reinforced with Glass Fiber-Reinforced Polymer (GFRP) Bars—Code and Commentary.” Held on April 5, 2023, the workshop brought together engineers, owners, contractors, design consultants, and building officials to share their experiences in design and construction with FRP-reinforced concrete.