Behavior of Engineered Cementitious Composites with Expanded Glass for Thermal Applications

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Behavior of Engineered Cementitious Composites with Expanded Glass for Thermal Applications

Author(s): Adeyemi Adesina and Sreekanta Das

Publication: Materials Journal

Volume: 120

Issue: 4

Appears on pages(s): 3-14

Keywords: engineered cementitious composites (ECCs); expanded glass (EG); fly ash (FA); portland cement (PC); thermal conductivity

DOI: 10.14359/51738816

Date: 7/1/2023

Abstract:
Expanded glass (EG) made from recycled glass waste was used as an aggregate in the production of engineered cementitious composites (ECCs) to improve their thermal conductivity. The corresponding influence of the EG content on the physical, mechanical, and durability properties was evaluated. The EG was used as up to 100% replacement of the conventional silica sand (SS) in ECCs. The physical properties evaluated are thermal conductivity and density, while the mechanical properties evaluated are the compressive, flexural, and tensile strengths alongside the permeability properties and drying shrinkage. The findings from this study showed that the use of EG as a replacement for SS as aggregate in ECCs resulted in an improvement in the thermal insulation properties and a reduction in density. The 28-day thermal conductivity of ECCs made with EG as 100% replacement of SS is 53.8% lower than that of the ECCs made with only SS as the aggregate.

Related References:

1. Martínez-Molina, A.; Tort-Ausina, I.; Cho, S.; and Vivancos, J.-L., “Energy Efficiency and Thermal Comfort in Historic Buildings: A Review,” Renewable and Sustainable Energy Reviews, V. 61, Aug. 2016, pp. 70-85. doi: 10.1016/j.rser.2016.03.018

2. Agoudjil, B.; Benchabane, A.; Boudenne, A.; Ibos, L.; and Fois, M., “Renewable Materials to Reduce Building Heat Loss: Characterization of Date Palm Wood,” Energy and Buildings, V. 43, No. 2-3, Feb.-Mar. 2011, pp. 491-497. doi: 10.1016/j.enbuild.2010.10.014

3. Wu, Y.; Krishnan, P.; Yu, L. E.; and Zhang, M.-H., “Using Lightweight Cement Composite and Photocatalytic Coating to Reduce Cooling Energy Consumption of Buildings,” Construction and Building Materials, V. 145, Aug. 2017, pp. 555-564. doi: 10.1016/j.conbuildmat.2017.04.059

4. Coppola, B.; Courard, L.; Michel, F.; Incarnato, L.; Scarfato, P.; and Di Maio, L., “Hygro-Thermal and Durability Properties of a Lightweight Mortar Made with Foamed Plastic Waste Aggregates,” Construction and Building Materials, V. 170, May 2018, pp. 200-206. doi: 10.1016/j.conbuildmat.2018.03.083

5. Asasutjarit, C.; Hirunlabh, J.; Khedari, J.; Charoenvai, S.; Zeghmati, B.; and Shin, U. C., “Development of Coconut Coir-Based Lightweight Cement Board,” Construction and Building Materials, V. 21, No. 2, Feb. 2007, pp. 277-288. doi: 10.1016/j.conbuildmat.2005.08.028

6. Almeshal, I.; Tayeh, B. A.; Alyousef, R.; Alabduljabbar, H.; Mustafa Mohamed, A.; and Alaskar, A., “Use of Recycled Plastic as Fine Aggregate in Cementitious Composites: A Review,” Construction and Building Materials, V. 253, Aug. 2020, Article No. 119146. doi: 10.1016/j.conbuildmat.2020.119146

7. Li, V. C.; Wang, S.; and Wu, C., “Tensile Strain-Hardening Behavior of Polyvinyl Alcohol Engineered Cementitious Composite (PVA-ECC),” ACI Materials Journal, V. 98, No. 6, Nov.-Dec. 2001, pp. 483-492. doi: 10.14359/10851

8. Hisseine, O. A., and Tagnit-Hamou, A., “Development of Ecological Strain-Hardening Cementitious Composites Incorporating High-Volume Ground-Glass Pozzolans,” Construction and Building Materials, V. 238, Mar. 2020, Article No. 117740. doi: 10.1016/j.conbuildmat.2019.117740

9. Zhang, Z.; Yang, F.; Liu, J.-C.; and Wang, S., “Eco-Friendly High Strength, High Ductility Engineered Cementitious Composites (ECC) with Substitution of Fly Ash by Rice Husk Ash,” Cement and Concrete Research, V. 137, Nov. 2020, Article No. 106200. doi: 10.1016/j.cemconres.2020.106200

10. Xu, L.-Y.; Huang, B.-T.; and Dai, J.-G., “Development of Engineered Cementitious Composites (ECC) Using Artificial Fine Aggregates,” Construction and Building Materials, V. 305, Oct. 2021, Article No. 124742. doi: 10.1016/j.conbuildmat.2021.124742

11. Kralj, D., “Experimental Study of Recycling Lightweight Concrete with Aggregates Containing Expanded Glass,” Process Safety and Environmental Protection, V. 87, No. 4, July 2009, pp. 267-273. doi: 10.1016/j.psep.2009.03.003

12. Adewoyin, O.; Adesina, A.; and Das, S., “Physico-Thermal and Microstructural Properties of Thermal-Efficient Mortars Made with Low Cement Content,” Construction and Building Materials, V. 325, Mar. 2022, Article No. 126850. doi: 10.1016/j.conbuildmat.2022.126850

13. Adewoyin, O.; Adesina, A.; and Das, S., “Performance Evaluation of Thermal-Efficient Lightweight Mortars Made with Expanded Glass as Aggregates,” Journal of Materials in Civil Engineering, ASCE, V. 34, No. 5, May 2022, p. 04022068. doi: 10.1061/(ASCE)MT.1943-5533.0004208

14. Adesina, A., and Das, S., “Sustainable Utilization of Recycled Asphalt as Aggregates in Engineered Cementitious Composites,” Construction and Building Materials, V. 283, May 2021, Article No. 122727. doi: 10.1016/j.conbuildmat.2021.122727

15. Lu, D.; Tang, Z.; Zhang, L.; Zhou, J.; Gong, Y.; Tian, Y.; and Zhong, J., “Effects of Combined Usage of Supplementary Cementitious Materials on the Thermal Properties and Microstructure of High-Performance Concrete at High Temperatures,” Materials (Basel), V. 13, No. 8, Apr. 2020, Article No. 1833. doi: 10.3390/ma13081833

16. Sargam, Y.; Wang, K.; and Alleman, J. E., “Effects of Modern Concrete Materials on Thermal Conductivity,” Journal of Materials in Civil Engineering, ASCE, V. 32, No. 4, Apr. 2020, p. 04020058. doi: 10.1061/(ASCE)MT.1943-5533.0003026

17. Huang, X.; Ranade, R.; Zhang, Q.; Ni, W.; and Li, V. C., “Mechanical and Thermal Properties of Green Lightweight Engineered Cementitious Composites,” Construction and Building Materials, V. 48, Nov. 2013, pp. 954-960. doi: 10.1016/j.conbuildmat.2013.07.104

18. Özbay, E.; Karahan, O.; Lachemi, M.; Hossain, K. M. A.; and Atis, C. D., “Dual Effectiveness of Freezing-Thawing and Sulfate Attack on High-Volume Slag-Incorporated ECC,” Composites Part B: Engineering, V. 45, No. 1, Feb. 2013, pp. 1384-1390. doi: 10.1016/j.compositesb.2012.07.038

19. Özbay, E.; Karahan, O.; Lachemi, M.; Hossain, K. M. A.; and Atiş, C. D., “Investigation of Properties of Engineered Cementitious Composites Incorporating High Volumes of Fly Ash and Metakaolin,” ACI Materials Journal, V. 109, No. 5, Sept.-Oct. 2012, pp. 565-571. doi: 10.14359/51684088

20. Adesina, A., and Das, S., “Mechanical Performance of Engineered Cementitious Composite Incorporating Glass as Aggregates,” Journal of Cleaner Production, V. 260, July 2020, Article No. 121113. doi: 10.1016/j.jclepro.2020.121113

21. ASTM D5334-14, “Standard Test Method for Determination of Thermal Conductivity of Soil and Soft Rock by Thermal Needle Probe Procedure,” ASTM International, West Conshohocken, PA, 2014, 8 pp.

22. ASTM C109/109M-16a, “Standard Test Method for Compressive Strength of Hydraulic Cement Mortars (Using 2-in. or [50-mm] Cube Specimens),” ASTM International, West Conshohocken, PA, 2016, 10 pp.

23. JSCE Concrete Committee, “Recommendations for Design and Construction of High Performance Fiber Reinforced Cement Composites with Multiple Fine Cracks (HPFRCC),” Japan Society of Civil Engineers, Tokyo, Japan, 2008, 113 pp.

24. Adesina, A., and Das, S., “Performance of Engineered Cementitious Composites Incorporating Crumb Rubber as Aggregate,” Construction and Building Materials, V. 274, Mar. 2021, Article No. 122033. doi: 10.1016/j.conbuildmat.2020.122033

25. ASTM C1609/C1609M-07, “Standard Test Method for Flexural Performance of Fiber-Reinforced Concrete (Using Beam With Third-Point Loading),” ASTM International, West Conshohocken, PA, 2007, 9 pp.

26. ASTM C642-13, “Standard Test Method for Density, Absorption, and Voids in Hardened Concrete,” ASTM International, West Conshohocken, PA, 2013, 3 pp.

27. ASTM C1757-13, “Standard Test Method for Determination of One-Point, Bulk Water Sorption of Dried Concrete (Withdrawn 2022),” ASTM International, West Conshohocken, PA, 2013, 3 pp.

28. ASTM C1585-13, “Standard Test Method for Measurement of Rate of Absorption of Water by Hydraulic-Cement Concretes,” ASTM International, West Conshohocken, PA, 2013, 6 pp.

29. ASTM C1202-12, “Standard Test Method for Electrical Indication of Concrete’s Ability to Resist Chloride Ion Penetration,” ASTM International, West Conshohocken, PA, 2012, 8 pp.

30. ASTM C596-07, “Standard Test Method for Drying Shrinkage of Mortar Containing Hydraulic Cement,” ASTM International, West Conshohocken, PA, 2007, 3 pp.

31. ASTM C597-02, “Standard Test Method for Pulse Velocity Through Concrete,” ASTM International, West Conshohocken, PA, 2002, 4 pp.

32. Shi, C., “Pozzolanic Reaction and Microstructure of Chemical Activated Lime-Fly Ash Pastes,” ACI Materials Journal, V. 95, No. 5, Sept.-Oct. 1998, pp. 537-545. doi: 10.14359/396

33. Vance, K.; Aguayo, M.; Oey, T.; Sant, G.; and Neithalath, N., “Hydration and Strength Development in Ternary Portland Cement Blends Containing Limestone and Fly Ash or Metakaolin,” Cement and Concrete Composites, V. 39, May 2013, pp. 93-103. doi: 10.1016/j.cemconcomp.2013.03.028

34. Wu, Y.; Wang, J.-Y.; Monteiro, P. J. M.; and Zhang, M.-H., “Development of Ultra-Lightweight Cement Composites with Low Thermal Conductivity and High Specific Strength for Energy Efficient Buildings,” Construction and Building Materials, V. 87, July 2015, pp. 100-112. doi: 10.1016/j.conbuildmat.2015.04.004

35. Jin, Q., and Li, V. C., “Development of Lightweight Engineered Cementitious Composite for Durability Enhancement of Tall Concrete Wind Towers,” Cement and Concrete Composites, V. 96, Feb. 2019, pp. 87-94. doi: 10.1016/j.cemconcomp.2018.11.016

36. ASTM C330/C330M-09, “Standard Specification for Lightweight Aggregates for Structural Concrete,” ASTM International, West Conshohocken, PA, 2009, 4 pp.

37. ACI Committee 213, “Guide for Structural Lightweight-Aggregate Concrete (ACI 213R-03),” American Concrete Institute, Farmington Hills, MI, 2003, 38 pp.

38. Kaze, C. R.; Lemougna, P. N.; Alomayri, T.; Assaedi, H.; Adesina, A.; Das, S. K.; Lecomte-Nana, G.-L.; Kamseu, E.; Chinje Melo, U.; and Leonelli, C., “Characterization and Performance Evaluation of Laterite Based Geopolymer Binder Cured at Different Temperatures,” Construction and Building Materials, V. 270, Feb. 2021, Article No. 121443. doi: 10.1016/j.conbuildmat.2020.121443

39. Abdel Tawab, O. F.; Amin, M. R.; Ibrahim, M. M.; Abdel Wahab, M.; Abd El Rahman, E. N.; Hassanien, R. H.; Hatem, M. H.; and Ghaly, A. E., “Recycling Waste Plastic Bags as a Replacement for Cement in Production of Building Bricks and Concrete Blocks,” Journal of Waste Resources and Recycling, V. 2, No. 1, 2020, 13 pp.

40. Adesina, A., “Overview of the Influence of Waste Materials on the Thermal Conductivity of Cementitious Composites,” Cleaner Engineering and Technology, V. 2, June 2021, Article No. 100046. doi: 10.1016/j.clet.2021.100046

41. Keskin, S. B.; Sulaiman, K.; Sahmaran, M.; and Yaman, I. O., “Effect of Presoaked Expanded Perlite Aggregate on the Dimensional Stability and Mechanical Properties of Engineered Cementitious Composites,” Journal of Materials in Civil Engineering, ASCE, V. 25, No. 6, June 2013, pp. 763-771. doi: 10.1061/(ASCE)MT.1943-5533.0000553

42. Zhang, Z.; Ma, H.; and Qian, S., “Investigation on Properties of ECC Incorporating Crumb Rubber of Different Sizes,” Journal of Advanced Concrete Technology, V. 13, No. 5, 2015, pp. 241-251. doi: 10.3151/jact.13.241

43. Huang, X.; Ranade, R.; Ni, W.; and Li, V. C., “On the Use of Recycled Tire Rubber to Develop Low E-Modulus ECC for Durable Concrete Repairs,” Construction and Building Materials, V. 46, Sept. 2013, pp. 134-141. doi: 10.1016/j.conbuildmat.2013.04.027

44. Yang, E.-H.; Yang, Y.; and Li, V. C., “Use of High Volumes of Fly Ash to Improve ECC Mechanical Properties and Material Greenness,” ACI Materials Journal, V. 104, No. 6, Nov.-Dec. 2007, pp. 620-628. doi: 10.14359/18966

45. Li, G., and Zhao, X., “Properties of Concrete Incorporating Fly Ash and Ground Granulated Blast-Furnace Slag,” Cement and Concrete Composites, V. 25, No. 3, Apr. 2003, pp. 293-299. doi: 10.1016/S0958-9465(02)00058-6

46. Şahmaran, M.; Lachemi, M.; Hossain, K. M. A.; and Li, V. C., “Internal Curing of Engineered Cementitious Composites for Prevention of Early Age Autogenous Shrinkage Cracking,” Cement and Concrete Research, V. 39, No. 10, Oct. 2009, pp. 893-901. doi: 10.1016/j.cemconres.2009.07.006

47. Zhou, Y.; Xi, B.; Sui, L.; Zheng, S.; Xing, F.; and Li, L., “Development of High Strain-Hardening Lightweight Engineered Cementitious Composites: Design and Performance,” Cement and Concrete Composites, V. 104, Nov. 2019, Article No. 103370. doi: 10.1016/j.cemconcomp.2019.103370

48. Adesina, A., and Das, S., “Evaluation of the Durability Properties of Engineered Cementitious Composites Incorporating Recycled Concrete as Aggregate,” Journal of Materials in Civil Engineering, ASCE, V. 33, No. 2, Feb. 2021, p. 04020439. doi: 10.1061/(ASCE)MT.1943-5533.0003563

49. Xuan, Z., and Jun, Z., “Influence of Zeolite Addition on Mechanical Performance and Shrinkage of High Strength Engineered Cementitious Composites,” Journal of Building Engineering, V. 36, Apr. 2021, Article No. 102124. doi: 10.1016/j.jobe.2020.102124


ALSO AVAILABLE IN:

Electronic Materials Journal