Struts and Ties Realization in Reinforced Concrete Ring Deep Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Struts and Ties Realization in Reinforced Concrete Ring Deep Beams

Author(s): Khattab Saleem Abdul-Razzaq, Wisam H. Khaleel, and Asala A. Dawood

Publication: Structural Journal

Volume: 120

Issue: 4

Appears on pages(s): 151-164

Keywords: beam; curvature; deep; proposed strut-and-tie model (STM); reinforced concrete (RC); ring; strut; tie

DOI: 10.14359/51738771

Date: 7/1/2023

Abstract:
This study aims to shed light on the inclined direct stress pathsof curved struts in deep ring beams by converting them into real members. Five specimens were tested with three loading and three supporting points. Three specimens were conventional rings and two were in the form of a frame that took its cross-sectional dimensions from the strut-and-tie model (STM) in ACI 318-19. The effect of reinforcing struts was studied by reinforcing the rings with both proposed and conventional reinforcements, and the frames with theproposed reinforcement only. The findings show that the proposed reinforcement reduced weight and cost by approximately 18% and 13%, respectively, and provided openings for services by approximately 24%. Additionally, strut curvature was found to reduce load capacity by 3 to 6%, meaning that the STM is safe and can be used efficiently in this type of deep curved member.

Related References:

1. Abdul-Razzaq, K. S.; Jalil, A. M.; and Dawood, A. A., “Ring Deep Beam–A Parametric Study,” AIP Conference Proceedings, V. 2213, No. 1, 2020, p. 020128. doi: 10.1063/5.0000056

2. Talal, A. A.; Khaleel, W. H.; Hassan, B. N.; Abdul-Razzaq, K. S.; and Dawood, A. A., “A Finite Element Parametric Study of Reinforced Concrete Horizontally Circular Deep Beams,” E3S Web of Conferences, V. 318, 2021, p. 03013.

3. Mansur, M. A., and Rangan, B. V., “Study of Design Methods for Reinforced Concrete Curved Beams,” ACI Journal Proceedings, V. 78, No. 3, May-June 1981, pp. 226-254.

4. Hsu, T. T., “Torsion of Structural Concrete-Behavior of Reinforced Concrete Rectangular Members,” Torsion of Structural Concrete, SP-18, American Concrete Institute, Farmington Hills, MI, 1968, pp. 261-306.

5. Hsu, T. T.; Inan, M.; and Fonticiella, L., “Behavior of Reinforced Concrete Horizontally Curved Beams,” ACI Journal Proceedings, V. 75, No. 4, Apr. 1978, pp. 112-123.

6. Badawy, H. E. I.; McMullen, A. E.; and Jordaan, I. J., “Experimental Investigation of the Collapse of Reinforced Concrete Curved Beams,” Magazine of Concrete Research, V. 29, No. 99, 1977, pp. 59-69. doi: 10.1680/macr.1977.29.99.59

7. Tamura, T., and Murata, H., “Experimental Study on the Ultimate Strength of R/C Curved Beam,” Fracture Mechanics of Concrete and Concrete Structures—High Performance, Fiber Reinforced Concrete, Special Loadings and Structural Applications (FraMCos-7), Jeju, South Korea, May 2010, pp. 1783-1788.

8. Abdul-Razzaq, K. S., and Dawood, A. A., “Corbel Strut and Tie Modeling–Experimental Verification,” Structures, V. 26, 2020, pp. 327-339. doi: 10.1016/j.istruc.2020.04.021

9. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 623 pp.

10. Schlaich, J.; Schafer, K.; and Jennewein, M., “Toward a Consistent Design of Structural Concrete,” PCI Journal, V. 32, No. 3, 1987, pp. 74-150. doi: 10.15554/pcij.05011987.74.150

11. Schlaich, J., and Schafer, K., “Design and Detailing of Structural Concrete Using Strut-and-Tie Models,” Structural Engineering, V. 69, No. 6, 1991, pp. 113-125.

12. Sahoo, D. K.; Singh, B.; and Bhargava, P., “An Appraisal of the ACI Strut Efficiency Factors,” Magazine of Concrete Research, V. 61, No. 6, 2009, pp. 445-456. doi: 10.1680/macr.2008.00112

13. Sahoo, D. K.; Singh, B.; and Bhargava, P., “Effect of Inclination on the Strength of Struts,” Magazine of Concrete Research, V. 63, No. 2, 2011, pp. 111-117. doi: 10.1680/macr.9.00178

14. Kondalraj, R., and Appa Rao, G., “Experimental Verification of ACI 318 Strut-and-Tie Method for Design of Deep Beams without Web Reinforcement,” ACI Structural Journal, V. 118, No. 1, Jan. 2021, pp. 139-152.

15. Akhtaruzzaman, A. A., and Hasnat, A., “Torsion in Concrete Deep Beams with an Opening,” ACI Structural Journal, V. 86, No. 1, Jan.-Feb. 1989, pp. 20-25.

16. Samman, T. A., and Mesawa, A. A., “Torsional Behavior of High-Strength Concrete Deep Beams with Variable Dimensions,” Engineering and Science, V. 9, No. 1, 1997, pp. 41-57. doi: 10.4197/Eng.9-1.3

17. Abdul-Razzaq, K. S., and Jebur, S. F., “Suggesting Alternatives for Reinforced Concrete Deep Beams by Reinforcing Struts and Ties,” MATEC Web of Conferences, V. 120, 2017, p. 01004.

18. Abdul-Razzaq, K. S.; Mustafa Jalil, A.; and Asaad Dawood, A., “Reinforcing Struts and Ties in Concrete Continuous Deep Beams,” Engineering Structures, V. 240, 2021, p. 112339. doi: 10.1016/j.engstruct.2021.112339

19. Abdul-Razzaq, K. S., and Farhood, M. A., “Design-Oriented Testing and Modeling of Reinforced Concrete Pile Caps,” KSCE Journal of Civil Engineering, V. 23, No. 8, 2019, pp. 3509-3524. doi: 10.1007/s12205-019-1650-5

20. Abdul-Razzaq, K. S., and Dawood, A. A., “Reinforcing Struts and Ties in Concrete Corbels,” ACI Structural Journal, V. 118, No. 4, July 2021, pp. 153-162.

21. Abdul-Razzaq, K. S.; Talal, A. A.; and Dawood, A. A., “The Role of Reinforcement in Concrete Ring Deep Beams,” ACI Structural Journal, V. 120, No. 2, Mar. 2023, pp. 129-141.

22. Prakash, S.; Li, Q.; and Belarbi, A., “Behavior of Circular and Square Reinforced Concrete Bridge Columns under Combined Loading Including Torsion,” ACI Structural Journal, V. 109, No. 3, May-June 2012, pp. 317-328.

23. ASTM C39/C39M-03, “Standard Specification for Testing Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2003.

24. ASTM C496-96, “Standard Specification for Splitting Tensile Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 1996.

25. ASTM C78-02, “Standard Test Method for Flexural Strength Of Concrete (Using Simple Beam with Third-Point Loading),” ASTM International, West Conshohocken, PA, 2002.

26. ASTM A615/A615M-05, “Standard Specification for Deformed and Plain Billet-Steel Bars for Concrete Reinforcement,” ASTM International, West Conshohocken, PA, 2005, 5 pp.

27. ASTM A496-02, “Standard Specification for Steel Wire, Deformed, for Concrete Reinforcement,” ASTM International, West Conshohocken, PA, 2002, 5 pp.


ALSO AVAILABLE IN:

Electronic Structural Journal



  

Edit Module Settings to define Page Content Reviewer