Seismic Behavior of Slab-Column Connections Using High Performance Fiber Reinforced Concretes

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Seismic Behavior of Slab-Column Connections Using High Performance Fiber Reinforced Concretes

Author(s): Antonio Ramos, Brisid Isufi, and Rui Marreiros

Publication: Symposium Paper

Volume: 357

Issue:

Appears on pages(s): 123-138

Keywords: flat plate, flat slab, high performance fiber reinforced concrete, high strength concrete, punching shear, seismic loading.

DOI: 10.14359/51738763

Date: 4/1/2023

Abstract:
Significant research efforts have been devoted to achieving high performance of slab – column connections subjected to lateral loading. Solutions such as using stirrups and headed studs have been shown to work well. With the development of concrete materials with enhanced properties, new possibilities have arisen to employ solutions that are easy to apply and cause less congestion of reinforcement. A total of nine tests on flat slab specimens subjected to combined gravity and lateral loading are discussed, including two new specimens with High Performance Fiber Reinforced Concrete (HPFRC) over a limited region near the column. The main experimental variables were the flexural reinforcement ratio and the punching shear improvement method: none, headed studs, High Strength Concrete (HSC) or HPFRC. It is shown that excellent behavior is achieved with a relatively small amount of HPFRC, extended up to 1.5 times the effective depth of the slab from the face of the column. Punching was completely avoided until the end of the loading protocol (6% drift) for the specimens with HPFRC, whereas reference specimens without punching shear reinforcement failed at 1% drift and specimens with HSC reached 3% drifts. Additionally, the use of HPFRC led to an increased unbalanced moment transfer capacity and lateral stiffness, though this effect was more pronounced for specimens with lower flexural reinforcement ratio.

Related References:

Almeida, André F. O., Bruno Alcobia, Miguel Ornelas, Rui Marreiros, and António Pinho Ramos. 2020. “Behaviour of Reinforced-Concrete Flat Slabs with Stirrups under Reversed Horizontal Cyclic Loading.” Magazine of Concrete Research 72(7):339–56.

Almeida, André F. O., Micael M. G. Inácio, Válter J. G. Lúcio, and António Pinho Ramos. 2016. “Punching Behaviour of RC Flat Slabs under Reversed Horizontal Cyclic Loading.” Engineering Structures 117:204–19.

Almeida, André F. O., António Pinho Ramos, Válter Lúcio, and Rui Marreiros. 2020. “Behavior of RC Flat Slabs with Shear Bolts under Reversed Horizontal Cyclic Loading.” Structural Concrete 21(2):501–16.

Blazy, Julia, Sandra Nunes, Carlos Sousa, and Mário Pimentel. 2021. “Development of an HPFRC for Use in Flat Slabs.” RILEM Bookseries 30:209–20.

CEN. 2004. EN 1992-1-1. Eurocode 2 — Design of Concrete Structures. Part 1-1: General Rules and Rules for Buildings.

Cheng, Min-Yuan, Gustavo J. Parra-Montesinos, and Carol K. Shield. 2010. “Shear Strength and Drift Capacity of Fiber-Reinforced Concrete Slab-Column Connections Subjected to Biaxial Displacements.” Journal of Structural Engineering 136(9):1078–88.

Cheng, My and Gj Parra-Montesinos. 2010. “Evaluation of Steel Fiber Reinforcement for Punching Shear Resistance in Slab-Column Connections - Part II: Lateral Displacement Reversals.” ACI Structural Journal 107(01):110–18.

Durrani, A. J. and A. J. Diaz. 1992. “Seismic Resistance of Fiber-Reinforced Slab-Column Connections.” Pp. 3113–16 in Earthquake Engineering, Tenth World Conference. Rotterdam: Balkema.

Emam, Mohamed, H. Marzouk, and M. Sameh Hilal. 1997. “Seismic Response of Slab-Column Connections Constructed with High-Strength Concrete.” ACI Structural Journal 94(2):197–205.

EN 14651:2005+A1:2007(E) Test method for metallic fibre concrete – measuring the flexural tensile strength (limit of proportionality (LOP), residual). CEN European Committee for Standardization.

Gouveia, Nuno D., Duarte M. V. Faria, and António Pinho Ramos. 2019a. “Assessment of SFRC Flat Slab Punching Behaviour – Part I: Monotonic Vertical Loading.” Magazine of Concrete Research 71(11):587–98.

Gouveia, Nuno D., Duarte M. V. Faria, and António Pinho Ramos. 2019b. “Assessment of SFRC Flat Slab Punching Behaviour – Part II: Reversed Horizontal Cyclic Loading.” Magazine of Concrete Research 71(1):26–42.

Hallgren, Mikael. 1996. “Punching Shear Capacity of Reinforced High Strength Concrete Slabs.” KTH Royal Institute of Technology.

Harajli, M. H., D. Maalouf, and H. Khatib. 1995. “Effect of Fibers on the Punching Shear Strength of Slab-Column Connections.” Cement and Concrete Composites 17(2):161–70.

Inácio, Micael, Brisid Isufi, Massimo Lapi, and António Pinho Ramos. 2020. “Rational Use of High-Strength Concrete in Flat Slab-Column Connections under Seismic Loading.” ACI Structural Journal 117(6):297–310.

Inácio, Micael, Massimo Lapi, and Antonio Pinho Ramos. 2020. “Punching of Reinforced Concrete Flat Slabs – Rational Use of High Strength Concrete.” Engineering Structures 206:110194.

Inácio, Micael M. G., André F. O. Almeida, Duarte M. V. Faria, Válter J. G. Lúcio, and António Pinho Ramos. 2015.

“Punching of High Strength Concrete Flat Slabs without Shear Reinforcement.” Engineering Structures 103:275–84.

Isufi, Brisid, André Almeida, Rui Marreiros, António Pinho Ramos, and Válter Lúcio. 2021. “Slab – Column Connection Punching and Ductility Improvement Methods for Seismic Response of Buildings with Flat Slabs.” (Submitted for Publication).

Isufi, Brisid and António Pinho Ramos. 2021. “A Review of Tests on Slab-Column Connections with Advanced Concrete Materials.” Structures 32(May 2020):849–60.

Isufi, Brisid, António Pinho Ramos, and Válter Lúcio. 2019. “Reversed Horizontal Cyclic Loading Tests of Flat Slab Specimens with Studs as Shear Reinforcement.” Structural Concrete 20(1):330–47.

Isufi, Brisid, Mariana Rossi, and António Pinho Ramos. 2021. “Influence of Flexural Reinforcement on the Seismic Performance of Flat Slab – Column Connections.” Engineering Structures 242(September):112583.

Landler, Josef and Oliver Fischer. 2019. “Steigerung Der Durchstanztragfähigkeit Und Duktilität Durch Die Zugabe Moderner Hochleistungsstahlfasern.” Beton- Und Stahlbetonbau.

Marzouk, H. and A. Hussein. 1991. “Experimental Investigation on the Behavior of High-Strength Concrete Slabs.” ACI Structural Journal 88(6):701–13.

Marzouk, H. and Dajiu Jiang. 1997. “Experimental Investigation on Shear Enhancement Types for High-Strength Concrete Plates.” ACI Structural Journal 94(1):49–58.

Marzouk, H., Moustafa Osman, and A. Hussein. 2001. “Cyclic Loading of High-Strength Lightweight Concrete Slabs.” ACI Structural Journal 98(2):207–14.

Nunes, Sandra, Mário Pimentel, and Carlos Sousa. 2021. “Mechanical and Fracture Behaviour of an Hpfrc.” in BEfib2021. Valencia: RILEM-fib.

Ramos, António, Rui Marreiros, André Almeida, Brisid Isufi, and Micael Inácio. 2017. “Punching of Flat Slabs under Reversed Horizontal Cyclic Loading.” Pp. 253–72 in ACI Special Publication. Vol. 315, edited by C. E. Ospina, D. Mitchell, and A. Muttoni. ACI, fib.

Regan, P. E., A. Al-Hussaini, K. E. Ramdane, and H. Y. Xue. 1993. “Behaviour of High Strength Concrete Slabs.” Pp. 761–73 in Concrete 2000, edited by R. K. Dhir and M. R. Jones. E & FN Spon.

Schreiber, Sascha K. and Scott D. B. Alexander. 2001. Punching Shear Capacity of Slab-Column Connections with Steel-Fibre Reinforcement under Lateral Cyclic Loading. Edmonton, Alberta, Canada.

Scotta, Roberto and Paolo Giorgi. 2016. “Comparative Cyclic Tests of Exterior Flat Slab–Column Connections in Normal Concrete and Fiber-Reinforced Lightweight Aggregate Concrete.” Materials and Structures 49(10):4049–67.

Swamy, R. N. and S. A. R. Ali. 1982. “Punching Shear Behavior of Reinforced Slab-Column Connections Made with Steel Fiber Concrete.” ACI Journal Proceedings 79(5).

Tegos, J. A. and A. G. Tsonos. 1996. “Punching Strength Decay of Slab-Column Connections under Seismic Loading.” P. Paper No. 654 in Eleventh World Conference on Earthquake Engineering 11WCEE. Acapulco, Mexico: Elsevier Science Ltd.